Skip Nav Destination
Close Modal
Search Results for
die casting machines
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 315 Search Results for
die casting machines
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 December 2018
Image
Published: 01 December 2018
Image
Published: 01 November 2013
Fig. 27 Schematic showing the principal components of a hot chamber die casting machine. Source: Ref 6
More
Image
Published: 01 November 2013
Fig. 28 Schematic showing the principal components of a cold chamber die casting machine. Source: Ref 6
More
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
.... Figure 4.4 is a schematic of a horizontal cold chamber die casting machine. The die casting machine consists of a hollow shot sleeve (a hollow cylinder into which metal is poured) with a pouring slot and a hydraulically actuated plunger (with an intensifier). The shot sleeve fits into an opening...
Abstract
This chapter discusses the advantages, limitations, and applications of various aluminum casting processes, namely green sand casting process, air set or no-bake molding process, vacuum molding process, evaporative foam casting process, and die casting process. The processes covered also include gravity permanent molding, low-pressure permanent molding, counter pressure, squeeze casting, investment casting, rapid prototype casting, cast forge hybrid, and semisolid metal processes.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410103
EISBN: 978-1-62708-280-8
... of it are covered in section 6.2.11 , in this chapter. Die Cavity Positioning The die cavity should be positioned to: Lay out the die cavity within the tie bars of the die casting machine and the center of the shot sleeve. Maintain a clearance of a minimum 25 mm (1 in.) between the tie bar traverse...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
... costs, though significant, become less important. As volume requirements increase, the trend is toward automated molding processes, permanent molds, and die casting. For extended production in die and permanent mold operations, more expensive, difficult-to-machine tool steels provide improved life...
Abstract
This chapter begins with information on the historical development of aluminum alloy castings. It then covers the basic factors involved in the selection of a casting process. This is followed by sections describing the various categories of casting processes and their variants: expendable mold gravity-feed casting, nonexpendable (permanent) mold gravity feed casting, and pressure die casting. Next, the chapter describes the technologies used to produce premium engineered castings and when such castings may be relevant. The chapter concludes with descriptions of other process technologies used with castings, including metallurgical bonding, metal-matrix composites, and hot isostatic pressing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740047
EISBN: 978-1-62708-308-9
..., crucible, and vacuum melting, and common casting techniques such as sand casting, plaster and shell casting, evaporative pattern casting, investment casting, permanent mold casting, cold and hot chamber die casting, squeeze casting, semisolid metal processing, and centrifugal casting. casting...
Abstract
This chapter covers the practices and procedures used for shape casting metals and alloys. It begins with a review of the factors that influence solidification and contribute to the formation of casting defects. It then describes basic melting methods, including induction, cupola, crucible, and vacuum melting, and common casting techniques such as sand casting, plaster and shell casting, evaporative pattern casting, investment casting, permanent mold casting, cold and hot chamber die casting, squeeze casting, semisolid metal processing, and centrifugal casting.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250129
EISBN: 978-1-62708-345-4
... with a variety of steels, bronzes, and aluminum alloys. With machinable materials, the process is still useful if the gear is integral with some complicated shape that is very difficult to produce by machining. Large quantities of small, low-cost gears are made by the cold chamber die casting process (die...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
... and fatigue strength Zinc 1.0–3.0% in die casting alloys: reduces die soldering, 0.1% max in primary and 0.3% max in secondary, increases corrosion Chromium 0.15% max: reduces machinability 5.3 Alloys for Gravity and Low-Pressure Permanent Molds, Squeeze and Die Casting Table 5.3...
Abstract
This chapter is a collection of tables listing: cast alloy designations of Aluminum Association, along with their general applications; the chemical compositions of the frequently used alloys for gravity permanent molds, low-pressure permanent molds, squeeze castings, and die castings; the typical tensile properties of die cast alloys; and the designations of different heat treatments and their description. The tables also list the temperatures and times of typical heat treatment cycles for different permanent mold cast alloys; typical components in sand, gravity, and low-pressure permanent mold castings and die castings, the functional requirements of each process, and the corresponding suitable alloys and heat treatments; and alloys that are high vacuum die cast for structural castings. The chapter also presents examples of photomicrographs of some alloys cast by different processes.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410247
EISBN: 978-1-62708-280-8
... mold casting D 712 F Machine tools and other machinery Machine tool beds, coordinate measuring machines, wood working machinery V-process casting, air set sand casting 356 T6 Marine products Piping, valves Die casting A 518 F Pistons, connecting rods, housings Die casting A 413 F...
