... Abstract Organic coatings (paints and plastic or rubber linings), metallic coatings, and nonmetallic inorganic coatings (conversion coatings, cements, ceramics, and glasses) are used in applications requiring corrosion protection. These coatings and linings may protect substrates by three basic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870191
EISBN: 978-1-62708-299-0
... the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries. aluminum aluminum alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350095
EISBN: 978-1-62708-315-7
... Abstract This chapter provides practical information on surface treatments that work by altering the surface chemistry of metals and alloys. It discusses the use of phosphate and chromate conversion coatings as well as anodizing, steam oxidation, diffusion coatings, and pack cementation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray, and ceramic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030169
EISBN: 978-1-62708-282-2
... coatings. The processing steps that can have relatively significant impact on corrosion resistance are homogenization, rolling, extrusion, quenching, aging, and annealing. chemical composition corrosion resistance aluminum aluminum alloys claddings anodizing conversion coatings homogenization...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120085
EISBN: 978-1-62708-269-3
... of scale and how it can be removed via belt grinding, abrasive blasting, and molten salt descaling baths. It also discusses the role of acid pickling, barrel finishing, polishing, and buffing as well as the use of chemical conversion coatings and protective platings. barrel finishing chemical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
.... Inorganic coatings are also used to provide a barrier between the environment and the metal. Inorganic coatings include enamels, glass linings, and conversion coatings. Porcelain enamel coatings are inert in water and resistant to most weather. They are common on appliances and plumbing fixtures. Glass...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... or lubricate surfaces, including solid film, chemical conversion, and vacuum coatings, surface oiling and texturing, and lubricating platings. It compares and contrasts methods based on thickness and depth and their relative effect on friction, erosion, and wear. coatings friction and wear properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... Improved fatigue strength due to compressive stresses induced on the exposed surface, also relieves tensile stresses that contribute to stress-corrosion cracking Changing the surface chemistry Phosphate chemical conversion coatings Used primarily on steels for enhanced corrosion resistance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040067
EISBN: 978-1-62708-300-3
... Aluminum Lubrication in the cold forging of aluminum is especially important because of the high adhesion between the aluminum and the die material. The lubrication systems used for the cold forging of aluminum are given in Fig. 7.4 . In general, one of three conversion coatings are used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 February 2005
DOI: 10.31399/asm.tb.chffa.t51040211
EISBN: 978-1-62708-300-3
... of steels. The success of the zinc phosphatizing treatment is influenced by the composition of the steel, especially the chromium content. Consequently, special procedures and other conversion coatings, such as oxalates, are preferred for austenitic stainless steels. Stearate-type soaps, which adhere...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350231
EISBN: 978-1-62708-315-7
..., or diffusion. anodizing. Forming a conversion coating on a metal surface by anodic ox- idation; most frequently applied to aluminum. arc spraying (ASP). A thermal spraying process using an arc between two consumable electrodes of surfacing materials as a heat source and a compressed gas to atomize and propel...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390100
EISBN: 978-1-62708-459-8
... lubricants (emulsions, synthetics, solutions); and a wide range of coatings and carriers. It also discusses solid-film lubricants (oxide films, polymer films, layer-lattice compounds) and environmental and safety concerns. aqueous lubricants coatings compounded lubricants greases metalworking...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870045
EISBN: 978-1-62708-299-0
... also influential. Two-coat polyurethane paint systems experienced far fewer incidences of filiform corrosion than did single-coat systems. Filiform corrosion rarely occurred when bare aluminum was anodized using chromic acid or primed with chromate or chromate-phosphate conversion coatings. Because...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390325
EISBN: 978-1-62708-459-8
..., extensive metal flow, and significant surface generation, and should ideally match the process of interest [ 63 ]. Bay, et al. [ 64 ] found in evaluations of MoS 2 and conversion coatings that the normal pressure and interface temperature have the most importance, while surface expansion, sliding distance...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030380
EISBN: 978-1-62708-282-2
... of positive charge from an electronic to an ionic conductor. An anodic reaction is an oxidation process. A common example in corrosion is: Me ! Men+ + neÀ. anodizing. Forming an anodic coating or conversion coating on a metal surface by anodic oxidation; frequently applied to aluminum. anolyte...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040020
EISBN: 978-1-62708-428-4
... conversion and harvesting, in particular in the following applications: Wear Resistant and Corrosion Resistant Coatings The cost of wear and corrosion are estimated to be a significant fraction (up to 3-5%) of the gross domestic product in developed economies. These phenomena result in the degradation...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550141
EISBN: 978-1-62708-307-2
..., and mechanical properties of cast and wrought magnesium alloys. It also describes the processes used to produce magnesium parts, the causes and effects of corrosion, and the use of protective coatings and treatments. cast magnesium alloys corrosion protection corrosion resistance extrusion...