Skip Nav Destination
Close Modal
Search Results for
cryogenic steel casting
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 135 Search Results for
cryogenic steel casting
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200311
EISBN: 978-1-62708-354-6
... high alloy steels. austenitic high alloy steel casting cryogenic steel casting ferritic carbon steel casting low-temperature steel casting martensitic high alloy steel casting martensitic low alloy steel casting Opening image for Chapter 23, “Low-Temperature and Cryogenic Steels...
Abstract
This chapter defines low-temperature and cryogenic steels and describes their alloy classifications and their ambient and low-temperature properties. These steels include ferritic carbon and low alloy steels, martensitic low alloy steels, martensitic high alloy steels, and austenitic high alloy steels.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860371
EISBN: 978-1-62708-348-5
...) , and Mazandarany, Parker, Koenig, and Read (1980) . Mazandarany et al. found that postweld annealing at 1040° C improved the 4-K K Ic ( J ) properties of 316L SM A weld deposits. Castings Austenitic stainless steel castings are used for cryogenic equipment having heavy sections or complex geometries...
Abstract
This chapter discusses the structural alloys being used for cryogenic applications in commercially significant quantities. It emphasizes the practical considerations involved in the material selection process and provides the information necessary to make preliminary selections of alloys most suitable for the intended cryogenic application. The chapter provides general information on a class or group of alloys, their representative mechanical and physical properties, and their fabrication characteristics. The materials covered are austenitic stainless steels, nickel steels, aluminum alloys, and other metals and alloys.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170242
EISBN: 978-1-62708-297-6
... . Standard composition ranges for austenitic manganese steel castings Table 1 Standard composition ranges for austenitic manganese steel castings ASTM A 128 grade Composition, % C Mn Cr Mo Ni Si (max) P (max) A 1.05–1.35 11.0 min … … … 1.00 0.07 B-1 0.9–1.05 11.5–14.0...
Abstract
This article provides an overview of austenitic manganese steels. It describes the standard composition ranges of commercial products and explains how various alloying elements affect mechanical properties, processing, and performance. The article also discusses special grades of manganese steels and the types of applications for which they have been developed.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860269
EISBN: 978-1-62708-348-5
..., notably carbon and low-alloy steels, become brittle at low temperatures. Therefore, many cryogenic structures require the use of conservative design procedures to ensure adequate structural safety. The prevention of brittle fracture is an important consideration because of the sudden and uncontrolled...
Abstract
This chapter reviews the concepts of fracture mechanics and their application to materials evaluation and the design of cryogenic structures. Emphasis is placed on an explanation of technology, a review of fracture mechanics testing methods, and a discussion on the many factors contributing to the fracture behavior of materials at cryogenic temperatures. Three approaches of elastic-plastic fracture mechanics are covered, namely the crack opening displacement, the J-integral, and the R-curve methods. The chapter also discusses the influence of thermal and metallurgical effects on toughness at low temperatures.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440001
EISBN: 978-1-62708-262-4
..., and the heating portion of the process must produce a homogeneous austenitic phase. The actual temperature used depends on the composition of the steel, but the usual temperature is approximately 870 °C (1600 °F). Because of characteristics inherent in cast steel, normalizing is commonly applied to ingots prior...
Abstract
This chapter introduces the principal heat treating processes, namely normalizing, annealing, stress relieving, surface hardening, quenching, and tempering. An overview of four of the more popular surface hardening treatments, namely carburizing, carbonitriding, nitriding, and nitrocarburizing, is provided.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310243
EISBN: 978-1-62708-286-0
.... The stiff corrugated bulkheads are themselves structural strengtheners for the entire ship. The vertical corrugations also facilitate tank cleaning as internal stiffeners are eliminated. Cryogenic containers are still the bastion of austenitic stainless steels. As leaner austenitic alloys have become...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.pnfn.t65900119
EISBN: 978-1-62708-350-8
... Casting Part geometry All of these factors will induce residual stresses that can be effectively relieved only by heat—which, of course, is applied during the nitriding process. Nitriding also acts as an additional temper, thus adding further dimensional stability to the steel. Control...
