DOI: 10.31399/asm.tb.sfa.t52780171
EISBN: 978-1-62708-268-6
...Abstract Abstract After the failure analysis team hypothesizes failure causes, prepares a failure mode assessment and assignment, and evaluates all potential failure causes, it may find in some cases that several causes are still suspect but cannot be confirmed. In this situation, an experiment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700215
EISBN: 978-1-62708-279-2
...Abstract Abstract This chapter briefly reviews the experience-based guidelines that were developed for forming and welding advanced high-strength steels (AHSS). It discusses the benefits of using HSS in car body structures and components that are analyzed by the performance indices developed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110666
EISBN: 978-1-62708-247-1
... with a section describing the distinction between quality and reliability and moves on to provide an overview of the concept of experiment design along with an example. The chapter then discusses the purposes of reliability engineering and introduces four basic statistical distribution functions useful...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400105
EISBN: 978-1-62708-316-4
.... If the punch die clearance is large, the unsupported regions of the cup wall may experience a form of undergo out-of-plane deformation (similar to wrinkling) called puckering . The punch force is transmitted from the bottom of the cup to the deformation zone (flange) through tension on the wall of the cup...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500073
EISBN: 978-1-62708-317-1
... sequence design for a new part generally is based on experience and knowledge gained from producing similar parts and necessary prototype runs. This experience-based methodology requires extensive resources and increases the design lead time. There are several articles and books that summarize the basic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700225
EISBN: 978-1-62708-279-2
...-Symmetric Aluminum Panel Drawing using Active Drawbeads , CIRP Ann.-Manuf. Techn. , Vol 48 ( No. 1 ), 1999 , p 209 – 212 10.1016/S0007-8506(07)63167-9 15.7 Du C. et al . , Springback Control with Variable Binder Force—Experiments and FEA Simulation , NUMIFORM 2004—Proc. of the 8th...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780147
EISBN: 978-1-62708-268-6
... is defective. This chapter focuses on the latter possibility. Based on the author’s experience, many people (especially the system designers) may be reluctant to conclude that designs can be defective. This is perhaps a natural reaction and explains why a first reaction is to find a nonconforming part...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500051
EISBN: 978-1-62708-317-1
.... finite element method forming tools process simulation sheet metal forming springback UNTIL RECENTLY, the design of metal forming tools was based mainly on knowledge gained through experience and expensive trial-and-error processes. However, today the metal forming industry is making use...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140001
EISBN: 978-1-62708-264-8
.... chemical composition crystal structure phase transformation pure iron STEELS ARE OVER 95% Fe, so a good starting point for understanding steel is to study the nature of solid iron. Consider the following experiment. A bar of pure iron (e.g., 25 mm, or 1 in., in diameter) is sectioned to form a thin...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490383
EISBN: 978-1-62708-340-9
... Plants , Armor A.F. , Bakker W.T. , Jaffee R.I. , and Touchton G. , Ed., Report CS-5181-SR , Electric Power Research Institute , Palo Alto, CA , 1988 , p 5-85 to 5-108 14. Townsend R.T. , CEGB Experience and U.K. Developments in Materials for Advanced Fossil...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260213
EISBN: 978-1-62708-336-2
... of an aluminum extrusion plant Each unit has its own quality checklist to determine the quality/performance of the individual unit. This system will not only assess the quality but also will do experiments of each unit or combined units to develop new products or to determine new process parameters...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630xvi
EISBN: 978-1-62708-270-9
..., and/or published literature for each failure. As failure analysts gain experience and expertise practicing this scientific art, they must use that intelligence and experience to enhance and sharpen the technical assessment and analysis, not abandon them. Lastly, failure analysts must consider that each failure...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2000
DOI: 10.31399/asm.tb.aet.t68260233
EISBN: 978-1-62708-336-2
... the start of substantial quality, cost, and productivity improvements in the organization. At the highest levels of maturity, companies use design of experiments and statistical process control methods extensively and make relatively modest use of acceptance sampling. The introduction of statistical process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060069
EISBN: 978-1-62708-343-0
... apply also to fractional loops, we generalize the following treatment for all positive numerical values of U and V . We consider first an argument for combining the multiple loops in Fig. 4.3 , based on simple logic and experience. From the previous examples, we can expect that the combination...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140301
EISBN: 978-1-62708-335-5
... A3.3 is a smooth specimen as used by the Naval Engineering Experiment Station. Figure A3.4 is a smooth specimen with a larger diameter used for die cast alloys. Fig. A3.2 Test sections of (a) smooth and (b) notched rotating beam fatigue specimens. Dimensions in inches Fig. A3.3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270031
EISBN: 978-1-62708-301-0
...) 5.7 Failure Modes and Effects Analysis (FMEA) 5.8 Failure Experience: Information Storage and Retrieval 5.9 Expert Systems for Failure Analysis References References 1. Bramfitt B.L and Lawrence S.J. , Field Metallography Techniques , Metallography and Microstructures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780001
EISBN: 978-1-62708-268-6
... about failure analysis address component or material failures. Component failures are relatively easy to address (e.g., resistors can fail open or sometimes short circuit; metal parts can fail in fatigue, in tension, or in other discernable failure modes; plastic components can experience brittle...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040059
EISBN: 978-1-62708-300-3
... in metal flow in the second test, the coupling determination of heat transfer and friction in one test is desired. Thus, ring tests were selected in Burte’s experiments [ Burte et al., 1989 ]. Using ring tests, the interface friction and interface heat transfer coefficients were determined at the same time...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
... experience disbonds. In addition to disbonds, resin-based materials can also experience crazing, cracking, structural failures, and delaminations. Composite materials are usually held together with adhesive bonds. If disbonds occur, several conditions should be assessed. Bondline dimensions (bond...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780249
EISBN: 978-1-62708-281-5
... cycles-to-failure curves for several polymers tested at a frequency of 30 Hz. PS, polystyrene; EP, epoxy; PET, polyethylene terephthalate; PMMA, polymethyl methacrylate; PPO, polyphenylene oxide; PE, polyethylene; PP, polypropylene; PTFE, polytetrafluoroethylene. Source: Ref 5 Experiments...