...Abstract Abstract During a routine preflight inspection of a piston aircraft engine, part of a cooling fin was found that had broken off the cylinder. The piece, made of aluminum-silicon alloy, was cleaned and examined. Based on the fracture characteristics revealed by an electron microscope...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
...-insulated) copper tubes. Source: Wieland-Werke AG Fig. 2.88 Manometer springs in extruded and drawn tin-bronze tubes. Source: Wieland-Werke AG Fig. 2.86 (a) Tube coils and finned tubes in extruded copper tubes. (b) Test stand for finned tubes. Source: Wieland-Werke AG Fig. 2.87...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.t53630237
EISBN: 978-1-62708-270-9
... properly if the cooling system does not operate properly. Air-cooled engines may overheat if the cooling fins on the outside of the engine are clogged with dirt, leaves, or other debris. It does not take much dirt or insulating deposit on cooling surfaces to greatly reduce the thermal conductivity and heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220077
EISBN: 978-1-62708-341-6
... unit separate from the pumping station, they offer a method of reducing water consumption. Typically, vapor-cooled systems ( Fig. 5.2 ) utilize a mist of water sprayed onto the fins of an air-to-water heat exchanger. This water is lost as a vapor or mist of steam, but because of the high heat input...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460185
EISBN: 978-1-62708-285-3
.... , and Jodoin B. , “ Near-Net Shape Fins for Compact Heat Exchanger Produced by Cold Spray ,” Thermal Spray 2013: Innovative Coating Solutions for the Global Economy ( Busan, South Korea ), 2013 10.1007/s11666-013-9968-x 7.6 Grasme D. , First Serial Application of Cold Spraying for Coating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.cw.t51820077
EISBN: 978-1-62708-339-3
... of type 410 martensitic stainless steel Fig. 11 Heat-recovery steam generator Fig. 12 Feedwater economizer, finned tube harp assembly Fig. 13 The iron-chromium (Fe-Cr) alloy phase diagram. Fig. 3 Grain boundary martensite formation in a type 430 ferritic stainless...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430204
EISBN: 978-1-62708-253-2
... EDS analysis at different locations of tube sample Table 6.12 EDS analysis at different locations of tube sample Elements Surface amount, wt.% Crack ID Fin Oxygen 31.56 30.81 35.34 Sodium 1.99 0.86 1.55 Magnesium 1.85 0.68 0.55 Aluminum 1.42 0.54 1.10...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... thin cross sections (such as fins, louvers, walls) that could be distorted by the blasting media Avoid intricate designs and surface features Broaching/honing Typically used for inside diameters of tubes and other cylindrical parts, or for grooves, large holes, and other cavities Surfaces must...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410103
EISBN: 978-1-62708-280-8
... 6.1 Engineering Product Design 6.1.1 Parting Plane Cooling System should Avoid the Ejector Pins Die Cavity Positioning 6.1.3 Drafts for Aluminum Die Castings Selection of Casting-Cavity Part to be Cut into Ejector Location of Gates 6.1.10 Gate Pads Feeder Locations and Feeder...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
... for deep drawing, and easy to weld. Used for high-purity applications such as chemical processing equipment. Also for nameplates, fan blades, flue lining, sheet metal work, spun holloware, and fin stock 1350 Electrical conductors 2011 Screw machine products. Appliance parts and trim, ordnance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410247
EISBN: 978-1-62708-280-8
... products Piping, valves Die casting A 518 F Pistons, connecting rods, housings Die casting A 413 F Missiles Missile bodies, missile fins Investment cast C 355 T61/T62 Motorcycles Pistons Gravity permanent mold casting 242 T61 Air-cooled cylinder heads Gravity permanent mold casting...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460107
EISBN: 978-1-62708-285-3
..., and control the on/off sequence for filling the gas storage. The most common ambient high-pressure vaporizers use stainless steel tubing with aluminum fins, which provide high surface area to transfer heat from the ambient air to convert the liquid nitrogen to a gas. This type of vaporizer requires...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050175
EISBN: 978-1-62708-311-9
..., workpiece defects, heat treating practice, and tempering practice. Features such as sharp corners, fillets, radii, tooling marks, keyways and the number, location, and size of holes are termed stress risers . Abrupt changes in section thickness within a workpiece can promote nonuniform cooling during...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740001
EISBN: 978-1-62708-308-9
... in the steelworks. Other by-products, such as tar, are also extracted for further refining and sale. After carbonization, the coke is pushed out of the ovens and cooled. Limestone, mainly calcium carbonate, is added as a flux for easier melting and slag formation. The slag floats on top of the molten iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... Cooling 4.7.4 Low-Pressure Permanent Molding Cell Layout 4.7.5 Low-Pressure Permanent Molding Advantages 4.7.3 Oxide Prevention 4.9 Squeeze Casting Process Advantages and Applications Squeeze Casting Machines 4.7.6 Use of Vacuum in Low-Pressure Permanent Molding 4.8 Counter...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
...) lever, inboard flap hinge bolt, nose landing gear piston axle, multiple-leg aircraft-handling sling, aircraft hoist sling, internal spur gear, and MLG axle. In addition, the chapter provides information on full-scale fatigue testing, nondestructive testing, and failure analysis of fin attach bolts...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
...: Cooling the tool, workpiece, and chip Lubricating (reducing friction and minimizing erosion on the tool) Controlling the built-up edge on the tool Flushing away chips Protecting the workpiece from corrosion The relative importance of each function depends on the work material...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... by the initial composition and by the degree of nonequilibrium cooling. For higher-solidification-rate processes such as pressure die and permanent mold casting and for thinner sections in which more rapid solidification takes place, shrinkage porosity is strongly affected by the temperature at which mass...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140021
EISBN: 978-1-62708-335-5
..., molten metal is injected under pressure into water-cooled dies. Pressure is maintained until the part has solidified. Molten metal usually enters the mold by the action of a hydraulic ram in a containment chamber (shot chamber), resulting in rapid filling of the mold cavity. While lubrication is required...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8