... Abstract This appendix lists approximate equivalent hardness numbers and tensile strengths for Vickers hardness numbers for steel. equivalent hardness numbers steel tensile strength Vickers hardness This appendix is a reprint of a table giving approximate equivalent Brinell...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1996
DOI: 10.31399/asm.tb.phtpclas.t64560435
EISBN: 978-1-62708-353-9
... Abstract This appendix lists approximate equivalent hardness numbers and tensile strengths for Brinell hardness numbers for steel. Brinell hardness equivalent hardness numbers steel tensile strength This appendix is a reprint of a table giving approximate equivalent Rockwell...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1996
DOI: 10.31399/asm.tb.phtpclas.t64560437
EISBN: 978-1-62708-353-9
... Abstract This appendix lists approximate equivalent hardness numbers and tensile strengths for Rockwell C and B hardness numbers for steel. equivalent hardness numbers Rockwell hardness steel tensile strength This appendix is a reprint of tables giving approximate equivalent...
Image
Published: 01 October 2011
Fig. A3.1 Approximate equivalent hardness numbers for steel. Points represent data from hardness conversion tables in ASTM E140. More
Image
Published: 01 September 2008
Fig. A3.1 Approximate equivalent hardness numbers for steel. Points represent data from the hardness conversion tables. More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130529
EISBN: 978-1-62708-284-6
... Abstract This appendix is a collection of tables listing examples of published hardness conversion equations, approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and equivalent hardness numbers for Brinell hardness numbers and Vickers (diamond pyramid) hardness...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060465
EISBN: 978-1-62708-261-7
... Abstract This appendix includes tables and figures that provide approximate Brinell equivalent hardness numbers for steels. Brinell equivalent hardness number steel HARDNESS CONVERSIONS ( Fig. A3.1 and Table A3.1 ) are empirical relationships limited to specific categories...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410647
EISBN: 978-1-62708-265-5
... This appendix is a compilation of approximate equivalent hardness numbers and tensile strengths for carbon and alloy steels in the annealed, normalized, and quenched-and-tempered conditions. alloy steel carbon steel equivalent hardness number tensile strength Approximate equivalent...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560459
EISBN: 978-1-62708-291-4
... Abstract This appendix includes a temperature conversion table, a table containing equivalent hardness numbers, and a unit conversion table. equivalent hardness numbers steel temperature conversion table tensile strength Temperature Conversions The general arrangement...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200422
EISBN: 978-1-62708-354-6
... 696.3705 703.2652 710.1600 717.0548 723.9495 730.8443 737.7390 744.6338 751.5285 Approximate Equivalent Hardness Numbers for Brinell Hardness Numbers for Steel<xref ref-type="table-fn" rid="t68200422-td6-tn1a">(a)</xref> (<xref ref-type="bibr" rid="t68200422-ref3">3</xref>) Table D-6...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140039
EISBN: 978-1-62708-264-8
... that these equivalent hardnesses apply to steels only; that is, do not use them for aluminum, copper, and other nonferrous alloys. Approximate equivalent hardness numbers for several hardness tests on steels Table 5.3 Approximate equivalent hardness numbers for several hardness tests on steels HRC HV HB...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1985
DOI: 10.31399/asm.tb.sagf.t63420043
EISBN: 978-1-62708-452-9
... thickness. Hardness is the only criterion normally used to interpret the strength of the part being examined and can be used interchangeably with confidence. Table 3-2 lists the approximate equivalent hardness numbers for steel as tabulated by the Society of Automotive Engineers Handbook . 3...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560001
EISBN: 978-1-62708-291-4
..., to be aware of the usefulness and limitations of hardness testing. Tabor ( Ref 5 ) has shown that the Vickers indentation hardness number is related to the yield stress of the material in compression, although more strictly to the yield stress of the material after it has been work hardened by about 8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170091
EISBN: 978-1-62708-297-6
... on mechanical properties of CG irons produced by the in-mold process. Carbon equivalents ranged from 4.33 to 4.45. The pearlite/ferrite ratio, and thus the strength and hardness of CG irons, can be increased by the use of a number of alloying elements, such as copper, nickel, molybdenum, tin, manganese...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440207
EISBN: 978-1-62708-262-4
... low carbon equivalents respond better and more consistently to quench hardening because the combined carbon is higher. Measuring Hardness of Cast Irons Conventional hardness measurements on cast irons always indicate lower values than the true hardness of the matrix because the graphite...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310079
EISBN: 978-1-62708-326-3
... discussed. In addition, the article provides information on the hardenability limits of H-steels after a note on hardenability correlation curves and Jominy equivalence charts. hardenability hardenability curves hardness Jominy end-quench test Jominy equivalence chart steel Introduction...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2024
DOI: 10.31399/asm.tb.phtpp.t59380163
EISBN: 978-1-62708-456-7
... or hardness tester vendors. Approximate equivalent hardness numbers for steel Table 9.3 Approximate equivalent hardness numbers for steel HV HK, 500 g load and greater HRC, 150 kg load, brale indenter Superficial brale indenter HB, 3000 kg load, 10 mm ball HR15N scale, 15 kg load HR30N...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440283
EISBN: 978-1-62708-262-4
... to 8-pitch gears made mostly from 8620H steel. This procedure was used to monitor the process variation in carburizing for surface hardness, effective case depth, and core hardness. The test pin diameter chosen was based on the gear tooth thickness and the fact that the test pin center cooling rate...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720085
EISBN: 978-1-62708-305-8
... is determined and converted to a hardness number (without measurement units), which is inversely related to the depth. Hardness testers can either be portable instruments or laboratory devices. Static indentation and rebound testing are discussed in this chapter. These two methods account for virtually all...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.9781627082518
EISBN: 978-1-62708-251-8