... Abstract This chapter describes the molecular structures and chemical reactions associated with the production of thermoset and thermoplastic components. It compares and contrasts the mechanical properties of engineering plastics with those of metals, and explains how fillers and reinforcements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780089
EISBN: 978-1-62708-281-5
... at the 35th Annual Technology Conference on Reinforced Plastics , Section 12-D, 1-7, Composites Institute, Society of the Plastics Industry, 1980 54. Hagnauer G.L. and Pearce P.J. , The Effects of Impurities on the Hydrolytic Stability and Curing Behavior of an Epoxy Resin , Organic Coat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780003
EISBN: 978-1-62708-281-5
... in processing and facilitate mold release. Basic thermoset resins are generally filled and/or reinforced. A filler may be fibrous (e.g., wood flour, glass fiber, carbon fiber) or in flake or granular form (e.g., mica, talc, calcium carbonate). Depending on the end use, combinations of fillers are often used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870401
EISBN: 978-1-62708-314-0
... M 0 ] d where V 0 and M 0 represent initial volume and mass and c and d are swelling constants. For a typical epoxy resin (3501-6), the swelling constants are c = –0.61 and d = 0.87. The type of reinforcement can substantially change the moisture absorption behavior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550621
EISBN: 978-1-62708-307-2
... engineers into the design process at an earlier stage, and the importance given to manufacturing in present-day product design has reinforced the fact that materials and manufacturing are closely linked in determining final properties. Moreover, worldwide competitiveness has increased the general level...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... a dry reinforcement is being impregnated through rollers with a liquid resin. Fig. 5.1 Typical wet lay-up operation Fig. 5.2 Example of a simple impregnation process To provide a smooth surface finish on the tool side, a gel coat is often applied to the mold-released tool prior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
... . Misorientation lowers the strength and stiffness, as shown for the short-fiber reinforced epoxies in Fig. 10.6 . In addition, where two flow fronts come together and solidify, they can produce planes of weakness called knit lines . Furthermore, processes that contain significant shear forces, such as injection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780417
EISBN: 978-1-62708-281-5
.... References 1. Smith B.W. et al. , Fractographic Analysis of Interlaminar Fractures in Graphite-Epoxy Material Structures , International Conference: Post Failure Analysis Techniques for Fiber Reinforced Composites , Air Force Wright Aeronautical Laboratories, MLSE, July 1985 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the properties and processing characteristics of glass, aramid, carbon, and ultra-high molecular weight polyethylene fibers and related product forms, including woven fabrics, prepreg, and reinforced mats. It also includes a review of fiber terminology as well...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870101
EISBN: 978-1-62708-314-0
... • “ The Nilo Nickel-Iron Alloys for Composite Tooling ,” Inco Alloys International , 1994 • Black S. , Epoxy-Based Pastes Provide Another Choice for Fabricating Large Parts , High-Perform. Comp. , January/February 2001 , p 20 – 24 • Niu M.C.Y. , Composite Airframe Structures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
..., and performance-cost tradeoffs of common MMCs, including aluminum-matrix composites, titanium-matrix composites, and fiber-metal laminates. It also explains how fiber-reinforced composites and laminates are made, describing both continuous and discontinuous fiber matrix production processes. metal-matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... as production equipment and product forms, and include guidelines for optimizing tradeoffs when selecting fibers, resins, and production techniques. composite forms composite processing polymer-matrix composites reinforcement materials THE ADVANTAGES OF HIGH-PERFORMANCE COMPOSITES are many...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... to coat the sheet steel as it is unwound from a coil. The paint used in the coil-coating process can be of virtually any generic type, although alkyds, polyesters, epoxies, and zinc-rich epoxy coatings are the most prevalent. Certain lining materials, such as hand lay-up fiberglass-reinforced plastics...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
..., epoxy, bismaleimide, cyanate ester, polyimide, and phenolic resins and various toughening methods. The chapter also covers thermoplastic matrix materials and product forms and provides an introduction to the physiochemical tests used to characterize resins and cured laminates. physiochemical test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870373
EISBN: 978-1-62708-314-0
... , 2001 10.31399/asm.hb.v21.a0003417 9. Wardle M.W. , Aramid Fiber Reinforced Plastics—Properties , Comprehensive Composite Materials , Vol 2 , Polymer Matrix Composites , Elsevier Science Ltd. , 2000 10.1016/B0-08-042993-9/00182-0 10. “ Cycom 977-3 Toughened Epoxy Resin ,” Cytec...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... applications. Early work was conducted in the 1970s with boron or Borsic (a silicon carbide-coated boron fiber) reinforced aluminum for aircraft/spacecraft applications. Later work in the 1990s concentrated on SiC monofilaments in titanium ( Fig. 20.6 ) for the National Aerospace Plane. Potential applications...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
... 193 – 202 8.40 Samyn P. , Van Schepdael L. , Van Paepegem W. , Leedertz J.S. , Suister E. , DeBaets P. , Derieck P. , and Degrieck J.S. , Fracture Assessment of Carbon Fibre/Epoxy Reinforcing Rings Through a Combination of Full Scale Testing, Small Scale...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870255
EISBN: 978-1-62708-314-0
... polyimide (Nomex) High/moderate 500 Hexagonal 1.5–9    OX 1.8–4 High performance aramid Paper reinforced phenolic (N636) High/high 350 Hexagonal    2–9    flex-core 4.5 Aramid fabric reinforced epoxy High/moderate 350 Hexagonal 2.5           Bias weave carbon fabric...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
..., carbon and graphite, catalyzed resin coatings and ceramics are among the various materials available. Many materials will be immediately excluded because of service conditions, that is, pressures too high for RTP, temperatures too high for nonmetallic linings and coatings such as rubber or epoxy resins...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... to metals (e.g., niobium alloys). However, the silicide coating is brittle and susceptible to chipping. Another high-temperature coating consists of a borosilicate glass matrix reinforced with iron and nickel powders. The iron and nickel impart toughness to the composite. Chromium oxide is another...