Published: 01 December 1995
Fig. 2-107 Pump casing. Corrosion-resistant cast steel CN-7M More
Image
Published: 01 December 1995
Fig. 20-1 Ranges of chromium and nickel in standard grades of heat-and corrosion-resistant castings More
Image
Published: 01 December 1995
Fig. 22-10 Corrosion rates of cast heat-resistant alloys in reducing flue gases More
Image
Published: 01 December 1995
Fig. 2-77 6000 lb (2722 kg) cast corrosion-resistant alloy steel steam chest cover More
Image
Published: 01 December 1995
Fig. 2-140 Assorted corrosion resisting steel castings for gas turbine applications. Weights 25 to 400 lb (11 to 181 kg) More
Image
Published: 01 January 2022
Fig. 7.49 Corrosion resistance of unalloyed and alloyed cast iron More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200274
EISBN: 978-1-62708-354-6
... Abstract This chapter describes the definitions, designation, chemical composition, room-temperature properties, elevated-temperature properties, and corrosion resistance of cast high alloy steels and stainless steels. In addition, the corrosion resistance of cast corrosion-resistant alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310147
EISBN: 978-1-62708-286-0
... Abstract With typical alloy systems, casting is often the most convenient method by which to produce components. This is true for stainless steels, both for corrosion-resisting and for heat-resisting applications. This chapter discusses stainless steel casting alloys and their metallurgy...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060291
EISBN: 978-1-62708-261-7
... stainless steel cast stainless steels duplex stainless steel ferritic stainless steel martensitic stainless steel powder metallurgy stainless steel precipitation-hardening stainless steel STAINLESS STEELS are a special class of steel alloys known primarily for their corrosion-resistant properties...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310269
EISBN: 978-1-62708-286-0
... Abstract This appendix contains tables listing the composition of austenitic, ferrite, martensitic, precipitation-hardenable, and duplex stainless steels and of Alloy Casting Institute heat- and corrosion-resisting casting alloys. chemical composition austenitic stainless steel duplex...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240469
EISBN: 978-1-62708-251-8
... production process and concludes with a discussion on corrosion resistance. copper brasses bronzes copper-nickel alloys beryllium-copper alloys copper casting alloys wrought copper alloys pure copper corrosion resistance chemical composition industrial applications COPPER was probably...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... (approximately 10.5 wt%) of chromium and, depending on the alloy, other elements such as nickel, molybdenum, and nitrogen. Figure 1 shows the effects of selected alloying elements on a 19Cr-9Ni stainless steel casting alloy. The corrosion resistance of stainless steels is based on the protective nature...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300179
EISBN: 978-1-62708-323-2
... applications, oil-impregnated machine ways from cast iron resist atmosphere corrosion (because of the oil) for decades. 7.6 Important Grades for Tribological Applications Gray Irons The ferritic gray irons (class 20) ( Fig. 7.3 ) are not generally used for tribological applications, other than...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... of corrosion behavior between cast and wrought product forms. corrosion alloying elements nickel alloys microstructure solid-state transformation cold working heat-resistant alloys NICKEL-BASE ALLOYS are solid solutions based in the element nickel. Even though nickel base alloys, in general...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170432
EISBN: 978-1-62708-297-6
... temperatures. They also reduce weld cracking and porosity in casting because they narrow the freezing range of the alloys. Silicon The addition of silicon to magnesium alloys has been found to increase fluidity of the metal in the molten state. However, it decreases corrosion resistance of magnesium...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240433
EISBN: 978-1-62708-251-8
... processes, such as dissolution in dilute acids, imposes obvious limitations on the use of carbon and low-alloy steels. The addition of chromium dramatically improves the corrosion and oxidation resistance of steel. Chromium oxidizes and forms a thin, tightly adherent layer of oxide (Cr 2 O 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320031
EISBN: 978-1-62708-332-4
.... There are property overlaps, and there may be more than one choice for a particular application and performance requirement. These varied types and grades of materials offer unique properties of different modes of wear resistance, corrosion resistance, and high-temperature resistance. Alloy cast iron is addressed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200369
EISBN: 978-1-62708-354-6
... Abstract This chapter covers the basics of weldability of cast steels such as carbon and low alloy steels, corrosion-resistant high alloy steels, nickel-base alloys, heat-resistant high alloy steels, and wear-resistant high austenitic manganese steels. It provides an overview of weld overlay...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240509
EISBN: 978-1-62708-251-8
... magnesium alloys, as shown for a number of casting alloys in Fig. 27.3 , has led to corrosion resistance approaching that of some of the competing aluminum casting alloys. Fig. 27.1 Severely corroded magnesium part. Source: Ref 1 Fig. 27.2 Effect of iron on corrosion of pure magnesium...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550141
EISBN: 978-1-62708-307-2
..., and mechanical properties of cast and wrought magnesium alloys. It also describes the processes used to produce magnesium parts, the causes and effects of corrosion, and the use of protective coatings and treatments. cast magnesium alloys corrosion protection corrosion resistance extrusion...