Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200133
EISBN: 978-1-62708-354-6
... Abstract This chapter gives an overview of how steel castings may be effectively adapted to modern concurrent engineering processes. The chapter discusses computer aided design programs, solid modeling, solidification simulation programs, and rapid prototyping. computer-aided design...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220143
EISBN: 978-1-62708-341-6
... nondestructive inspection (NDI) methods and process simulation on computers. The first of these includes electromagnetic sorting of induction surface hardened parts, and lends itself readily to real-time control as well. Process simulation of induction heating is useful in the design stage as well...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2024
DOI: 10.31399/asm.tb.phtpp.t59380001
EISBN: 978-1-62708-456-7
... and set-point programmers; and process supervision or data management has been done by strip chart recorders or data loggers. This separation of functions requires communication among the logic controllers, loop controllers, and data-acquisition equipment. Finally, when a supervisory computer...