Abstract
This chapter presents guidelines for product designers to choose the best process and alloys while designing a casting. The discussion covers some of the factors pertinent to the selection of the best process for the product function and performance, namely geometric factors, mechanical properties, tooling cost per piece, and overall cost factors. The chapter contains tables listing several markets, products, popular processes, and common alloys and the common processes used for a variety of markets and products.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170520
EISBN: 978-1-62708-297-6
... lb) of die cast parts. Zinc castings are also extensively used in general hardware and electronic and electrical fittings of all kinds, including parts for domestic appliances (for example, washing machines, vacuum cleaners, mixers, and so on), oil burners, motor housings, locks, and clocks. Zinc...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... for the inner diameter, outer diameter, and length. Depending on the production quantity, the options are green machining, cold isostatic pressing, die compaction, and extrusion. Tape casting is best for thin, flat shapes. Die compaction is best for squat (low length-to-diameter ratio) or stepped shapes...
Abstract
The conversion of feedstock into a shape involves the application of heat and pressure, and possibly solvents. This chapter discusses the operating principle, advantages, limitations, and applications of such shaping processes, namely additive manufacturing, cold isostatic pressing, die compaction, extrusion, injection molding, slip casting, slurry processes, and tape casting. Information on equipment setup, requirements, and the various factors influencing these processes are described. In addition, the chapter provides information on novel approaches and processing costs applicable to these shaping processes.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400129
EISBN: 978-1-62708-316-4
..., dimensional accuracy, and stiffness as well as die change procedures. forming presses sheet metal forming EACH SHEET FORMING PROCESS is associated, in a practical sense, with at least one type of sheet forming machine or equipment. The sheet forming equipment varies by the rate at which energy...
Abstract
This chapter discusses the design and application of sheet forming presses. The discussion covers critical variables and design parameters, key components, basic machine configurations, and energy and load requirements. The chapter also discusses time-dependent characteristics, dimensional accuracy, and stiffness as well as die change procedures.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... casting LC A A A A A LC LC LC A LC Die casting NA NA NA NA A LC A A NA NA NA Impact extrusion NA A A LC A A A LC NA NA NA Cold heading NA A A A A A LC LC NA LC NA Closed die forging NA A A A A A NA A A LC LC Pressing and sintering (PM...
Abstract
This chapter describes the processes involved in the fabrication of wrought and cast metal products. It discusses deformation processes including bending and forming, material removal processes such as milling, cutting, and grinding, and joining methods including welding, soldering, and brazing. It also discusses powder consolidation, rolling, drawing and extrusion, and common forging methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550141
EISBN: 978-1-62708-307-2
... in composition can affect cost of heat treatment. Casting cost is also influenced by required tolerances, mold and die costs, and machining costs. The quantity of a part to be produced is an important factor affecting cost and must be considered in selecting the most economical method of production. Magnesium...
Abstract
Magnesium, by volume, is two-thirds the weight of aluminum and one-quarter the weight of steel. It also has good damping capacity, giving it an edge over other metals in high-vibration environments. This chapter discusses the basic metallurgy, alloy designations, compositions, and mechanical properties of cast and wrought magnesium alloys. It also describes the processes used to produce magnesium parts, the causes and effects of corrosion, and the use of protective coatings and treatments.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140253
EISBN: 978-1-62708-335-5
... casting rotating-beam fatigue curve. Smooth specimens from one lot. Specimen per Fig. A3.4, Appendix 3 . Fig. D6.90 380.0-F, die cast aluminum casting rotating-beam fatigue curve. Smooth specimens from one lot. Specimen per Fig. A3.4, Appendix 3 , as cast. Machined to nominal diameters...
Image
Published: 01 November 2013
Fig. 29 Components of a single-cavity die casting die for use in a hot chamber machine. Source: Ref 6
More
1