1-20 of 767 Search Results for

composition limits

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870251
EISBN: 978-1-62708-299-0
...Composition limits for wrought aluminum and aluminum alloys Table A-1 (Part 1) Composition limits for wrought aluminum and aluminum alloys AA No. Composition, wt% Si Fe Cu Mn Mg Cr Ni Zn Ga V Specified other elements Ti Unspecified other elements Al, min Each Total...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870259
EISBN: 978-1-62708-299-0
...Composition limits for unalloyed and alloyed aluminum castings (<italic>xxx</italic>.0) and ingots (<italic>xxx</italic>.1 or <italic>xxx</italic>.2) Table A-2 (Part 1) Composition limits for unalloyed and alloyed aluminum castings ( xxx .0) and ingots ( xxx .1 or xxx .2) Designation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
...Nominal composition and composition limits of aluminum alloy castings Table 2.1 Nominal composition and composition limits of aluminum alloy castings Based on industry handbooks, notably Aluminum Association Standards for Sand and Permanent Mold Castings , and the Aluminum Association...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240453
EISBN: 978-1-62708-251-8
... their compositional ranges, distinguishing features, advantages, limitations, and applications. cast iron cooling rate graphite formation cementite formation silicon aluminum nickel cobalt copper sulfur vanadium chromium tin molybdenum manganese microstructure white cast iron gray cast iron...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170210
EISBN: 978-1-62708-297-6
... to H19), tungsten hot-work steels (types H21 to H26), and molybdenum hot-work steels (types H42 and H43). Composition limits for hot-work steels are listed in Table 1 . Effects of Alloying Elements Cold-work tool steels, because they do not have the alloy content necessary to make them resistant...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 December 2020
DOI: 10.31399/asm.tb.phtbp.t59310079
EISBN: 978-1-62708-326-3
... the UNS designation. The H-steels are guaranteed by the supplier to meet these hardenability limits for a specified range of chemical composition. The tighter hardenability bands of four H-steels are compared in Fig. 10 with the wider hardenability bands of similar steel grades based on composition...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550001
EISBN: 978-1-62708-307-2
.... , Hong Kong Conmilit Press Limited , 2000 1.9 Horton R.E. and McCarty J.E. , Damage Tolerance of Composites , Composites , Vol 1 , Engineered Materials Handbook , ASM International , 1987 1.10 Rohatgi P.K. , Gupta N. , and Daoud A. , Synthesis...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
...Abstract Abstract This chapter provides basic engineering information on aluminum alloys with an emphasis on their use in applications where weight is a significant design factor. It discusses the advantages and limitations of various types of aluminum along with their compositions...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310137
EISBN: 978-1-62708-286-0
... stringers and inclusions Fig. 1 Possible aluminum/titanium precipitates Abstract Abstract This chapter discusses the composition, alloying characteristics, mechanical properties, corrosion resistance, advantages, limitations, and applications of martensitic, semiaustenitic, and austenitic...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050155
EISBN: 978-1-62708-311-9
... of oil-quenched 4340 steel bar. Single-heat results: ladle composition, 0.41C-0.67ΔMn-0.023ΔP-0.018ΔS-0.26ΔSi-1.77ΔNi-0.78ΔCr-0.26Mo; grain size, ASTM 6 to 8. Critical points: Ac 1 , temperature at which austenite begins to form on heating, 730 °C (1350 °F); Ac 3 , temperature at which transformation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.mgppis.t60400001
EISBN: 978-1-62708-258-7
..., chromium, and/or molybdenum. ASTM specification A 532 covers the abrasion-resistant white cast irons. There are ten different white cast irons, according to ASTM A532. These are listed subsequently: The typical compositional limits of malleable iron are (wt%): ASTM has a number of specifications...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060273
EISBN: 978-1-62708-261-7
... alloyed than M2, or more hardenable, or more wear resistant, and so forth based on its number designation. A comprehensive listing of the chemical composition limits for wrought tool steels and high-speed steels that are commonly used in industry today is provided in Table 11.2 . Composition limits...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170193
EISBN: 978-1-62708-297-6
...-solution strengthening. Table 1 lists compositions of some HSLA steels covered in ASTM specifications. Compositional limits for HSLA steel grades described in ASTM specifications Table 1 Compositional limits for HSLA steel grades described in ASTM specifications ASTM specification (a) Type...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140001
EISBN: 978-1-62708-335-5
... Casting in Recyclable Aluminum, Magnesium, Zinc, and ZA Alloys ,” Die Casting Development Council , 1996 9. “ The NFFS Guide to Aluminum Casting Design: Sand and Permanent Mold ,” Non-Ferrous Founders Society , 1994 10. “ Designations and Chemical Composition Limits for Aluminum Alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440009
EISBN: 978-1-62708-262-4
... or bainite) are phases—these are microstructures. A phase diagram is a graphical representation of the equilibrium temperature and composition limits of phase fields and phase reactions in an alloy system. In the iron-cementite system, temperature is plotted vertically, and composition is plotted...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430027
EISBN: 978-1-62708-253-2
... of temperature and overall composition. It represents the equilibrium temperature and composition limits of phase fields and phase reactions in an alloy system. Phase diagrams also provide quantitative understanding of phase transformations and related microstructural changes. A phase is a chemically homogeneous...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000001
EISBN: 978-1-62708-313-3
... components, nuclear reactors, industrial furnaces, heat exchangers, petrochemical equipment, petroleum production equipment, automotive turbochargers, and biomedical devices. Superalloys are among the most compositionally complex metallic alloys ever developed for commercial use. Their compositional...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220009
EISBN: 978-1-62708-259-4
.... For this reason, the definition of steel based on this chemical composition limit should be restricted to the so-called carbon steels . In the past, alloys with low carbon content used to be known as irons. In recent decades, the ability of refining processes to systematically attain very low carbon contents...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170123
EISBN: 978-1-62708-297-6
..., these steels contain no more than 0.035 P and 0.040 S. Compositional limits for weathering steel grades (ASTM A 588) used in building and bridge construction Table 9 Compositional limits for weathering steel grades (ASTM A 588) used in building and bridge construction Grade UNS designation...