Skip Nav Destination
Close Modal
Search Results for
conversion coatings
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 258 Search Results for
conversion coatings
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... Abstract Organic coatings (paints and plastic or rubber linings), metallic coatings, and nonmetallic inorganic coatings (conversion coatings, cements, ceramics, and glasses) are used in applications requiring corrosion protection. These coatings and linings may protect substrates by three basic...
Abstract
Organic coatings (paints and plastic or rubber linings), metallic coatings, and nonmetallic inorganic coatings (conversion coatings, cements, ceramics, and glasses) are used in applications requiring corrosion protection. These coatings and linings may protect substrates by three basic mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation, application, and inspection and quality assurance. The next section discusses the methods by which metals, and in some cases their alloys, can be applied to almost all other metals and alloys: electroplating, electroless plating, hot dipping, thermal spraying, cladding, pack cementation, vapor deposition, ion implantation, and laser processing. The last section focuses on nonmetallic inorganic coatings including ceramic coating materials, conversion coatings, and anodized coatings.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries. aluminum aluminum alloys...
Abstract
This chapter discusses corrosion prevention methods used with aluminum and its alloys. The methods range from relatively straightforward measures, such as proper handling and storage, to advanced early warning corrosion monitoring systems for military aircraft. The chapter summarizes the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Abstract
This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic coatings and various pack cementation and deposition processes. It also discusses the selection and use of industrial paints and paint application methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
... Abstract This chapter provides practical information on surface treatments that work by altering the surface chemistry of metals and alloys. It discusses the use of phosphate and chromate conversion coatings as well as anodizing, steam oxidation, diffusion coatings, and pack cementation...
Abstract
This chapter provides practical information on surface treatments that work by altering the surface chemistry of metals and alloys. It discusses the use of phosphate and chromate conversion coatings as well as anodizing, steam oxidation, diffusion coatings, and pack cementation. The chapter also covers ion implantation and laser alloying.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120085
EISBN: 978-1-62708-269-3
... of scale and how it can be removed via belt grinding, abrasive blasting, and molten salt descaling baths. It also discusses the role of acid pickling, barrel finishing, polishing, and buffing as well as the use of chemical conversion coatings and protective platings. barrel finishing chemical...
Abstract
Cleaning procedures serve to remove scale, tarnish films, and other contaminants that form or are otherwise deposited on the surface of titanium during processing operations such as hot working and heat treatment. This chapter explains what makes titanium susceptible to the formation of scale and how it can be removed via belt grinding, abrasive blasting, and molten salt descaling baths. It also discusses the role of acid pickling, barrel finishing, polishing, and buffing as well as the use of chemical conversion coatings and protective platings.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing. chemical composition corrosion resistance aluminum aluminum alloys claddings anodizing conversion coatings homogenization...
Abstract
This chapter addresses the general effects of composition, mechanical treatment, surface treatment, processing, and fabrication operations on the corrosion resistance of aluminum and its alloys. Different types of surface treatments covered include claddings, anodizing, and conversion coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
.... Inorganic coatings are also used to provide a barrier between the environment and the metal. Inorganic coatings include enamels, glass linings, and conversion coatings. Porcelain enamel coatings are inert in water and resistant to most weather. They are common on appliances and plumbing fixtures. Glass...
Abstract
The basic concept for most methods of corrosion protection is to remove one or more of the electrochemical cell components so that the pure metal or metal alloy of interest will not corrode. Another widely used corrosion protection approach is to change the nature of the anode so that it becomes the cathode (cathodic protection). This chapter briefly reviews these methods of corrosion protection. The factors affecting corrosion behavior are covered. In addition, the chapter provides information on coatings and inhibitors, which are used in corrosion protection.
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... or lubricate surfaces, including solid film, chemical conversion, and vacuum coatings, surface oiling and texturing, and lubricating platings. It compares and contrasts methods based on thickness and depth and their relative effect on friction, erosion, and wear. coatings friction and wear properties...
Abstract
This chapter covers coatings and treatments that are used to improve the friction and wear behaviors of materials. It describes modifications that work by hardening contacting surfaces, including heat treating, vacuum coating, thermal spray, and plating, and those that separate or lubricate surfaces, including solid film, chemical conversion, and vacuum coatings, surface oiling and texturing, and lubricating platings. It compares and contrasts methods based on thickness and depth and their relative effect on friction, erosion, and wear.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... Improved fatigue strength due to compressive stresses induced on the exposed surface, also relieves tensile stresses that contribute to stress-corrosion cracking Changing the surface chemistry Phosphate chemical conversion coatings Used primarily on steels for enhanced corrosion resistance...
Abstract
This chapter begins with a brief review of the different types of surface treatments and coatings used in industry and their effect on properties and performance. It then discusses the importance of corrosion and wear treatments and the consequences of failing to properly implement them in critical industries such as mining, energy production, transportation, and mineral and chemical processing. The chapter also describes basic approaches to dealing with corrosion and wear in steel.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040067
EISBN: 978-1-62708-300-3
... Aluminum Lubrication in the cold forging of aluminum is especially important because of the high adhesion between the aluminum and the die material. The lubrication systems used for the cold forging of aluminum are given in Fig. 7.4 . In general, one of three conversion coatings are used...
