1-20 of 31 Search Results for

degenerate problem tests

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060155
EISBN: 978-1-62708-343-0
... for treating multiaxiality, a concise listing of the rules, and an example problem in which axial creep-fatigue data is used to predict the torsional creep-fatigue life of type 304 and 316 stainless steel. The chapter also includes a brief introduction in which the authors outline the challenges presented...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560005
EISBN: 978-1-62708-291-4
... Abstract This chapter discusses the development of the nomenclature used to describe the constitution and structure of metals and alloys, particularly the phases observed in the microstructure of steel. It also points out some of the problems with current nomenclature and provides...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560221
EISBN: 978-1-62708-291-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060069
EISBN: 978-1-62708-343-0
... Abstract This chapter demonstrates the versatility of the strain-range partitioning method and its application to creep-fatigue problems involving complex loading histories. It begins with a derivation showing that it is possible to assess the damage of hysteresis loops combining two or more...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
... vendors and Advanced General Aviation Transport Experiments (e.g., Ref 8.9 ). The problem is resolved, to some extent, with the selection of easy-to-use test techniques for subscale testing. The purpose of this chapter is to describe suitable mechanical test techniques for characterizing laminated...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060021
EISBN: 978-1-62708-343-0
... a large collection of creep-rupture data corresponding to different alloy designations and heat treatments, identifying key relationships, similarities, and differences. It also presents a test method developed by the authors in which twelve materials are tested over a range of temperature, stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490183
EISBN: 978-1-62708-340-9
... life based on dimensional measurements; methods based on metallographic studies; methods based on temperature estimates; and a method for estimating remaining life under creep conditions based on stress-rupture testing of service-exposed material samples. The chapter also discusses the use of fracture...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.9781627083409
EISBN: 978-1-62708-340-9
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780204
EISBN: 978-1-62708-281-5
... initiation, the kinetics of craze growth, and the effect of crazing on toughness of the plastic. In addition, the article provides information on various tests to determine stress-to-craze value, strain-to-craze value, and fracture toughness of the plastic. ductile-brittle transitions crazing...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870201
EISBN: 978-1-62708-344-7
... infinity at a stress-intensity range that approaches the fracture toughness. However, the equation doesn’t degenerate properly to the Paris-Erdogan equation for the test condition used by these investigators. An alternate empirical equation has been proposed in the form: (Eq 9.6) d a d N...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.9781627083386
EISBN: 978-1-62708-338-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.9781627083447
EISBN: 978-1-62708-344-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110153
EISBN: 978-1-62708-247-1
...). Rework removal of the part from the motherboard or test card for preparation should be considered carefully. Once thinned, will the part survive the strain of reflow or test sockets? Will all the balls still make electrical contact in the socket after thinning due to added warpage of the package...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400087
EISBN: 978-1-62708-258-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Book Chapter

By L. L. Sparks
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860047
EISBN: 978-1-62708-348-5
... in the crystal lattice. The transport of heat and electrical currents by electrons was, at least qualitatively, explained using this approach. However, a major problem was created in the understanding of the specific heat of metallic conductors. If the electrons were treated as free electrons (independent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560081
EISBN: 978-1-62708-291-4
... with structural changes that can be detected by light microscopy. It is not our purpose to discuss the factors involved in any detail, but the later discussion of the microstructural features that do influence these properties will be assisted if the important principles are outlined. The general problem...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560039
EISBN: 978-1-62708-291-4
... structure, which in this instance, can be described as a partly degenerate pearlite ( Fig. 4.2 (Part 1) c ). However, the duplex constituent is not produced in the rim layers, but instead, thin films of cementite form at ferritic grain boundaries ( Fig. 4.2 (Part 1) b ). These films are a fully degenerate...