Published: 01 August 1999
Fig. 4 The relative resistance to stress-corrosion cracking of 7075-T6 plate is influenced by direction of stressing. Samples are alternatively immersed in 3.5% NaCl. Plate thickness: 6.4 to 38 mm (¼ to 3 in.). Source: Ref 1 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... in an aluminum plate would not be considered corrosion failure. On the other hand, an aluminum roofing sheet may experience some shallow pitting and staining to the extent that its appearance changes. This can be considered either an aesthetic corrosion failure or acceptable corrosion resistance, because...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
..., increased plating or paint adhesion, and for lubricity (e.g., to increase the formability of sheet metals) Chromate chemical conversion coatings Enhanced bare or painted corrosion resistance, improved adhesion of paint or other organic finishes, and provides the metallic surface with a decorative finish...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries. aluminum aluminum alloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... as measured property values. coating thickness corrosion resistance distortion wear resistance PROCESS COMPARISONS discussed in this chapter include: Process availability Corrosion resistance Wear resistance Cost Distortion or size change tendencies Thickness attainable...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
... Abstract This chapter is a compilation of terms and definitions related to surface engineering for corrosion and wear resistance. corrosion resistance surface treatment wear resistance Surface Engineering for Corrosion and Wear Resistance Copyright © 2001 ASM International® J.R...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... overlays, thermal spraying, and various deposition technologies. ceramic coating chemical vapor deposition cladding corrosion resistance electroless plating electroplating hot dip metallic coating physical vapor deposition thermal spraying weld overlays THE SURFACE-ENGINEERING METHODS...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... is extremely hard and corrosion resistant. The process is used for rebuilding mismachined or worn parts, for automotive valve stems, piston rings, shock rods, MacPherson struts, the bores of diesel and aircraft cylinders, and for hydraulic shafts. Hard chromium plating is also known as industrial...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
...) coatings, for example, TiN, TiAlN Glass Molding For glass molding, consider: Diffusion chromizing on cast iron molds for hot erosion-corrosion resistance Slurry/sinter formed ceramics (chromium oxide based) coatings Hard chrome plate (crack-free form is best) Parts in Sliding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870099
EISBN: 978-1-62708-299-0
... grain structure for plate is shown in Fig. 6 . The effect of grain orientation on resistance to stress-corrosion cracking is illustrated in Fig. 4 using data obtained for 7075-T6 alloy plate. Only two longitudinal specimens failed out of the 60 tested at a stress level of 75% of the longitudinal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.t65940451
EISBN: 978-1-62708-302-7
... • During E.D. , Corrosion Atlas , 3rd ed. , Elsevier Science Publishers , 1997 • Pruett K.M. , Chemical Resistance Guide for Metals and Alloys , Compass Publications , La Jolla, CA , 1995 • Schweitzer P.A. , Ed., Corrosion Resistance Tables , 4th ed. , Marcel Dekker...
Image
Published: 01 January 2000
Fig. 9 Effects of grain structure and stress direction on the SCC resistance of aluminum alloys. (a) Composite micrograph showing grain structure of a 38 mm (1.5 in.) alloy 7075-T6 plate. (b) the relative resistance to stress-corrosion cracking of 7075-T6 plate is influenced by direction More
Series: ASM Technical Books
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.tb.atia.t59340325
EISBN: 978-1-62708-427-7
... Abstract From canoes to catamarans, aluminum is used for a variety of marine applications. Fishing boats, pontoon boats, ferries, oceangoing liners, and military vessels all benefit from the weight savings, corrosion resistance, and weldability of aluminum products. This chapter shows examples...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... stovetops almost from the start of indoor plumbing; the glass keeps the work surfaces rust and scratch free. At almost the same time in history, faucets and related plumbing fixtures were chromium plated for the same reasons: corrosion protection and wear resistance. Chromium is the hardest metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870063
EISBN: 978-1-62708-299-0
... ) and aluminum-manganese (3 xxx ) alloys are quite resistant to exfoliation corrosion in all tempers. Exfoliation has been encountered in some highly cold worked aluminum-magnesium (5 xxx ) materials such as 5456-H321 boat hull plates. These developed a highly elongated grain structure and selective grain...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... individually or in multiple layers to provide protection and other functions required of the coating or lining. The coatings applied to substrates often are multifunctional, providing corrosion control, an aesthetic surface appearance, abrasion and impact resistance, electrical insulation, and/or other...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... Abstract The challenge of materials selection is to achieve adequate performance at the lowest possible cost. Corrosion resistance is not the only property to be considered in making materials selections. Typical requirements and some of the procedures involved in making a selection and some...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630211
EISBN: 978-1-62708-270-9
...) metal can be very effective if the base metal is completely and uniformly coated without pinholes, cracks, scratches, abrasions, and the like. For example, plating steel with lead or tin is very effective in corrosion resistance, unless the coating has some locations that are open to the base metal...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
... Titanium has a special place in the area of corrosion-resistant metals because it can be implanted in humans and resist salty body fluids. It is probably the number one material used for screws and plates and prosthetics; stainless steels were used up to the 1960s or ’70s, but titanium was mostly used...