1-20 of 20 Search Results for

electrostatic precipitators

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430017
EISBN: 978-1-62708-253-2
... in a superheater. Exhaust gases from the boiler are drawn by an induced-draft fan through an electrostatic precipitator and then vented off through the chimney stack. Most modern boilers have superheaters and a reheater arrangement. A superheater is a component of a steam generating unit in which steam...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290009
EISBN: 978-1-62708-319-5
... area, powder flow and rheology, and chemical analysis. The chapter then describes the general categories of powder fabrication methods, namely mechanical comminution, electrochemical precipitation, thermochemical reaction, and phase change and atomization. It provides information on the two largest...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... Mineral processing power generation Handling ores, slurries, pulverized coal, cement clinker, and flue gas neutralizing compounds Hardness, corrosion resistance, and electrical insulation Pipe linings, cyclone linings, grinding media, pump components, electrostatic precipitator insulators Wire...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.9781627082587
EISBN: 978-1-62708-258-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230117
EISBN: 978-1-62708-298-3
.... Electrochem. Soc. , Vol 99 , p 115 – 120 10.1149/1.2779672 • Janot C. , and Gibert H. , 1972 . Mossbauer Effect Study of the Precipitation of Iron in Beryllium , Mater. Sci. Eng. , Vol 10 ( No. 1 ), p 23 – 31 10.1016/0025-5416(72)90062-6 • Kjellgren B.R.F. , Beryllium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... hydrocarbon families or from thermoset resins of the epoxy and polyester families are applied to the surface to be protected by either electrostatic spray or fluidized-bed deposition. The metal being protected is usually preheated at the time of application, and after application it is reheated to an elevated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030200
EISBN: 978-1-62708-282-2
...-solution interface. Three types of adsorption could be possible with organic inhibitors: π-bond orbital adsorption, electrostatic adsorption, and chemisorption. A more simplistic view of this mechanism of corrosion inhibitors can be described as controlled precipitation of the inhibitor from its...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870375
EISBN: 978-1-62708-344-7
... working 200 fcc Austenitic No No Yes 300 fcc Austenitic No No Yes 400 bcc Ferritic Yes No Yes 500 and precipitation hardening bcc Martensitic Yes Yes No fcc, face-centered cubic; bcc, body-centered cubic Titanium alloys (AMS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.9781627082532
EISBN: 978-1-62708-253-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060013
EISBN: 978-1-62708-261-7
... in the crystal structure of metals and their role in mechanical deformation, annealing, precipitation, and diffusion. It describes the concept of solid solutions and the effect of temperature on solubility and phase transformations. The chapter also discusses the formation of solidification structures, the use...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940087
EISBN: 978-1-62708-302-7
... ions and by electrons ( Ref 2 ). In the solution, the metal ion, being positively charged, is surrounded by oriented polar water molecules, this configuration lowering the energy of electrostatic attraction between the negative poles of the water molecules and the positive metal ion. In transferring...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
... are susceptible to severe scratching or abrasion. The disposal of spent solutions and rinse waters requires waste treatment. Hexavalent chromium must be reduced to Cr 3+ before neutralizing and precipitation. Sodium pyrosulfite (Na 2 S 2 O 5 ) is usually used as the reducing agent in smaller operations...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
... or wedgeshaped cracks at grain triple points Reaction scales or internal precipitation Some cold flow in last stages of failure Contributing factors Load exceeded the strength of the part Check for proper alloy and processing by hardness check or destructive testing, chemical analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2012
DOI: 10.31399/asm.tb.pdub.t53420363
EISBN: 978-1-62708-310-2
... and Engineering of Materials , 2nd ed. , PWS-Kent Publishing Co. , 1989 A.9 Epler M. , Structures by Precipitation from Solid Solution , Metallography and Microstructures , Vol 9 , ASM Handbook , ASM International , 2004 10.31399/asm.hb.v09.a0003731 A.10 Guy A.G. , Elements...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
... but then phase separates (i.e., precipitates) during cure. Preformed particles are advantageous because they can be used as additives or fillers. Also, their domain size is easier to control than when a phase separation process is used. Unfortunately, commercially available preformed rubber particles...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110524
EISBN: 978-1-62708-247-1
... in semiconductor lasers is electrostatic discharge (ESD) or Electrical overstress (EOS). ESD tends to involve very short pulses that are less than the thermal time-constant of the device; EOS involves longer pulses, and usually shows signs of thermal transients, such as localized melting in the device. Extensive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.9781627083447
EISBN: 978-1-62708-344-7