Skip Nav Destination
Close Modal
Search Results for
corrosion-resistant coatings
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 508 Search Results for
corrosion-resistant coatings
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Image
Published: 01 March 2002
Fig. 13.14 Effect of a nickel-aluminide-type coating on the hot corrosion resistance of an IN-713 nickel-base superalloy turbine blade compared with an uncoated blade. (a) Uncoated blade after 118 test cycles, (b) micrograph showing severe degradation of IN-713 by hot corrosion, (c) aluminide
More
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000185
EISBN: 978-1-62708-312-6
... in corrosion-resistant coatings. automotive applications flake pigments metal foams stainless steel INDUSTRIAL USE of sintered stainless steels began in the 1960s in North America, approximately a decade after the application of sintered carbon steels. The main factors responsible...
Abstract
This chapter discusses the growing use of sintered stainless steels in automotive applications and various types of filters and filtering media. It also describes how these materials are produced in the form of metal foams and cellular structures and how they serve as flake pigments in corrosion-resistant coatings.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... Improved fatigue strength due to compressive stresses induced on the exposed surface, also relieves tensile stresses that contribute to stress-corrosion cracking Changing the surface chemistry Phosphate chemical conversion coatings Used primarily on steels for enhanced corrosion resistance...
Abstract
This chapter begins with a brief review of the different types of surface treatments and coatings used in industry and their effect on properties and performance. It then discusses the importance of corrosion and wear treatments and the consequences of failing to properly implement them in critical industries such as mining, energy production, transportation, and mineral and chemical processing. The chapter also describes basic approaches to dealing with corrosion and wear in steel.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240349
EISBN: 978-1-62708-251-8
... with a general overview of the factors influencing corrosion in iron and steel and a brief discussion of corrosion-resistant coatings. mill products hot rolling cold rolling forging extruding drawing electric arc furnace oxygen furnace plain carbon steels low-carbon steels medium-carbon plain...
Abstract
This chapter discusses various processes involved in the production of steel from raw materials to finished mill products. The processes include hot rolling, cold rolling, forging, extruding, or drawing. The chapter provides a detailed description of two main furnaces used for making steel: the electric arc furnace and the basic oxygen furnace. It also provides information on the classification and specifications for various steels, namely, plain carbon steels, low-carbon steels, medium-carbon plain carbon steels, and high-carbon plain carbon steels. The chapter concludes with a general overview of the factors influencing corrosion in iron and steel and a brief discussion of corrosion-resistant coatings.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040020
EISBN: 978-1-62708-428-4
... conversion and harvesting, in particular in the following applications: Wear Resistant and Corrosion Resistant Coatings The cost of wear and corrosion are estimated to be a significant fraction (up to 3-5%) of the gross domestic product in developed economies. These phenomena result in the degradation...
Abstract
This article summarizes the results of work completed by the ASM Thermal Spray Society Advisory Committee to identify key research challenges and opportunities in the thermal spray field. It describes and prioritizes research priorities related to emerging process methods, thermal spray markets and applications, and process robustness, reliability, and economics.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... for the reclamation of worn or out-of-tolerance parts, frequently with nickel-base alloys. Bronze alloys may be sprayed for some bearings and seal areas. Blends of tungsten carbide and nickel-base alloys are applied for wear resistance. Zinc is commonly coated on bridges and other structures for corrosion resistance...
Abstract
This article provides a brief description of commercially important thermal spray processes and gives examples of applications and application requirements. The processes covered are flame, wire arc, plasma, high-velocity oxyfuel processes, detonation gun, and cold spray methods. Examples are provided of the applications in aerospace, automotive, and medical device industries as well as the use of thermal spray as an additive manufacturing technique.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... upon foil penetration by the deepest pit. Service life can be extended by applying corrosion-resistant coatings. Primary emphasis should be placed on preventing exposure of both the graphite and the aluminum, and the graphite/aluminum composite should be frequently inspected while the component...
Abstract
This chapter discusses the ambient-temperature corrosion characteristics of aluminum metal-matrix composites (MMCs), including composites formed with boron, graphite, silicon carbide, aluminum oxide, and mica. It also discusses the effect of stress-corrosion cracking on graphite-aluminum composites and the use of protective coatings and design criteria for corrosion prevention.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... individually or in multiple layers to provide protection and other functions required of the coating or lining. The coatings applied to substrates often are multifunctional, providing corrosion control, an aesthetic surface appearance, abrasion and impact resistance, electrical insulation, and/or other...
Abstract
Organic coatings (paints and plastic or rubber linings), metallic coatings, and nonmetallic inorganic coatings (conversion coatings, cements, ceramics, and glasses) are used in applications requiring corrosion protection. These coatings and linings may protect substrates by three basic mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation, application, and inspection and quality assurance. The next section discusses the methods by which metals, and in some cases their alloys, can be applied to almost all other metals and alloys: electroplating, electroless plating, hot dipping, thermal spraying, cladding, pack cementation, vapor deposition, ion implantation, and laser processing. The last section focuses on nonmetallic inorganic coatings including ceramic coating materials, conversion coatings, and anodized coatings.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460209
EISBN: 978-1-62708-285-3
.... Recently, there have been some studies of the application of cold spray to the deposition of protective layers on automotive components. These layers can be broadly divided into two types: corrosion-resistant coatings and wear-resistant coatings. Corrosion-Resistant Coatings by Cold Spray...
