Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290001
EISBN: 978-1-62708-319-5
... dimensional specifications, as well as organic shapes Tailored porosity or embedded cooling channels Sorting through these options and factors involves experience. To introduce the ideas, Table 1.1 is an outline of key component features. Several pictures of target components are shown in Fig...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
.... Techniques in this area include visual examination, low-power magnification, optical and scanning electron microscopy, and photography. Dimensional inspection and related approaches for assessing suspected item dimensions and conformance to drawing and specification requirements and determining...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200206
EISBN: 978-1-62708-354-6
... Abstract Users of steel castings establish performance requirements for specific characteristics of the castings based on the planned use. They express tolerance for variation in those characteristics to the producer of the castings. One issue which should never be taken for granted...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200078
EISBN: 978-1-62708-354-6
... Shipping instructions Terms of payment If sample castings are required, the following additional requirements should be provided: Number of samples required Non-destructive examination requirements, if any, and applicable specifications with acceptance standards Dimensional examination...
Image
Published: 01 December 2003
Fig. 12 In-mold cooling time versus wall thickness predicted from one-dimensional, transient mold cooling analysis Material Unfilled PC Thickness, mm 1.62–3.81 Thermal conductivity, W/m · K 0.270 Specific heat, W · s/kg · K 1791 Melt temperature, °C 300 Mold More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200197
EISBN: 978-1-62708-354-6
..., and applicable specifications, will dictate the order and extent of these activities. The operations listed above will be reviewed in this chapter. Casting inspection takes place on several occasions and dictates the extent of remedial operations such as upgrading, dimensional adjustment, and surface finishing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140061
EISBN: 978-1-62708-335-5
... heat treatment, quenching, precipitation hardening, and annealing of aluminum alloys. The effects of these processes on dimensional stability and residual stresses are also discussed. Troubleshooting and diagnosis of heat treating problems are covered in the concluding section of the chapter...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870265
EISBN: 978-1-62708-299-0
... cracking or exfoliation corrosion. It applies to cast products that are artificially aged after solution heat treatment to provide dimensional and strength stability. T8, Solution Heat Treated, Cold Worked, and Artificially Aged This designation applies to products that are cold worked specifically...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... for densification and dimensional correction, followed by finishing operations. The finishing operations include machining, case and through hardening, steam treatment, and so on (Ref 1) . This chapter reviews failure aspects of structural ferrous PM parts, which form the bulk of the PM industry. Focus...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780075
EISBN: 978-1-62708-268-6
... is comprised of engineering drawings, specifications, process descriptions, test results, inspection data, and other documentation. Evaluating the pedigree of a failed product can help to rule in or rule out hypothesized failure causes. The documents making up a product pedigree are records of how...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200001
EISBN: 978-1-62708-354-6
... required by a purchaser to meet his specifications. Casting Process The manufacture of steel castings is discussed in this handbook, however, a simplified flow diagram ( Figures 1-1 and 1-2 ) is shown to give an overview of the process steps. Fig. 1-1 Simplified flow diagram of the basic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410253
EISBN: 978-1-62708-280-8
..., product launch, and continuous improvement. This is followed by sections covering product-process flow diagrams and also the process elements considered for process failure mode and effects analysis. Some of the aspects covered by the engineering specifications to meet the product performance requirements...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 1998
DOI: 10.31399/asm.tb.ts5.t65900325
EISBN: 978-1-62708-358-4
... or to bainite or martensite after cooling from tempering temperatures. The chapters on the various tool steels have presented examples of the dimensional changes that occur during tempering of specific tool steels, and Fig. 17-22 and 17-23 show, respectively, changes in dimensions of hardened D2 and H13...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720049
EISBN: 978-1-62708-305-8
... Abstract The coordinate measuring machine (CMM) is used for three-dimensional inspection of both in-process and finished parts. This chapter provides a detailed account of the operating principles, measurement techniques, capabilities, and applications of CMMs. The types of CMMs are described...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040001
EISBN: 978-1-62708-300-3
... Abstract This chapter provides a brief introduction to manufacturing processes used to produce metal parts and how they differ in terms of achievable geometries, tolerances, surface finishes, and production rate. manufacturing process dimensional accuracy surface roughness 1.1...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720021
EISBN: 978-1-62708-305-8
... and extreme close-up photography. Measuring Devices Measuring devices are considered part of visual examination because they are used to record the results of the examination. Visual examination, among other purposes, includes checking to see if parts meet dimensional specifications. These devices...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200065
EISBN: 978-1-62708-354-6
... the material specification (preferably ASTM) which meets the mechanical test property requirements, and whose scope encompasses the service for which the part is intended. The necessary quality level can then be established by specifying special inspection procedures and dimensional tolerances. Table 4-1...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780147
EISBN: 978-1-62708-268-6
.... Engineering drawings typically define dimensional and material requirements but not performance, reliability, safety, and other requirements, which are typically defined in specifications. The failure analysis team should review with the engineers exactly what requirements the product is supposed to meet...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
... of the important goals of the parts producer is to consistently reproduce that dimensional change that has been designed or factored into the size of the compacting die, in order to be able to meet print size specifications. This is normally done by advance testing of the powder under closely monitored conditions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250139
EISBN: 978-1-62708-345-4
.... Inspection and testing is done on dimensional specifications, mechanical properties, and surface durability (hardness). The information required to describe a gear for the P/M process and subsequent inspection methods are essentially the same as for a machine-cut gear. The part drawing should include...