1-20 of 162 Search Results for

continuous fiber reinforced composites

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780276
EISBN: 978-1-62708-281-5
...Abstract Abstract This article briefly reviews abrasive and adhesive wear failure of reinforced polymers and polymer composites, namely particulate-filled polymers, short-fiber-reinforced polymers, polymers with continuous fibers, and mixed reinforcements and fabrics. It includes scanning...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.fdmht.t52060223
EISBN: 978-1-62708-343-0
... stresses, and enhanced interfaces for oxidation. continuous-fiber metal-matrix composites elastic-viscoplastic property mismatch residual stress relaxation thermal expansion mismatch THE TECHNOLOGICAL ADVANTAGES of continuous-fiber-reinforced composites include increased static strength...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
...-related applications 11.1 Discontinuously Reinforced Ceramic-Matrix Composites 11.2 Applications for Discontinuously Reinforced Ceramic-Matrix Composites 11.3 Continuous Fiber Ceramic-Matrix Composites 11.4 Applications for Continuous Fiber Ceramic-Matrix Composites 11.5 Carbon-Carbon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
..., compositions, and performance-cost tradeoffs of common MMCs, including aluminum-matrix composites, titanium-matrix composites, and fiber-metal laminates. It also explains how fiber-reinforced composites and laminates are made, describing both continuous and discontinuous fiber matrix production processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
..., including stir and slurry casting, liquid metal infiltration, spray deposition, powder metallurgy, extrusion, hot rolling, and forging. The chapter also provides information on continuous-fiber aluminum and titanium composites as well as particle-reinforced titanium and fiber metal (glass aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030193
EISBN: 978-1-62708-349-2
...Abstract Abstract As fiber-reinforced polymeric composites continue to be used in more damage-prone environments, it is necessary to understand the response of these materials when subjected to impact from foreign objects. This chapter provides an overview of the analysis methods for impact...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... nonferrous alloy, and the reinforcement consists of high-performance carbon, metallic, or ceramic additions. Reinforcements, either continuous or discontinuous, may constitute from 10 to 70 vol% of the composite. Continuous fiber or filament (f) reinforcements include graphite, silicon carbide (SiC), boron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870001
EISBN: 978-1-62708-314-0
.... They may be spherical, platelets, or any other regular or irregular geometry. Particulate composites tend to be much weaker and less stiff than continuous-fiber composites, but they are usually much less expensive. Particulate reinforced composites usually contain less reinforcement (up to 40 to 50 volume...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
.... compression molding discontinuous-fiber composites fiber length fiber orientation reaction injection molding spray-up DISCONTINUOUS-FIBER COMPOSITES are used where the higher strength and stiffness of continuous-fiber composites are not required, as they are much less expensive to manufacture...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... Fig. 1 The material cost versus performance of various aluminum-matrix composites. DRA, discontinuously reinforced aluminum Fig. 2 Cross section of a continuous-fiber reinforced boron/aluminum composite. Shown here are 142 μm diameter boron filaments coated with B 4 C in a 6061 aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
... & Hall , 1993 , p 126 – 161 10.1007/978-1-4757-2216-1_4 • Composites , Ceramics Information Analysis Center , 1995 , p 1 – 31 • Cullum G.H. , Ceramic Matrix Composite Fabrication and Processing: Sol-Gel Infiltration , Handbook on Continuous Fiber-Reinforced Ceramic Matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... in all directions. They may be spherical, platelets, or any other regular or irregular geometry. Particulate composites tend to be much weaker and less stiff than continuous fiber composites but are usually much less expensive. Particulate-reinforced composites usually contain less reinforcement (up...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
... of the polymer matrix is to transfer the load between fibers as well as provide corrosion resistance, damage tolerance, and thermal and environmental stability ( Ref 1 ). Fiber-reinforced polymeric composites are developed from thermoplastic or thermoset resins combined with either discontinuous or continuous...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610377
EISBN: 978-1-62708-303-4
... to be much weaker and less stiff than continuous-fiber composites but are usually much less expensive. Particulate-reinforced composites usually contain less reinforcement (up to 40 to 50 vol%) due to processing difficulties and brittleness. A fiber has a length that is much greater than its diameter...
Book Chapter

By M. B. Kasen
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860413
EISBN: 978-1-62708-348-5
... of resin-impregnated reinforcement) to form a composite laminate or by continuous winding of the reinforcing fiber over a mandrel to form a filament-wound structure. A third construction method, in which continuous or discontinuous fibers of random orientation reinforce molded plastic structures, has...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030211
EISBN: 978-1-62708-349-2
...-Rate Effects on Thermoplastic-Matrix Crystallinity Fiber Nucleation of Spherulite Crystal Growth The use of fiber-reinforced polymeric composite materials continues to increase throughout the world due to their unique performance attributes. These heterogeneous and anisotropic materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870373
EISBN: 978-1-62708-314-0
... carbon fibers fastener hole defects fatigue properties fiber distortion glass fibers porosity voids THE MECHANICAL PROPERTIES of a composite material depend on many factors, including whether or not the fibers are continuous or discontinuous; the strength and stiffness of the fibers themselves...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... this question: can ductile titanium-aluminide intermetallic compounds be made that will compete with the nickel-base superalloys? Titanium matrix composite (TMC) materials are conventional titanium alloys strengthened by a reinforcement of continuous fibers. Composite material concepts have been explored...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730115
EISBN: 978-1-62708-283-9