Abstract
This chapter discusses the effect of friction and lubrication on forgings and forging operations. The discussion covers lubrication mechanisms, the use of friction laws, tooling and process parameters, and the lubrication requirements of specific materials and forging processes. The chapter also describes several test methods for evaluating lubricants and explains how to interpret associated test data.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040211
EISBN: 978-1-62708-300-3
... of steels. The success of the zinc phosphatizing treatment is influenced by the composition of the steel, especially the chromium content. Consequently, special procedures and other conversion coatings, such as oxalates, are preferred for austenitic stainless steels. Stearate-type soaps, which adhere...
Abstract
This chapter discusses the process of cold forging and its effect on various materials. It describes billet preparation and lubrication procedures, cold upsetting techniques, and the use of slab analysis for estimating cold forging loads. It likewise describes extrusion processes, explaining how to estimate friction and flow stress and predict extrusion loads and energy requirements. The chapter also discusses the tooling used in cold forging, the parameters affecting tool life, and the relative advantages of warm forging.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
..., or diffusion. anodizing. Forming a conversion coating on a metal surface by anodic ox- idation; most frequently applied to aluminum. arc spraying (ASP). A thermal spraying process using an arc between two consumable electrodes of surfacing materials as a heat source and a compressed gas to atomize and propel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870045
EISBN: 978-1-62708-299-0
... also influential. Two-coat polyurethane paint systems experienced far fewer incidences of filiform corrosion than did single-coat systems. Filiform corrosion rarely occurred when bare aluminum was anodized using chromic acid or primed with chromate or chromate-phosphate conversion coatings. Because...
Abstract
Pitting is the most common corrosion attack on aluminum alloy products. This chapter explains why pitting occurs and how it appears in different types of aluminum. It discusses pitting rates, pitting potentials, and pitting resistance as well as testing and prevention methods. It also discusses the problem of crevice corrosion and how it is influenced by crevice geometry and operating environment. The discussion covers the most common forms of crevice corrosion, including water staining, poultice corrosion, and filiform corrosion, along with related testing and prevention methods.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030380
EISBN: 978-1-62708-282-2
... of positive charge from an electronic to an ionic conductor. An anodic reaction is an oxidation process. A common example in corrosion is: Me ! Men+ + neÀ. anodizing. Forming an anodic coating or conversion coating on a metal surface by anodic oxidation; frequently applied to aluminum. anolyte...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040020
EISBN: 978-1-62708-428-4
... conversion and harvesting, in particular in the following applications: Wear Resistant and Corrosion Resistant Coatings The cost of wear and corrosion are estimated to be a significant fraction (up to 3-5%) of the gross domestic product in developed economies. These phenomena result in the degradation...
Abstract
This article summarizes the results of work completed by the ASM Thermal Spray Society Advisory Committee to identify key research challenges and opportunities in the thermal spray field. It describes and prioritizes research priorities related to emerging process methods, thermal spray markets and applications, and process robustness, reliability, and economics.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.htpa.t53310235
EISBN: 978-1-62708-346-1
...-11; DIN EN ISO 2006-03 - national annexes such as HB, HV, HR - Tables become Part 4 ISO 2002-10 ISO 2002-10 DIN EN ISO DIN EN ISO 2003-05 2003-05 Testing of thin coatings 2003 Parameters of the tensile test from IIT Hardness conversion (basis DIN 50150 : 2000) 14577-4 TR 29381 18265...
Abstract
This chapter reviews the general principles involved in codifying standards and describes the historical development of materials testing standards. It provides information on the standards related to the Brinell, Vickers, Rockwell, and Knoop methods as well as those for the instrumented indentation test and hardness conversions.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410001
EISBN: 978-1-62708-280-8
... information on the process of conversion of steel and iron parts to aluminum. aluminum castings casting 1.1 Introduction Casting is one of the most economical manufacturing processes for providing shape to components of machinery and is used in a wide range of industries. It has evolved over...
Abstract
Casting is one of the most economical manufacturing processes for providing shape to components of machinery and is used in a wide range of industries. This chapter is a brief account of the advantages, applications, limitations, and market growth of aluminum casting. It also provides information on the process of conversion of steel and iron parts to aluminum.
Book Chapter
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030033
EISBN: 978-1-62708-282-2
... of coatings. The standard coating system uses a chromate conversion layer covered by organic paint coats. The primer coat might contain chromate pigments for further corrosion protection. The chromate conversion layer is formed by immersion into an acidic bath containing dichromate, fluoride, and ferricyanide...
Abstract
This chapter concentrates on the better-known and widely studied phenomenon of pitting corrosion of passive metals. The discussion focuses on different parameters that influence pitting corrosion, namely environment, metal composition, potential, temperature, surface condition, and inhibitors. It also provides information on various stages of pitting: passive film breakdown, metastable pitting, pit growth, and pit stifling or death.