... Abstract After shaping and first-stage binder removal, the component (with remaining backbone binder) is heated to the sintering temperature. Further heating induces densification, evident as dimensional shrinkage, pore rounding, and improved strength. This chapter begins with a discussion on...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140055
EISBN: 978-1-62708-335-5
... • Diem M.M. and Mashi S.J. , Simultaneous Densification and Solution Heat Treatment of Aluminum Castings , Proc. International Symposium of Aluminum Applications: Thrusts and Challenges, Present and Future , ASM Materials Solutions Conference ( Pittsburgh, PA ), Oct 2003 Hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140055
EISBN: 978-1-62708-335-5
... • Diem M.M. and Mashi S.J. , Simultaneous Densification and Solution Heat Treatment of Aluminum Castings , Proc. International Symposium of Aluminum Applications: Thrusts and Challenges, Present and Future , ASM Materials Solutions Conference ( Pittsburgh, PA ), Oct 2003 Hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
... Content and Mechanical Properties of 17-4 PH Stainless Steel Fabricated by PIM Process and Sintering , Met. Mater. Int. , Vol 12 , 2006 , p 101 – 106 10.1007/BF03027464 12. Kwon Y.S. , Wu Y. , Suri P. , and German R.M. , Simulation of the Sintering Densification and Shrinkage...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
.... , Vol 43 , 2000 , p 233 – 237 10.1179/003258900665998 • Li C. , Zhou Y. , Xie Y. , Zhou D. , and Zhang D. , Effects of Milling Time and Sintering Temperature on Structural Evolution, Densification Behavior, and Properties of a W-20wt%Cu Alloy , J. Alloy. Compd. , Vol...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230267
EISBN: 978-1-62708-298-3
... intermediate forms that will be further worked into mill products, such as extrusions, sheet, foil, and wire. The ease in consolidating normal-purity grades of beryllium is related to the oxide coating and contaminants, especially silicon. Silicon is a sintering aid that permits full densification of the...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000039
EISBN: 978-1-62708-312-6
.... , Jandesha W. Jr. , Sanderow H. , Vol 7 , MPIF , 2002 , p 7 - 127 to 7 - 126 11. Takeda T. and Tamura K. , Densification of Stainless Steel Powder Compacts Powder During Sintering , J. Jpn. Soc. Powder Met. , Vol 17 ( No. 5 ), Jan 1971 , p 28 – 36 10.2497/jjspm...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
...: Powder mixing (matrix and reinforcement) Green body fabrication Machining if required Binder removal Consolidation and densification Inspection The process flow for the powder method is shown in Fig. 21.7 . A uniform, fine dispersion of the reinforcement and matrix powder helps...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... densification and dimensional correction, followed by finishing operations. The finishing operations include machining, case and through hardening, steam treatment, and so on (Ref 1) . This chapter reviews failure aspects of structural ferrous PM parts, which form the bulk of the PM industry. Focus is on...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
... (NASA) and the locations of the turbopump and blisk. The blisks were produced by CVI of a woven preform, which was subsequently machined and thermally treated to complete densification. The final turbopump assembly is shown in Fig. 11.17 . Exhaust nozzle flaps and seals . Ceramic-matrix composites...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... beryllium and the deposit parallel to the spray direction, although the latter increased at a slower rate ( Fig. 22.29 ) [ Castro et al. 1998 ]. This was attributed to the interaction between contiguous splat layers. At the elevated temperature, some densification occurred. For many purposes, the as-sprayed...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... Handbook Desk Edition , ASM International , 1995 10.31399/asm.hb.emde.a0003053 10.12 Densification and Sintering of Ceramics , Engineered Materials Handbook Desk Edition , ASM International , 1995 10.31399/asm.hb.emde.a0003054 10.13 Joining Ceramics , Engineered Materials Handbook Desk...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280117
EISBN: 978-1-62708-267-9
... properties that some designers prefer. While direct isothermal powder superalloy forging might be preferred for cost reasons, the use of powder billets and/or preforms ensures that full densification has been achieved and that reasonable amounts of deformation energy have been applied to the metal before the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460173
EISBN: 978-1-62708-285-3
... from compounds or solutions. The remelting process by induction plasma technology leads to powder densification and spheroidization. It essentially consists of in-flight heating and melting of feed material particles followed by cooling and solidification under controlled conditions. A wide...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
.... Postsolidification densification: Hot isostatic processing (HIP) of castings can result in improved levels of internal soundness, higher tensile properties, ductility, and fatigue performance. The physical and mechanical properties of aluminum castings may be altered through: Unlike most sources, the...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290001
EISBN: 978-1-62708-319-5
.... Because of the densification, the component shrinks to approach full density. On cooling, the sintered component is then ready for finishing operations, such as heat treating, painting, electroplating, machining, or polishing. The idea of shaping an object from powder, using a transient binder phase...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
... and fatigue performance. Heat treatment: Mechanical properties can be altered by postsolidification thermal treatment, including annealing, solution heat treatment, and precipitation aging. Postsolidification densification: Hot isostatic processing (HIP) of castings can result in improved...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740373
EISBN: 978-1-62708-308-9
... employed technique for producing P/M parts. The processing steps are shown in Fig. 20 . Fig. 20 General steps in the P/M process. Source: Ref 9 As a metal powder deforms during compaction, its hardness increases (work hardens), and its rate of densification decreases with increasing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480161
EISBN: 978-1-62708-318-8
... densification by hot isostatic pressing (HIP) ( Ref 8.6 ). The good mechanical properties of titanium alloy castings are a result of the high cleanliness of titanium castings, the ability to close and completely heal pores by the HIP operation (essentially, diffusion bond surfaces together to give a...