Abstract
Distortion is defined as an irreversible and usually unpredictable dimensional change in a component due to thermal processing or temperature variations and loading in service. This chapter describes two types of distortion: size distortion and shape distortion. It addresses how distortion can be managed by controlling certain factors. The chapter discusses the cause and effect of distortion during nitriding, the processes involved in stock removal prior to nitriding, and the criteria for post-machining operations.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860413
EISBN: 978-1-62708-348-5
... of composite systems for cryogenic applications. Figure 12.1 Temperature dependence of critical property ratios for uniaxial composite laminates and annealed stainless steel. 12.1.2 Composite Systems and Terminology Composite terminology is complex because of interacting diverse technologies...
Abstract
Composite systems for cryogenic applications are discussed in this chapter. This chapter emphasizes filamentary-reinforced composites because they are the most widely used composite materials. It begins with a discussion on the approach to designing and fabricating with low-pressure laminate composites. This is followed by a section providing an overview of the materials in modern cryogenic technology. Then, the chapter describes the effect of cryogenic temperatures on materials properties; it also introduces the various joining techniques developed for composite materials. The effects of radiation on the properties of the materials are covered as well as the processes involved in testing laminates at cryogenic temperatures. Finally, the chapter provides information available on concrete aggregate composites.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.9781627083485
EISBN: 978-1-62708-348-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050301
EISBN: 978-1-62708-311-9
..., if not all, of the transformation to martensite occurs. core hardness. The hardness found near the center of a bar. critical temperature range. The range in temperature at which austenite starts to form and completes forming. cryogenic treatment. The cooling of steel parts in freezers ranging from 129...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.9781627083119
EISBN: 978-1-62708-311-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
... on tensile and yield strength, fracture toughness, hardness, ductility, and creep and fatigue behaviors. The chapter covers wrought, cast, and powder metal titanium alloys and contains an extensive amount of property data. aging alloy composition cast titanium alloys creep properties fatigue...
Abstract
This chapter examines the process, structure, and property relationships in titanium alloys. It provides information on microstructures and strengthening mechanisms, the role of alloy and interstitial elements, and the effect of composition, processing, and surface treatments on tensile and yield strength, fracture toughness, hardness, ductility, and creep and fatigue behaviors. The chapter covers wrought, cast, and powder metal titanium alloys and contains an extensive amount of property data.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860203
EISBN: 978-1-62708-348-5
... with H ; large Moderate Fe 3 O 4 , rare earth garnets Antiferromagnetism Increases Peaks at critical temperature Variable with H ; moderate None to small Some stainless steels Small Ni–O, Mn, Cr a Data often indicate a moderate increase in magnitude with decreasing temperature...
Abstract
This chapter provides a view of magnetism in materials used at low temperatures. The discussion covers the concepts, definitions, and systems of units that are unique to the study of magnetic properties. The chapter provides a description of some of the techniques and devices used for determining magnetic properties.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200197
EISBN: 978-1-62708-354-6
... nondestructive testing steel castings Introduction After pouring, castings are allowed to solidify and cool. They are later removed from the molds in the shakeout operation. A series of activities then follow which are generally referred to as finishing and heat treatment. These activities can...
Abstract
After pouring, castings are allowed to solidify and cool. They are later removed from the molds in the shakeout operation. A series of activities then follow, which are generally referred to as finishing and heat treatment. These activities can be broadly categorized as shakeout, abrasive blast cleaning, removal of risers, ingates, and discontinuities, rough inspection, removal of discontinuities, finishing welding, heat treatment, and final visual, dimensional, and NDT inspection. This chapter provides a detailed discussion on these activities.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
... Abstract This chapter covers the basics of weldability of cast steels such as carbon and low alloy steels, corrosion-resistant high alloy steels, nickel-base alloys, heat-resistant high alloy steels, and wear-resistant high austenitic manganese steels. It provides an overview of weld overlay...
