1-20 of 554 Search Results for

corrosion performance

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000147
EISBN: 978-1-62708-312-6
... and ferroxyl tests, and elevated-temperature oxidation resistance tests. It also provides corrosion resistance and performance data from various sources. References References 1. Wear and Erosion; Metal Corrosion , Vol 3.02 , Annual Book of ASTM Standards , ASTM International , 2002 2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.9781627082662
EISBN: 978-1-62708-266-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
... and delivery time Need for further testing Material costs Fabrication costs Maintenance and inspection costs Return or investment analysis Information necessary for estimating corrosion performance Table 2 Information necessary for estimating corrosion performance Corrodent...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820143
EISBN: 978-1-62708-339-3
... to fillet welds, but all rods and electrodes rated will develop presently specific minimum strengths for butt welds); D, ductility (rating based on free bend elongation of the weld); C, corrosion resistance in continuous or alternate immersion of fresh or salt water, T, performance in service at sustained...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140133
EISBN: 978-1-62708-264-8
... steels would be developed later. This chapter discusses each of these four major types of stainless steel and their respective compositions, properties, and uses. It explains how alloying, heat treating, and various hardening processes affect corrosion performance, and includes a detailed discussion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120307
EISBN: 978-1-62708-269-3
... values for various grades of commercially pure and alloyed titanium. The values were derived from published sources and in-house laboratory tests. These data serve only as a starting point or initial guideline for corrosion performance. Corrosion Rates This Appendix is a compilation of general...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870161
EISBN: 978-1-62708-299-0
...Abstract Abstract This chapter describes the factors that affect the corrosion performance of aluminum assemblies joined by methods such as welding, brazing, soldering, and adhesive bonding. The factors covered include galvanic effects, crevices, and assembly stresses in products susceptible...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
...Abstract Abstract This chapter compares and contrasts surface-engineering processes based on process availability, corrosion and wear performance, distortion effects, penetration depth or attainable coating thickness, and cost. It provides both quantitative and qualitative information as well...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
...Abstract Abstract This chapter begins with a brief review of the different types of surface treatments and coatings used in industry and their effect on properties and performance. It then discusses the importance of corrosion and wear treatments and the consequences of failing to properly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030172
EISBN: 978-1-62708-282-2
.... Figure 4 shows the effects of iron and 13 other elements on the saltwater corrosion performance of magnesium in binary alloys with increasing levels of the individual elements. Six of the elements included in Fig. 4 (aluminum, manganese, sodium, silicon, tin, and lead), as well as thorium, zirconium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090241
EISBN: 978-1-62708-266-2
... laboratory tests reliably predict stress-corrosion performance in service; for example, results of an 84-day alternate immersion test of alloy 7075 and alloy 7178 products correlated well with performance of these products in a seacoast environment. Residual stresses are induced in aluminum alloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030349
EISBN: 978-1-62708-282-2
...Abstract Abstract This chapter examines methods of internal corrosion prediction for multiphase pipelines and details methodologies to perform internal corrosion direct assessment for natural gas pipelines. Further, real-time monitoring techniques for assessing actual corrosion at critical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030070
EISBN: 978-1-62708-282-2
... the initial dissolution occurs in the particle, as opposed to the surrounding matrix. The net effect is similar, in that a pit is initiated at the location of galvanic attack. More discussion of the impact of these copper-bearing particles on corrosion performance is included in the section on 2 xxx alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
...-corrosion cracking of 7075-T6 plate is influenced by direction of stressing. Samples are alternatively immersed in 3.5% NaCl. Plate thickness: 6.4 to 38 mm (¼ to 3 in.) Fig. 5 Intergranular corrosion of a type 304L stainless steel tube in a shuttle orbiter ammonia boiler. (a) Test performed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460185
EISBN: 978-1-62708-285-3
... stressed, thicker layers (up to 13 mm, or 0.5 in.) can be deposited without debonding. The ability to achieve superior corrosion and wear properties: Higher density and the absence of inflight oxidation/reaction result in excellent corrosion performance. Better adhesion with the substrate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170432
EISBN: 978-1-62708-297-6
... of assemblies can prevent galvanic corrosion. Because chloride solutions are particularly corrosive to magnesium and magnesium alloys, the following discussion will address the effects of various alloying/residual elements on salt water/salt spray corrosion performance. More detailed information...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... discusses protective coatings, including aluminide diffusion, overlay, and thermal barrier types, and how they perform in different environments based on their ability to tolerate strain. coatings corrosion resistance corrosion testing hot corrosion superalloys Overview Oxidation/Corrosion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480331
EISBN: 978-1-62708-318-8
... with titanium for long periods. Presumably, performance is related to operating variables. Titanium valve plates and springs provide good service in gas compressors for ammonia synthesis. Lighter-weight Ti-5Al-2.5Sn alloy springs and plates operate at higher speeds and are said to be less prone to corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090367
EISBN: 978-1-62708-266-2
.... Selection depends largely on the information required. Test Objectives General Considerations Tests for predicting the stress-corrosion performance of an alloy in a particular service application should be conducted with a stress system similar to that anticipated in service. Table 17.1 lists...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
... of High Performance Alloys ,” Paper 407, presented at Corrosion/86 , National Association of Corrosion Engineers, 1986 5.29 Streicher M.A. , Effect of Composition and Structure on Crevice, Intergranular, and Stress Corrosion of Some Wrought Ni-Cr-Mo Alloys , Corrosion , Vol 32 , 1976 , p...