EISBN: 978-1-62708-354-6
... Abstract This chapter discusses the following conventional molding processes for static casting: green sand molding, dry sand molding, vacuum molding, and expendable pattern casting. It also discusses core and mold processes for steel castings. The chapter provides an overview of sand molds...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740047
EISBN: 978-1-62708-308-9
..., crucible, and vacuum melting, and common casting techniques such as sand casting, plaster and shell casting, evaporative pattern casting, investment casting, permanent mold casting, cold and hot chamber die casting, squeeze casting, semisolid metal processing, and centrifugal casting. casting...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
.... In the dry sand process, resins, oil, or other chemical binding agents are used to precoat the molding sand. The dry sand mold is then thermally or chemically cured. Another dry sand method reacts carbon dioxide (CO 2 ) gas with sodium silicate in the sand blend to form a silica gel bond. The important...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370013
EISBN: 978-1-62708-447-5
... machines through the belt conveyor (18). Sand delivery to the molding sand hopper is engineered to skip the sand drying step if the moisture of the sand is at an acceptable level. Sand, clay binder (bentonite), and sea coal are mulled in the sand muller (15) and delivered to the hopper (19) above...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200001
EISBN: 978-1-62708-354-6
... or gases to form a dry hard mold. Dimensional accuracy is good, and the process is suited to all sizes of parts; however, sand reclamation costs are high, and the process is more expensive than green sand. Vacuum Molding Vacuum molding uses dry unbonded sand. The mold relies on the vacuum for its...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370021
EISBN: 978-1-62708-447-5
... Abstract This chapter focuses on the elements and functions of sand conditioning equipment which are critical to achieving good quality castings. The sand conditioning equipment include sand muller; core sand mixers; sand conveyors and bucket elevators; sand aerators; mold conveyors; shakeout...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370059
EISBN: 978-1-62708-447-5
...-setting aids. 4.1 Molding Flask Designs Smaller castings made in captive foundries are produced in green sand, especially if the castings are not intricately cored. Medium-sized castings that have multiple cores are produced in no-bake lines. Both can be produced using flaskless molding. Molding...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240095
EISBN: 978-1-62708-251-8
.... In addition, since plaster can absorb significant moisture from the atmosphere, the mold may require slow drying prior to casting. Shell molding can also be used in place of sand casting when a better surface finish or tighter dimensional control is required. Since it requires precision metal patterns...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200437
EISBN: 978-1-62708-354-6
... . . . A plate attached to a pattern to facilitate drawing of a pattern from the mold. G-4 Glossary of Foundry Terms Drum, Magnetic . . . An electrically energized pulley or drum used for removing magnetic materials from sand, nonferrous borings, and turnings, etc. Dry and Baked Compression Test A sand test...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370001
EISBN: 978-1-62708-447-5
... close to the core room, if sand drying is planned. A simple method for adding new sand to the molding sand to offset sand loss can be designed, if make-up additions are done once every two to three days. Locating the core room close to the molding shop; this will reduce handing damage to the cores...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370177
EISBN: 978-1-62708-447-5
... halves are sand blasted or blasted with dry ice at station 5 to remove the old coating. The molds are then preheated to 230 °C (450 °F) in the oven (6). The mold halves are then moved to station 7, where a manipulator or a tilt table orients the mold halves at an angle suitable for spray coating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... Abstract This chapter discusses the advantages, limitations, and applications of various aluminum casting processes, namely green sand casting process, air set or no-bake molding process, vacuum molding process, evaporative foam casting process, and die casting process. The processes covered...
Book

By Jagan Nath
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320323
EISBN: 978-1-62708-332-4
... is the most common for gray iron, malleable iron, and ductile iron for both molds and cores. Small and medium steel castings are produced in silica sand. Medium to larger steel castings are produced in olivine sand. Thick-walled and very heavy steel castings use chromite and zircon sands at areas prone...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
... The engineering design of the gating system is a critical process element that influences both surface quality and internal integrity of the castings. Anomalies such as laps, slag inclusions, gas cavities, sand erosion, mold spalling, and shrinkage can be avoided if gating and venting systems are properly...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200164
EISBN: 978-1-62708-354-6
.... A number of factors should be considered in the construction and design of the pattern, for example: the molding method used by the foundry (e.g., green sand, air set, etc.), parting line, coring, and risering and gating techniques used. Definitions In discussing pattern equipment with foundrymen...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370187
EISBN: 978-1-62708-447-5
... molding process. The low-pressure semipermanent molding process uses steel molds with expendable sand cores, like the gravity semipermanent molding process. The process applications range from decorative automotive wheels to critical safety components for automotive chassis (substructure) and complex...
Book

By Jagan Nath
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.9781627084475
EISBN: 978-1-62708-447-5
Book

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6