... Abstract This chapter discusses the effects of metallurgical variables on dealloying corrosion. It begins by describing the processes involved in dealloying of metal alloys in aqueous environments. This is followed by a discussion on the morphology of porous dealloyed structures below and above...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... Abstract This chapter discusses common forms of corrosion, including uniform corrosion, galvanic corrosion, pitting, crevice corrosion, dealloying corrosion, intergranular corrosion, and exfoliation. It describes the factors that contribute to stress-corrosion cracking, hydrogen embrittlement...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
..., fretting corrosion, intergranular corrosion, exfoliation, dealloying corrosion, stress-corrosion cracking, and corrosion fatigue. The chapter discusses the processes involved in corrosion control by retarding either the anodic or cathodic reactions. The rate of corrosion is reduced by conditioning...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... corrosion; galvanic corrosion; erosion-corrosion, including cavitation erosion and fretting corrosion; intergranular corrosion, including sensitization and exfoliation; dealloying; environmentally assisted cracking, including stress-corrosion cracking, corrosion fatigue, and hydrogen damage (including...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350011
EISBN: 978-1-62708-315-7
... and exfoliation Dealloying Environmentally assisted cracking, including stress-corrosion cracking (SCC), corrosion fatigue, and hydrogen damage (including hydrogen embrittlement, hydrogen-induced blistering, high-temperature hydrogen attack, and hydride formation) Figure 3 illustrates schematically...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030003
EISBN: 978-1-62708-282-2
... Abstract This chapter provides an introduction to various forms of corrosion, namely uniform corrosion, localized corrosion, mechanically assisted degradation, environmentally induced cracking, microbiologically influenced corrosion, and metallurgically influenced corrosion. uniform...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030126
EISBN: 978-1-62708-282-2
... Abstract This chapter focuses on stress-corrosion cracking (SCC) of metals and their alloys. It is intended to familiarize the reader with the phenomenological and mechanistic aspects of stress corrosion. The phenomenological description of crack initiation and propagation describes well...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910497
EISBN: 978-1-62708-250-1
... deactivation. The process of prior removal of the active corrosive con- stituents, usually oxygen, from a corrosive liquid by controlled cor- rosion of expendable metal or by other chemical means, thereby making the liquid less corrosive. dealloying. The selective corrosion of one or more components of a solid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090001
EISBN: 978-1-62708-266-2
... in the formation of a film on the metal surface. These films may be passivating layers, tarnish films, or dealloyed layers. In many cases, these films reduce the rate of general or uniform corrosion, making the alloy desirable for resistance to uniform corrosion in the environment. As a result, SCC is of greatest...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090221
EISBN: 978-1-62708-266-2
... Abstract This chapter describes the conditions under which copper-base alloys are susceptible to stress-corrosion cracking (SCC) and some of the environmental factors, such as temperature, pH, and corrosion potential, that influence crack growth and time to failure. It explains that, although...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030380
EISBN: 978-1-62708-282-2
... constituents, usually oxygen, from a corrosive liquid by controlled corrosion of expendable metal or by other chemical means, thereby making the liquid less corrosive. dealloying. The selective corrosion of one or more components of a solid solution alloy. Also called parting or selective leaching. See also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... require metallographic examination for evidence of dealloying, stress-corrosion cracking (SCC), intergranular corrosion, and other corrosion phenomena. Nonmetallic materials, such as thermoplastics, coatings, reinforced thermosetting resins, elastomers, and ceramics, are also evaluated in laboratory...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030070
EISBN: 978-1-62708-282-2
... Abstract This chapter describes the effects of metallurgical variables on the corrosion of aluminum alloys. Emphasis is placed on the effect of constituent particles on pitting corrosion of aluminum. corrosion aluminum alloys aluminum THE METALLURGICAL EFFECTS on corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... Abstract All materials are susceptible to corrosion or some form of environmental degradation. Although no single material is suitable for all applications, usually there are a variety of materials that will perform satisfactorily in a given environment. The intent of this chapter is to review...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... the process. D dealloying. The selective corrosion of one or more components of a solid- solution alloy. Also called parting or selective leaching. See also dezin- cification and graphitic corrosion. degreasing. The removal of grease and oils from a surface. Can be ac- complished by immersion in liquid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030039
EISBN: 978-1-62708-282-2
... Crevice corrosion shares many characteristics and phenomenology with other forms of localized corrosion such as pitting, intergranular attack, environmentally assisted cracking, and dealloying. In all of those cases, the electrochemical and chemical conditions within an occluded region become altered...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
... corrosion Intergranular corrosion, including sensitization and exfoliation Dealloying, including dezincification and graphitic corrosion Environmentally assisted cracking, including stress-corrosion cracking, corrosion fatigue, and hydrogen damage In theory, the eight forms of corrosion...