... Abstract This chapter discusses five forms of mechanically assisted degradation of metals: erosion, fretting, fretting fatigue, cavitation and water drop impingement, and corrosion fatigue. Emphasis is placed on the mechanisms and the factors affecting these forms of degradation. erosion...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780329
EISBN: 978-1-62708-281-5
... analog in the corrosion of metals, in that function is slowly degraded in the external environment by chemical reactions and must be treated as limiting the true usefulness of the materials. In the future, the full and successful outdoor use of engineering plastics will undoubtedly depend on a clear...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870401
EISBN: 978-1-62708-314-0
... Abstract This chapter describes the conditions under which environmental degradation is likely to occur in polymer matrix composites and the potential damage it can cause. It discusses the problems associated with moisture absorption and exposure to solvents, fuels, ultraviolet radiation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030003
EISBN: 978-1-62708-282-2
... Abstract This chapter provides an introduction to various forms of corrosion, namely uniform corrosion, localized corrosion, mechanically assisted degradation, environmentally induced cracking, microbiologically influenced corrosion, and metallurgically influenced corrosion. uniform...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060369
EISBN: 978-1-62708-261-7
... Abstract Corrosion can be defined as a chemical or electrochemical reaction between a material and its environment that causes the material and its properties to degrade. In most cases, it refers to the electrochemical oxidation of metals accompanied by the production of oxides or salts of the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... Abstract All materials are susceptible to corrosion or some form of environmental degradation. Although no single material is suitable for all applications, usually there are a variety of materials that will perform satisfactorily in a given environment. The intent of this chapter is to review...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780146
EISBN: 978-1-62708-281-5
..., photo-oxidative degradation, environmental corrosion, and chemical corrosion of polymers. It also includes some of the techniques used to detect changes in structure during polymer exposure to hostile environments. In addition, the article describes the effects of environment on polymer performance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030235
EISBN: 978-1-62708-282-2
... the necessary action will be taken is affected by financial, technical, safety, social, and/or political issues ( Ref 37 ). To prevent corrosion/degradation, the designer can: Avoid obvious design weaknesses (see subsequent examples) Use more reliable materials, even if this entails...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030005
EISBN: 978-1-62708-282-2
.... atmospheric corrosion Pourbaix diagrams biologically influenced corrosion ATMOSPHERIC CORROSION is the degradation and destruction of metallic materials and their structure and properties due to interaction with the terrestrial atmosphere at its characteristic air temperature, humidity, air chemistry...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
.... Combined attack of alloys simultaneously by two or more reactants is often called mixed gas attack. Gaseous-induced degradation of superalloys is the principal means of elevated-temperature corrosion attack, but deposits which significantly affect the gas-induced corrosion processes can be formed on...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090191
EISBN: 978-1-62708-266-2
... Garzarolli F. , Rubel H. , and Steinberg E. , Behavior of Water Reactor Core Materials with Respect to Corrosion Attack , Proc. Environmental Degradation of Materials in Nuclear Power Systems—Water Reactors , National Association of Corrosion Engineers , 1984 , p 1 – 24 6.5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030167
EISBN: 978-1-62708-282-2
... degrade, rather than enhance, the corrosion properties. This is the case for most aluminum alloys. Alloying elements that are typically used to increase the corrosion resistance have low solubility in aluminum when alloyed using conventional techniques. In addition to alloying, there are metallurgical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430204
EISBN: 978-1-62708-253-2
...). Erosion-corrosion is defined as the degradation of the material due to both mechanical and chemical processes. In the case of pipes and tubes, EC is mainly found at locations such as bends, elbows, and joints. Erosion-corrosion takes the form of grooves, waves, gullies, teardrop-shaped pits, and horseshoe...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... , 1990 2. Gleeson B. , High-Temperature Corrosion of Metallic Alloys and Coatings , Corrosion and Environmental Degradation , Vol II , Wiley-VCH , 2000 , p 173 10.1002/9783527619306.ch14 3. Rebak R.B. , Corrosion of Non-Ferrous Alloys, Part I: Nickel-, Cobalt-, Copper...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430290
EISBN: 978-1-62708-253-2
... degraded and almost absent ( Fig. 6.113a ). The outer surface facing the fire side had corrosion damage, forming shallow pits followed by intergranular corrosion ( Fig. 6.113b ). The outer surface was covered with a thick crust of scaling (350 μm thick), whereas the inner surface had adherent scaling with...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030025
EISBN: 978-1-62708-282-2
... Abstract This chapter focuses on resistance characteristics and methods of protecting different forms of high-temperature gaseous corrosion, namely high-temperature oxidation, sulfidation, carburization, hydrogen effects, and hot corrosion. high-temperature gaseous corrosion high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
.... , and Subudhi M. , Expert Panel Report on Proactive Materials Degradation Assessment (PMDA) , NUREG CR-6923, U.S. Nuclear Regulatory Commission , Washington, DC , 2007 5.90 Anderson P.L. , Stress Corrosion Cracking of Current Structural Materials in Commercial Nuclear Power Plants...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
... Abstract Corrosion testing and monitoring are powerful tools in the fight to control corrosion. This chapter provides a general overview of three major categories of corrosion tests, namely laboratory tests, pilot-plant tests, and field tests. It begins with brief sections describing the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230459
EISBN: 978-1-62708-298-3
... Abstract This chapter covers the corrosion behavior of beryllium in aqueous environments. It describes the chemical reactions that drive the corrosion process, the conditions required for equilibrium, and the factors that affect corrosion resistance. It discusses the stability of the native...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... stresses may be required. In atmospheric corrosion, resistance to ultraviolet degradation, bacteria, and fungi is sometimes an important consideration. The coating process can be broken down into the following steps: Design and selection Surface preparation Application Inspection and...