Abstract
This chapter covers the basics of weldability of cast steels such as carbon and low alloy steels, corrosion-resistant high alloy steels, nickel-base alloys, heat-resistant high alloy steels, and wear-resistant high austenitic manganese steels. It provides an overview of weld overlay and hard facing; cast-weld construction; and plasma arc cutting and plasma arc welding. The chapter discusses different types of welding processes. These include shielded metal-arc welding, air carbon arc cutting process, gas tungsten-arc welding, gas metal-arc welding process, flux-cored arc welding, submerged arc welding, and electroslag and electro-gas welding.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320217
EISBN: 978-1-62708-332-4
... on steel. Then, it provides an overview of steel casting applications. Next, the chapter reviews engineering guidelines for steel castings and feeder design. The following section provides information on feeding aids. Further, the chapter describes the elements of gating systems for steel castings. It also...
Abstract
Steel is broadly classified as plain-carbon steels, low-alloy steels, and high-alloy steels. This chapter begins by describing microconstituents of low- and medium-carbon steel, including bainite and martensite. This is followed by a section discussing the effect of alloying elements on steel. Then, it provides an overview of steel casting applications. Next, the chapter reviews engineering guidelines for steel castings and feeder design. The following section provides information on feeding aids. Further, the chapter describes the elements of gating systems for steel castings. It also describes the alloys, properties, applications, and engineering details of steel. Finally, the chapter explains defects in steel castings and presents guidelines for problem solving with examples.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... to refine stainless steel. The chapter also provides information on the classification and composition of stainless steel castings. It concludes with a brief description of the Schaeffler constitution diagram which is useful in predicting the type of stainless steel as a function of its alloy content...
Abstract
This chapter discusses the classification, composition, properties, and applications of five types of stainless steels: austenitic, ferritic, duplex, martensitic, and precipitation-hardening steels. It discusses the process involved in argon oxygen decarburization that is used to refine stainless steel. The chapter also provides information on the classification and composition of stainless steel castings. It concludes with a brief description of the Schaeffler constitution diagram which is useful in predicting the type of stainless steel as a function of its alloy content.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
... steels, called free-machining steels ( Sec. 13.7.1 ) [ 40 – 43 ]. The formation of Al 2 O 3 layers on CBN has been used to explain the improved machinablility of certain cast irons [ 44 ]. Many other examples exist, such as various SiO-containing tribolayers on a TiN-coated carbide tool when machining...
Abstract
In contrast to most plastic deformation processes, the shape of a machined component is not uniquely defined by the tooling. Instead, it is affected by complex interactions between tool geometry, material properties, and frictional stresses and is further complicated by tool wear. This chapter covers the mechanics and tribology of metal cutting processes. It discusses the factors that influence chip formation, including tool and process geometry, cutting forces and speeds, temperature, and stress distribution. It reviews the causes and effects of tool wear and explains how to predict and extend the life of cutting tools based on the material of construction, the use of cutting fluids, and the means of lubrication. It presents various methods for evaluating workpiece materials, chip formation, wear, and surface finish in cutting processes such as turning, milling, and drilling. It also discusses the mechanics and tribology of surface grinding and other forms of abrasive machining.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
... Abstract With typical alloy systems, casting is often the most convenient method by which to produce components. This is true for stainless steels, both for corrosion-resisting and for heat-resisting applications. This chapter discusses stainless steel casting alloys and their metallurgy...
Abstract
With typical alloy systems, casting is often the most convenient method by which to produce components. This is true for stainless steels, both for corrosion-resisting and for heat-resisting applications. This chapter discusses stainless steel casting alloys and their metallurgy. Foundry methods are discussed to the degree they are specific to the stainless alloys.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... the classification, composition, properties, treatments, and applications of austenitic, ferritic, martensitic, duplex, precipitation-hardening, powder metallurgy, and cast stainless steels. It also reviews the history of stainless steels and provides information on alloy designation systems. austenitic...
Abstract
Steels that resist corrosive attack from normal atmospheric exposure and contain a minimum of 10.5% Cr and 50% Fe are generally classified as stainless steels. Their special qualities lie in a chromium-rich oxide surface film that quickly regrows when damaged. This chapter discusses the classification, composition, properties, treatments, and applications of austenitic, ferritic, martensitic, duplex, precipitation-hardening, powder metallurgy, and cast stainless steels. It also reviews the history of stainless steels and provides information on alloy designation systems.