Abstract
This chapter discusses the application of high-pressure cold spray to the automotive industry field, with special attention to three applications: additive manufacturing, fabrication methods, and protective coatings. Various studies on the automotive application of cold spray are reviewed. The background and purpose of each application are presented and practical cases are discussed.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... overlays, thermal spraying, and various deposition technologies. ceramic coating chemical vapor deposition cladding corrosion resistance electroless plating electroplating hot dip metallic coating physical vapor deposition thermal spraying weld overlays THE SURFACE-ENGINEERING METHODS...
Abstract
This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld overlays, thermal spraying, and various deposition technologies.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
... of the relatively poor corrosion resistance of line pipe steels in underground environments, a combination of mitigation strategies consisting of coatings and cathodic protection (CP) is required. In this article, the most common causes and contributing factors for corrosion and SCC, as well as prevention...
Abstract
This chapter discusses the most common causes and contributing factors for external corrosion and stress-corrosion cracking on oil and natural gas pipelines, as well as describes procedures for prevention, mitigation, detection, assessment, and repair. The forms of external corrosion covered include differential cell corrosion, microbiologically influenced corrosion, and stray current corrosion.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... protective coatings, including aluminide diffusion, overlay, and thermal barrier types, and how they perform in different environments based on their ability to tolerate strain. coatings corrosion resistance corrosion testing hot corrosion superalloys Overview Introduction Elevated...
Abstract
Superalloys tend to operate in environments where they are subjected to high-temperature corrosion, oxidation, and the erosive effects of hot gases. This chapter discusses the nature of these attacks and the effectiveness of various protection methods. It describes the primary forms of oxidation, the development of protective oxides, and the conditions associated with mixed gas corrosion and hot corrosion attack. It discusses oxidation and corrosion testing, the equipment used, and various ways to present the associated data. It describes the effect of gaseous oxidation on different alloys, discusses the formation of oxide scale in the presence of mixed gases, and explains how alloy composition contributes to oxide growth. The chapter discusses the underlying chemistry of hot corrosion, how to identify its effects, and how it progresses under various conditions. It also discusses protective coatings, including aluminide diffusion, overlay, and thermal barrier types, and how they perform in different environments based on their ability to tolerate strain.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
... that it becomes the cathode (cathodic protection). This chapter briefly reviews these methods of corrosion protection. The factors affecting corrosion behavior are covered. In addition, the chapter provides information on coatings and inhibitors, which are used in corrosion protection. corrosion protection...
Abstract
The basic concept for most methods of corrosion protection is to remove one or more of the electrochemical cell components so that the pure metal or metal alloy of interest will not corrode. Another widely used corrosion protection approach is to change the nature of the anode so that it becomes the cathode (cathodic protection). This chapter briefly reviews these methods of corrosion protection. The factors affecting corrosion behavior are covered. In addition, the chapter provides information on coatings and inhibitors, which are used in corrosion protection.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... applied by surfacing for the purpose of improved corrosion resistance or other properties. See also coating, surfacing, and hard- facing. clad metal. A composite metal containing two or more layers that have been bonded together. The bonding may have been accomplished by corolling, coextrusion, welding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940451
EISBN: 978-1-62708-302-7
... Film Lubricants • D 2671, Test Methods for Heat-Shrinkable Tubing for Electrical Use • D 2803, Test Method for Filiform Corrosion Resistance of Organic Coatings on Metal • D 2809, Test Method for Cavitation Erosion-Corrosion Characteristics of Aluminum Pumps with Engine Coolants • D...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080003
EISBN: 978-1-62708-304-1
... Abstract This chapter explains how materials selection becomes much more difficult when designing for high-temperature corrosion environments. It also discusses the use of cladding and weld overlays to compensate for material deficiencies and prolong service life. corrosion resistance...
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries. aluminum aluminum alloys...
Abstract
This chapter discusses corrosion prevention methods used with aluminum and its alloys. The methods range from relatively straightforward measures, such as proper handling and storage, to advanced early warning corrosion monitoring systems for military aircraft. The chapter summarizes the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
... of the alloy. A common solution to a corrosion problem is to substitute and alloy with greater corrosion resistance for the alloy that has corroded. Coatings Coatings for corrosion protection can be divided into two broad groups—metallic and nonmetallic (organic and inorganic). With either type...
Abstract
Corrosion can be defined as a chemical or electrochemical reaction between a material, usually a metal, and its environment that produces a deterioration of the material and its properties. This chapter describes the effects and economic impact of corrosion in major industrial plants. The emphasis in this chapter, as well as in other chapters in this book, is on aqueous corrosion, or corrosion in environments where water is present. The chapter describes the classification of various forms of corrosion based on the nature of the corrodent, mechanism of corrosion, and appearance of the corroded metal. It discusses five primary methods of corrosion control, namely, material selection, coatings, inhibitors, cathodic protection, and design. Examples of the opportunities in corrosion control and the means to implement a program to capitalize on those opportunities are presented in a table. The chapter concludes with varied sources of information pertaining to corrosion and corrosion prevention.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing. chemical composition corrosion resistance aluminum aluminum alloys claddings anodizing conversion coatings homogenization...
Abstract
This chapter addresses the general effects of composition, mechanical treatment, surface treatment, processing, and fabrication operations on the corrosion resistance of aluminum and its alloys. Different types of surface treatments covered include claddings, anodizing, and conversion coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing.
1