Skip Nav Destination
Close Modal
By
İlker Emin Dağ, Baris Avar, Mrutyunjay Panigrahi
By
Erhard Klar, Prasan K. Samal
Search Results for
continuous mesh belt sintering furnaces
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 27
Search Results for continuous mesh belt sintering furnaces
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Sintering Densification
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290169
EISBN: 978-1-62708-319-5
... small batch furnaces to continuous furnaces for large-scale production. The process atmosphere depends on the material, ranging from air for oxide ceramics to vacuum for reactive metals. Measurement of the progress in sintering includes changes in dimensions, density, and properties. Hot isostatic...
Abstract
After shaping and first-stage binder removal, the component (with remaining backbone binder) is heated to the sintering temperature. Further heating induces densification, evident as dimensional shrinkage, pore rounding, and improved strength. This chapter begins with a discussion on the events that are contributing to sintering densification, followed by a discussion on the driving forces, such as surface energy, and high-temperature atomic motion as well as the factors affecting these processes. The process of microstructure evolution in sintering is then described, followed by a discussion on the tools used for measuring bulk properties to monitor sintering and density. The effects of key parameters, such as particle size, oxygen content, sintering atmosphere, and peak temperature, on the sintered properties are discussed. Further, the chapter covers sintering cycles and sintering practices adopted as well as provides information on dimensional control and related concerns of sintering. Cost issues associated with sintering are finally covered.
Book Chapter
Furnaces and Related Equipment for Heat Treating
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440055
EISBN: 978-1-62708-262-4
.... The conveyor usually is driven by large diameter drums at each end of the furnace. The belt may return either outside or inside the furnace, depending on the function the furnace is performing. This type of furnace is suited to continuous annealing, carburizing, carbonitriding, tempering, sintering...
Abstract
This chapter, a detailed account of furnaces and related equipment for heat treating, begins by describing three basic modes of heat transmission, namely conduction, convection, and radiation, followed by a discussion on the working principle, applications, advantages, and disadvantages of furnaces classified based on the heat transfer medium employed. The types of furnaces covered are batch-type, continuous-type, liquid bath, fluidized bed, and vacuum. The subsequent sections provide information on furnace parts, fixtures, quenching mediums, and quenching systems. The final section of the chapter describes the types of atmospheres available, emphasizing their applications and limitations.
Book Chapter
Sintering and Corrosion Resistance
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000059
EISBN: 978-1-62708-312-6
...-resistance properties, are treated in detail. Sintering Furnaces Most commercial sintering of stainless steel parts is performed in continuous mesh belt conveyor furnaces at temperatures up to approximately 1150 °C (2100 °F). Pusher, walking beam, and vacuum furnaces are used for higher temperatures...
Abstract
This chapter discusses the sintering process for stainless steel powders and its influence on corrosion resistance. It begins with a review of sintering furnaces and atmospheres and the effect of temperature and density on compact properties such as conductivity, ductility, and strength. It then describes the relationship between sintered density and corrosion resistance and how it varies for different types of powders and operating environments. The chapter also explains how stainless steel powders respond to different sintering atmospheres, including hydrogen, hydrogen-nitrogen, and vacuum, and liquid-phase sintering processes.
Book Chapter
Powder Metallurgy
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740373
EISBN: 978-1-62708-308-9
... properties of a part are developed. It is usually accompanied by shrinkage of the part. Sintering can also involve alloying and homogenization of mixed powder parts. Sintering can be conducted in either a batch or a continuous furnace. In a batch furnace operation, a discrete batch of parts is cycled...
Abstract
This chapter covers the basic steps of the powder metallurgy process, including powder manufacture, powder blending, compacting, and sintering. It identifies important powder characteristics such as particle size, size distribution, particle shape, and purity. It compares and contrasts mechanical, chemical, electrochemical, and atomizing processes used in powder production, discusses powder treatments, and describes consolidation techniques along with secondary operations used to obtain special properties or improve dimensional precision. It also discusses common defects such as ejection cracks, density variations, and microlaminations.
Book Chapter
The Economic Contribution of Powder Metallurgy Industries, Associations, and Employment Opportunities
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 September 2024
DOI: 10.31399/asm.tb.pmamfa.t59400367
EISBN: 978-1-62708-479-6
.... ◎ … ◎ … ◎ ◎ Mitsubishi Steel Mfg. Co., Ltd. … … ◎ … … ◎ Equipment manufacturers Products Compacting press Repressing press Sintered furnace Heat treating furnace Atmosphere gas generator Mesh belt Kohtaki Precision Machine Co., Ltd. ◎ ◎ … … … … Taiyo Wire Cloth Co., Ltd...
Abstract
This chapter discusses the economic importance of powder metallurgy in various countries, the types of jobs created, and the role of powder metallurgy associations around the world.
Book
Powder Metallurgy Stainless Steels: Processing, Microstructures, and Properties
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.9781627083126
EISBN: 978-1-62708-312-6
Book Chapter
Glossary of Practical Heat Treating Terms
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 April 2024
DOI: 10.31399/asm.tb.phtpp.t59380235
EISBN: 978-1-62708-456-7
... in the formation of bainite. batch furnace A furnace used to heat treat a single load at a time. Batch-type furnaces are necessary for large parts such as heavy forgings and are preferred for complex alloy grades requiring long cycles. See car furnace, horizontal batch furnace. belt furnace A continuous-type...
Abstract
The appendix provides a glossary of practical heat treating terms.
