Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870123
EISBN: 978-1-62708-344-7
... with the irreversible hardening of type 304 stainless steel. crack initiation cumulative fatigue damage analysis damage curve irreversible hardening linear damage rule Introduction Linear Damage Rule (LDR) and Its Limitations Treatment of Loading-Order Effects by a Double Linear Concept Predicated...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060231
EISBN: 978-1-62708-343-0
... G.R. , Re-Examination of Cumulative Fatigue Damage Analysis—An Engineering Perspective , Eng. Fract. Mech. , Vol 25 (No. 5/6) , 1986 , p 539 – 571 10.1016/0013-7944(86)90022-6 10.11 Manson S.S. and Halford G.R. , Practical Implementation of the Double Linear Damage Rule...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870075
EISBN: 978-1-62708-344-7
... of Cumulative Fatigue Damage Analysis for Cold End Rotating Structures, preprint 79-1190 , AIAA/SAE/ASME 15th Joint Propulsion Conference , (Las Vegas, NV) , June 18 – 20 , 1979 4.16 Manson S.S. and Halford G.R. , Correction to: Practical Implementation of the Double Linear Damage Rule...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610303
EISBN: 978-1-62708-303-4
... the damage tolerance requirements used by different industries, and discusses various approaches for fatigue design. References References 1. Broek D. , Concepts of Fracture Control and Damage Tolerance Analysis , Fatigue and Fracture , Vol 19 , ASM Handbook , ASM International , 1996...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060173
EISBN: 978-1-62708-343-0
... component design 8.86 ABD ITC Interactive time-cycle fractions 8.78 ABD RCF Relaxation creep fatigue 8.87 ABE CDC Cumulative damage under creep 8.88 ABDE PFC Phenomenological fatigue creep 8.89 AE FCD Fatigue + creep damage mechanisms 8.90 A FNC French Nuclear...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870179
EISBN: 978-1-62708-344-7
...-67, Society of Automotive Engineers (SAE) , Warrendale, PA , 1997 8.20 Walcher J. Gray D. and Manson S.S. , “Aspects of Cumulative Fatigue Damage Analysis of Cold End Rotating Structures,” American Institute of Aeronautics and Astronautics preprint 79-1190 , 1979...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490265
EISBN: 978-1-62708-340-9
... can be used, whereas in other cases a complex finite-element analysis may be required. The Schlottner and Seeley method provides a unique way of estimating damage based on time life fractions using a strain-exhaustion criterion. LCF Life Expenditure in Pure Fatigue For pure-fatigue conditions...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870001
EISBN: 978-1-62708-344-7
... served by a different formulation from that used for body-centered cubic metals. Cumulative fatigue damage—that is, when a specimen or part is subjected to several loading levels throughout its life—is the subject of Chapter 6 . There had long been an objective in research circles to be able...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240243
EISBN: 978-1-62708-251-8
... Cumulative Damage 14.5 Fatigue Crack Nucleation and Growth 14.6 Fatigue Crack Propagation 14.7 Crack Closure 14.8 Geometrical Stress Concentrations 14.9 Manufacturing Stress Concentrations 14.10 Environmental Effects 14.11 Fatigue Life Improvement 14.12 Fatigue Design Methodologies...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540383
EISBN: 978-1-62708-309-6
..., and back to ground taxi must be defined for a fatigue analysis. This stress variation, or GAG cycle, is one of the most important contributors to structural fatigue damage. Figure A4.1 illustrates two GAG cycle definitions commonly used in fatigue analysis: the mean-to-mean GAG cycle and the once...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540121
EISBN: 978-1-62708-309-6
...Abstract Abstract This chapter examines the stress-strain characteristics of metals and alloys subjected to cyclic loading and the cumulative effects of fatigue. It begins by explaining how a single load reversal can lower the yield stress of a material and how repeated reversals can cause...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.9781627083447
EISBN: 978-1-62708-344-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630117
EISBN: 978-1-62708-270-9
... Life with Particular Emphasis on Cumulative Damage , Metal Fatigue , Sines G. and Waisman J.L. , Ed., McGraw-Hill , 1959 , p 278 – 292 4. Fractography and Atlas of Fractographs , Vol 9 , Metals Handbook , 8th ed. , American Society for Metals , 1974 , p 68 – 70 , 85 – 89...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060069
EISBN: 978-1-62708-343-0
..., “Cumulative Fatigue Damage,” of the companion volume ( Ref 4.6 ), however, when loadings of very different magnitudes are involved, a linear damage accumulation approach can yield unconservative results in some cases. Strictly speaking, a nonlinear damage rule, such as the Double Linear Damage Rule, should...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610147
EISBN: 978-1-62708-303-4
... , SAE. Source: Ref 11 Fig. 21 Log strain versus log reversals to failure. Source: Ref 11 Fig. 27 Cumulative damage during high-to-low loading sequence. Source: Ref 14 Fig. 28 Development of extrusions and intrusions during fatigue crack initiation. Source: Ref 8...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320189
EISBN: 978-1-62708-347-8
.... , “Bending Strength of Spur and Helical Gear Teeth,” Fall Technical Meeting , American Gear Manufacturers Association , 1967 • Miner M.A. , Cumulative Damage in Fatigue , J. Appl. Mech. , Vol 12 , 1945 10.1115/1.4009458 • Oda S. , Shimatomi Y. , and Nobuyuki K...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.9781627083478
EISBN: 978-1-62708-347-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490059
EISBN: 978-1-62708-340-9
... to estimate cumulative damage under changing conditions, and how to assess the effect of multiaxial stress based on uniaxial test data. It also includes information on rupture ductility, creep fracture, and creep-crack growth and their effect on component life and performance. References References 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490183
EISBN: 978-1-62708-340-9
... ash Oil ash Erosion Fly ash Falling slag Sootblower Coal particle Fatigue Vibration Thermal Corrosion Lack of quality control Maintenance cleaning damage Chemical excursion damage Material defects Welding defects Stress-Rupture Failures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270005
EISBN: 978-1-62708-301-0
... of the prosthesis and failure analysis, it was found that a crack had nucleated on a microweld on the surface of the implant and propagated by fatigue. It was found that the prosthesis had been made by an ordinary casting process and the surface porosity was covered by repair welding. Defective repair welding...