1-20 of 564 Search Results for

corrosion-resistant materials

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... Abstract This chapter discusses the factors influencing the corrosion resistance of bulk materials, namely alloying, metallurgical factors, and mechanical treatments. corrosion resistance bulk materials alloying metallurgical factors mechanical treatments THE CORROSION RESISTANCE...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... Abstract The challenge of materials selection is to achieve adequate performance at the lowest possible cost. Corrosion resistance is not the only property to be considered in making materials selections. Typical requirements and some of the procedures involved in making a selection and some...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030215
EISBN: 978-1-62708-282-2
... Abstract This chapter outlines the step-by-step processes by which materials are selected in order to prevent or control corrosion and includes information on materials that are resistant to the various forms of corrosion. The various forms of corrosion covered are general (uniform) corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
...-temperature gases ( Fig. 1 ). Fig. 1 Compositional and property linkages for stainless steels Nickel-base alloys make up an important segment of the corrosion-resistant materials, taking over from stainless steels and other alloys as service temperature or environment corrosivity...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
... , 1975 • Corrosion Engineering Handbook , Schweitzer P.A. , Ed., Marcel Dekker , 1996 • Corrosion Resistance Tables , 4th ed. , 3-volume set, Schweitzer P.A. , Ed., Marcel Dekker , 1995 • Corrosion-Resistant Materials Handbook , 4th ed. , DeRenzo D.J. , Ed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030235
EISBN: 978-1-62708-282-2
... care and attention. Unexpected premature failures can be harmful to personnel and adjacent equipment or parts. On occasion, a poor design can cause premature failure of even the most advanced corrosion-resistant materials. References 1. Uhlig H.H. , Corrosion Handbook...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
... corrosion-resistant materials, specifying a smooth finish on all critical metal surfaces, and coating with tough, resilient materials such as rubber and some plastics. For turbine blades, aeration of water serves to cushion the damage caused by the collapse of bubbles. Neoprene or similar elastomeric...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080259
EISBN: 978-1-62708-304-1
.... and Whitehead M.E. , Microanalysis of Scales and Deposits Formed on Corroding Furnace Tubes in Coal-Fired Boilers , in Corrosion Resistant Materials for Coal Conversion Systems , Meadowcroft D.B. and Manning M.I. , Ed., Applied Science , London , 1982 , p 63 7. Hay K.A...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910301
EISBN: 978-1-62708-250-1
... and operation. In addition, it cannot be overemphasized that poor design may render corrosion-resistant materials susceptible to premature corrosion. The results of a survey of chemical-process plants ( Ref 1 ) showed that design faults ranked highest (58%) as the causes for failure. Of almost equal ranking...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310247
EISBN: 978-1-62708-286-0
... in this chapter, Tables 1 through 5 list the relevant alloys for petroleum industry applications. Many, but not all, of these alloys are listed in the National Association of Corrosion Engineers (NACE) MR0175, Sulfide Stress Corrosion Cracking Resistant Metallic Materials for Oil Field Equipment ; the tables...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430087
EISBN: 978-1-62708-253-2
... efficiency, as well as greater demand on construction materials. This chapter discusses the primary requirements for boiler tube materials, including oxidation and corrosion resistance, fatigue strength, thermal conductivity, and the ability to resist creep and rupture. It also provides information...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
..., and they should be marked with materials (paints, crayons, and so on) free from zinc and other low-melting metals. Cadmium is probably second to zinc in importance as an agent of liquid-metal embrittlement because of its applications as a corrosion-resistant coating to a variety of hardware, particularly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
... Abstract Durability is a generic term used to describe the performance of a material or a component made from that material in a given application. In order to be durable, a material must resist failure by wear, corrosion, fracture, fatigue, deformation, and exposure to a range of service...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820099
EISBN: 978-1-62708-339-3
... the influence of ferrite-austenite balance on corrosion resistance and the influence of different welding conditions on various material properties of alloy 2205 (UNS S31803). corrosion resistance duplex stainless steel weld corrosion welding weldments DUPLEX STAINLESS STEELS are two-phase alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... materials Superalloys for creep resistance at high temperature Hardfacing and wear-resistant alloys Corrosion-resistant alloys High-speed steels, tool steels, and other steels Cobalt-base tool materials (e.g., the matrix of cemented carbide tool materials) Electrical-resistance alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030025
EISBN: 978-1-62708-282-2
... , 1981 • Holmes D.R. and Rahmel A. , Ed., Materials and Coatings to Resist High-Temperature Corrosion , Applied Science , 1978 • Hot Corrosion Problems Associated With Gas Turbines , STP 421, American Society for Testing and Materials , 1967 • Khanna A.S...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350011
EISBN: 978-1-62708-315-7
.... Crevice corrosion can be prevented or reduced through improved design to avoid crevices, regular cleaning to remove deposits, by selecting a more corrosion-resistant material, and by coating carbon steel or cast iron components with epoxy or other field-applied or factory-applied organic coatings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090241
EISBN: 978-1-62708-266-2
... Abstract Aluminum is protected by a barrier oxide film that, if damaged, reforms immediately in most environments. Despite this inherent corrosion resistance, there are conditions where aluminum alloys, like many materials, are subject to the effects of stress-corrosion cracking (SCC...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910193
EISBN: 978-1-62708-250-1
... in an environment, even at trace levels, can have a major impact on corrosion behavior. Chlorides particularly detrimental to materials that depend on a passive film for their corrosion resistance (e.g., stainless steels). In the presence of chloride ion, the passive film can break down locally and result...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870135
EISBN: 978-1-62708-299-0
... almost completely eliminated. Therefore, it can be concluded that two actions are necessary for the prevention and control of airframe microbiological corrosion problems. These are the selection of the proper structural materials, the use of biocides and coatings resistant to water and to microorganisms...