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2024
DOI: 10.31399/asm.tb.phtpp.9781627084567
EISBN: 978-1-62708-456-7
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.9781627084475
EISBN: 978-1-62708-447-5
Book Chapter
Low-Pressure Permanent and Semipermanent Mold Casting and Counter-Pressure Casting
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 30 November 2023
DOI: 10.31399/asm.tb.ceeg.t59370187
EISBN: 978-1-62708-447-5
... 3 ) shows an LPPM machine designed to switch the crucible furnaces for continuous operation. When the first crucible furnace has been emptied, the second crucible furnace moves in, ready for production. This interchangeable furnace design reduces downtime. Fig. 10.5 A row of LPPM machines...
Abstract
The low-pressure permanent molding (LPPM) and semipermanent molding (LPSPM) processes are versatile, and they meet the quality requirements of a variety of high-integrity, large-sized, and thin-walled aluminum castings for various industries. This chapter presents the major features, operation sequence, advantages, and applications of LPPM, LPSPM, and counter-pressure casting.
Book Chapter
Structural Ceramics
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
... resistance, and dimensional stability at extreme temperatures Compact heat exchanges, heat exchanger tubes, radiant tubes, furnace components, insulators, thermocouple protection tubes, kiln furniture Internal combustion engine components Engine components High-temperature resistance, wear resistance...
Abstract
Ceramics normally have high melting temperatures, excellent chemical stability and, due to the absence of conduction electrons, tend to be good electrical and thermal insulators. They are also inherently hard and brittle, and when loaded in tension, have almost no tolerance for flaws. This chapter describes the applications, properties, and behaviors of some of the more widely used structural ceramics, including alumina, aluminum titanate, silicon carbide, silicon nitride, zirconia, zirconia-toughened alumina (ZTA), magnesia-partially stabilized zirconia (Mg-PSZ), and yttria-tetragonal zirconia polycrystalline (Y-TZP). It also provides information on materials selection, design optimization, and joining methods, and covers every step of the ceramic production process.
Book Chapter
Nitridation
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080067
EISBN: 978-1-62708-304-1
... is often used as a protective atmosphere in heat treating and sintering operations. Molecular nitrogen can be severely nitriding for many metals and alloys, particularly when temperatures are sufficiently high. Ammonia (NH 3 ) is a commonly used nitriding gas for case hardening at temperatures from 500...
Abstract
Oxidation usually dominates high-temperature corrosion reactions, but under certain conditions, some alloys may be affected by nitridation as well. This chapter explains why nitridation occurs and how it attacks various metals, in some cases, penetrating deeper than oxidation. It provides images and data describing the nitridation process and its effects on metals and alloys in high-temperature air as well as NH3-H2O, NH3 and H2-N2-NH3, and N2 environments. It also includes test data showing that nitridation is more severe in a nitrogen atmosphere than an ammonia environment at 1090 °C (2000 °F).
Book Chapter
Powder Metallurgy Processing
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280117
EISBN: 978-1-62708-267-9
... to the level of creep-rupture strengths required of airfoils. Furthermore, the cast superalloys could be made hollow (to conserve weight) and cast with simple internal passages for cooling. Consequently, P/M technology languished for a few years, despite some continued interest in the ODS alloys as sheet...
Abstract
Gas turbine disks made from nickel-base superalloys are often produced using powder metallurgy (P/M) techniques because the alloy compositions normally used are difficult or impractical to forge by conventional methods. This chapter discusses the P/M process and its application to superalloys. It describes the gas, vacuum, and centrifugal atomization processes used to make commercial superalloy powders. It explains how the powders are consolidated into preforms or billets using hot isostatic pressing, extrusion, or a combination of the two. It also provides information on spray forming and consolidation by atmospheric pressure, and includes a section on powder-based disk components, where it discusses the general advantages of P/M as well as the effects of inclusions, carbon contamination, and the formation of oxide and carbide films due to prior particle boundary conditions. The chapter concludes with a detailed discussion on mechanically alloyed superalloy compositions, the product forms into which they are made, and some of the applications where they are used.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Book
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.sch6.9781627083546
EISBN: 978-1-62708-354-6
Book Chapter
Specimen Preparation for Light Microscopy
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
... Proprietary oil-water emulsion 6 50 350 0.0001-in feed, machine surface grinding Proprietary oil-water emulsion 4 30 150 Alumina 38A 60 MVBE wheel Hand grinding Nil 15 40 170 Lathe turning 0.001-in feed Proprietary oil-water emulsion 1 15 150 Belt surfacing Alumina 100 mesh...
Abstract
This chapter explains how to prepare metallographic samples for light microscopy and how to anticipate and avoid related problems. It describes standard practices and procedures for sectioning, mounting, grinding, and polishing and identifies common defects along with their causes and cures. It also provides recommendations for handling specific materials and addresses safety concerns.
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.9781627083041
EISBN: 978-1-62708-304-1
Book Chapter
The Role of Materials in Defining Process Constraints
Available to PurchaseBook: Principles of Brazing
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230143
EISBN: 978-1-62708-351-5
... coatings is restricted. Thick film Requires simple equipment. Lends itself to high-volume production using screen printing and firing in belt furnaces Relies on manufacturers’ proprietary formulations. Relatively high process temperatures are used. Only thick films can be applied by this technique...
Abstract
This chapter considers the role of materials in brazing operations and the manner in which they impact on the choice of processing conditions and their optimization. The concepts covered are metallurgical and mechanical constraints, and constraints imposed by the components and their solutions as well as service environment considerations.
Book Chapter
Glossary
Available to PurchaseSeries: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400245
EISBN: 978-1-62708-258-7
..., irregularly shaped particles of hard material. abrasive belt. A coated abrasive product, in the form of a belt, used in production grinding and polishing. abrasive disk. (1) A grinding wheel that is mounted on a steel plate, with the exposed at side being used for grinding. (2) A disk-shaped, coated abrasive...
Abstract
This chapter presents definitions of terms related to the metallurgy and metallographic study of irons and steels.