... by metal without failure under de nite conditions of corrosion and fatigue and for a speci c number of stress cycles and a speci ed period of time. corrosion inhibitor. See inhibitor. corrosionist. A person working in the eld of corrosion; anyone working to prevent corrosion or protect against corrosion...