1-20 of 58 Search Results for

electro-chemical plating

Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... deposition. The precipitation or plating-out of a metal from so- lutions of its salts through the introduction of another metal or reagent to the solution. chemical polishing. A process that produces a polished surface by the ac- tion of a chemical etching solution. The etching solution is com- pounded so...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
..., increased plating or paint adhesion, and for lubricity (e.g., to increase the formability of sheet metals) Chromate chemical conversion coatings Enhanced bare or painted corrosion resistance, improved adhesion of paint or other organic finishes, and provides the metallic surface with a decorative finish...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060429
EISBN: 978-1-62708-261-7
... or extrusion by from metal surfaces by chemical or electro- pouring the metal into a short mold. The base chemical reaction. of the mold is a platform that is gradually lowered while the metal solidifies, the frozen delta iron. Solid phase of pure iron that is stable shell of metal acting as a retainer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
..., submerged arc welding, and electroslag and electro-gas welding. austenitic manganese steel carbon steel cast-weld parts corrosion resistance heat resistance high alloy steel nickel-base alloys plasma arc welding steel castings weldability welding processes Introduction Welding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.9781627082617
EISBN: 978-1-62708-261-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910497
EISBN: 978-1-62708-250-1
.... The partial derivative of the total electro- chemical free energy of a constituent with respect to the number of moles of this constituent where all factors are kept constant. It is analogous to the chemical potential of a constituent except that it in- cludes the electric as well as chemical contributions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200158
EISBN: 978-1-62708-354-6
... of different compositions can be assembled in a one-piece component. Fig. 11-1 Schematic cost comparison between cast and fabricated components For successful cast-weld construction the methods of welding must be examined for their capability of producing the desired chemical composition...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170003
EISBN: 978-1-62708-297-6
... changing the chemical composition of the surface of a part by such processes as plating, cladding, nitriding, ion implantation, carburizing, and hot dip galvanizing, this book is limited to only those alloying processes that affect the bulk of the material, while surface modification is discussed in other...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... Abstract This chapter discusses coating technologies that are applicable to beryllium, including physical and chemical vapor deposition, thermal evaporation, electroplating, sputtering, ion plating, and plasma arc spraying. It describes the advantages and disadvantages of each method...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
... inspected. Electro-deposited nickel was specified for plating on the inside diameter surface. This plating is relatively soft, ductile, and has a relatively high melting point. However, electroless nickel, which has high phosphorus content, was substituted without authorization. This plating is hard...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110447
EISBN: 978-1-62708-247-1
... is playing irreplaceable role in FA root cause finding flow. Metallic electro-chemical migration, i.e., dendrite formation, occurs under very specific conditions and has common characteristics: presence of moisture between two pins under DC bias and an electrochemical process which involves moving of charged...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... are equivalent. In a square bar, the planes parallel to the hot-rolling direction are equivalent longitudinal planes. In a rectangular section or in a plate, the planar surface is parallel to the hot-working axis, has the largest surface area, and is the surface in most frequent contact with the mill rolls...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130503
EISBN: 978-1-62708-284-6
... plate. Common types of weld discontinuities illustrated in <xref ref-type="fig" rid="t51130503-f1">Fig. 1</xref> Table 1 Common types of weld discontinuities illustrated in Fig. 1 No. Discontinuity Location (a) 1 Porosity (b) W  Cluster(1b in Fig. 1 )  Piping(1d in Fig...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130043
EISBN: 978-1-62708-284-6
... of specimens, mechanical testing, macroexamination, microexamination, metallographic examination, determination of the fracture mechanism, chemical analysis, exemplar testing, and analysis and writing the report. The chapter ends with a discussion on various processes involved in the determination...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340211
EISBN: 978-1-62708-427-7
... (plate, sheet, tube, extrusion, etc.) encounter a variety of end-user operations that produce the final shape of a part. Numerous forming techniques (hot, warm, or cold) are used throughout the industry. To select or develop the correct alloy, temper, and dimensions to meet the customers’ forming...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.t52790257
EISBN: 978-1-62708-356-0
... steels and other metals and includes references to and discussions of a great many stainless steel patents. Stainless Tanks The first application of stainless steel plate for tanks takes place when a large chemical plant in the United Kingdom installs stainless steel tanks for the storage...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2010
DOI: 10.31399/asm.tb.hss.9781627083560
EISBN: 978-1-62708-356-0
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
.... chemical composition microstructure phases solidification superalloys THE MICROSTRUCTURE OF SUPERALLOYS is highly complex, with a large number of dispersed intermetallics and other phases that modify alloy behavior through their composition, morphology, and location. This chapter gives an overview...