... review of conventional TDR and its application limitations to advanced packages in semiconductor industry. The article introduces electro optical terahertz pulse reflectometry (EOTPR) and discusses how its improvements of using high frequency impulse signal addressed application challenges and quickly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110010
EISBN: 978-1-62708-247-1
... reflectometry, and electro-optical terahertz pulse reflectometry. The final step is the step-by-step inspection and deprocessing stage that begins once the defect has been imaged. electrical verification electro-optical terahertz pulse reflectometry external optical inspection infrared microscopy IR...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110025
EISBN: 978-1-62708-247-1
... L. , Venkata M. , Tran L. , Donna W. , Qiu W. , Alton J. , Taday P.F. , and Lin M. : “ Advanced Fault Isolation Technique Using Electro-Optical Terahertz Pulse Reflectometry ,” Proc. 19th Int. Symp. Phys. Fail. Anal. Integr. Circuits (IPFA) , July 2-6, 2012...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110111
EISBN: 978-1-62708-247-1
... . Electro optical terahertz pulse reflectometry - an innovative fault isolation tool . In IEEE Electronic Components and Technology Conference , 2010 . 10.1109/ECTC.2010.5490646 [21] Elmore W. C. and Heald M. A. . Physics of Waves . Dover Publications, Inc. , New York , 1985 . [22...