1-20 of 247 Search Results for

eutectic system

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 March 2012
Fig. 10.27 Temperature-composition space model of a ternary eutectic system with the reaction L → α + β + γ. Adapted from Ref 10.3 More
Image
Published: 01 March 2012
Fig. 10.29 Temperature-composition space model of a ternary eutectic system with the reaction L + α → β + γ. Adapted from Ref 10.3 More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420087
EISBN: 978-1-62708-310-2
... Abstract This chapter begins by presenting a generic eutectic phase diagram and identifying critical points, lines, and features. It then describes the composition and properties of aluminum-silicon and lead-tin eutectic systems, the characteristics of eutectic morphologies, the solidification...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240075
EISBN: 978-1-62708-251-8
... diagram can be used to determine three important types of information: the phases that are present, the composition of the phases, and the percentages or fractions of the phases. The chapter then describes the construction of one common type of binary phase diagram i.e., the eutectic alloy system...
Image
Published: 01 March 2012
Fig. 10.20 Three-phase equilibria in a ternary system with a eutectic reaction. Adapted from Ref 10.3 More
Image
Published: 01 December 2008
Fig. 4.4 Free-energy diagram for a eutectic ternary system. (a) Composition of a liquid phase (a liquidus surface or a primary crystallization surface of A) in equilibrium with A crystal. (b) Three-phase equilibrium of a liquid phase with A crystal and B crystal (a monovariant eutectic) More
Image
Published: 01 December 2008
Fig. 4.5 Calculated examples of phase diagrams for a eutectic ternary system. (a) Projection of a primary crystallization surface. (b) View of isothermal section. (c) View of vertical section (30% C) More
Image
Published: 01 April 2004
Fig. 2.51 Vertical section through the Au-Pb-Sn ternary system between eutectic lead-tin (Pb-62Sn) composition and gold, with the 8% Au concentration marked by a dashed line. The plan view of this section is marked by a dashed line on the liquidus projection of the Au-Pb-Sn ternary system More
Image
Published: 01 April 2004
Fig. 2.54 Vertical section through the Ag-Au-Sn ternary system between eutectic silver-tin solder (Ag-96.5Sn) and gold. The plan view of this section is marked by the dashed line in Fig. 2.53 . More
Image
Published: 01 December 2008
Fig. 9.11 The driving force on diffusion during eutectic solidification Δ G eff . (a) The phase diagram for eutectic system. (b) The free energy diagram ( T = T 1 ). (c) The diffusion of component atoms More
Image
Published: 01 July 1997
Fig. 12 Effect of composition on hot cracking susceptibility of welds in a eutectic system. Regions of hot crack susceptibility: A, no cracking; B, liquid healing is possible; C, hot crack sensitive. Source: Ref 19 More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420191
EISBN: 978-1-62708-310-2
.... eutectic reactions peritectic reactions space model ternary phase diagram TERNARY SYSTEMS are those having three components. It is not possible to describe the composition of a ternary alloy with a single number or fraction, as was done with binary alloys, but the statement of two independent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440049
EISBN: 978-1-62708-352-2
... of a fourth element to the temperature of the Ga-In-Sn eutectic Table 2.13 Effect of addition of a fourth element to the temperature of the Ga-In-Sn eutectic Order Alloy system Melting point, °C Temperature depression, −δ T 3 Ga-In-Sn 12 0 4 Ga-In-Sn + Ag 9 3 Ga-In-Sn + Al 9...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310331
EISBN: 978-1-62708-326-3
... Abstract Cast irons, like steels, are iron-carbon alloys but with higher carbon levels than steels to take advantage of eutectic solidification in the binary iron-carbon system. Like steel, heat treatment of cast iron includes stress relieving, annealing, normalizing, through hardening...
Image
Published: 01 August 2005
Fig. 5.12 Liquidus surface of the gold-germanium-silicon system. A continuous eutectic valley links the two binary eutectic points. This eutectic valley crosses the 22 carat fineness at the composition 91.6Au-6.8Ge-1.6Si. More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.tm.t52320259
EISBN: 978-1-62708-357-7
... C γ F e = 4.7 × 10 − 5  exp  ⁡ ( − 155 , 000 / R T ) As shown by the solid curves in Fig. 9.8 ( b , lower), γ → α transformation of Fe-C system is considerably slower than γ → α transformation of pure iron. 9.3 Thermodynamics of Eutectic Solidification...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230179
EISBN: 978-1-62708-298-3
... . 15.1 Beryllium-Silver (Ag-Be) Figure 15.1 . This system has one incongruent melting compound, AgBe 2 . The compound melts peritectically at a temperature of 1010 °C (1850 °F), and it decomposes at temperatures below 760 °C (1400 °F). The eutectic between this compound and pure silver is at 880...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060013
EISBN: 978-1-62708-261-7
... of equilibrium phase diagrams, the role of enthalpy and Gibb’s free energy in chemical reactions, and a method for determining phase compositions along the solidus and liquidus lines. atomic diffusion body-centered cubic systems crystal defects equilibrium phase diagram face-centered cubic systems...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.9781627082969
EISBN: 978-1-62708-296-9
Image
Published: 01 April 2004
Fig. 2.50 Liquidus projection of the Au-Pb-Sn ternary system. The first phase to form on solidification is labeled for each phase field. The 4% Au isoconcentration line is marked on the figure as is the tie line between lead-tin eutectic solder and pure gold. A concentration of 4% gold More