Published: 01 November 2010
Fig. 6.8 Resin flow patterns during thermoplastic composite processing. Source: Ref 3 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780028
EISBN: 978-1-62708-281-5
... of engineering plastics and commodity plastics follows, and the final section briefly outlines the most common plastics manufacturing processes. thermal properties mechanical properties physical properties engineering plastics commodity plastics chemical composition manufacturing process molecular...
Image
Published: 01 November 2010
Fig. 6.1 Typical thermoplastic composite process cycle. Source: Ref 1 More
Image
Published: 01 October 2012
Fig. 8.43 Typical thermoplastic composite process cycle. Source: Ref 8.17 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870183
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses thermoplastic composite fabrication processes and related equipment and procedures. The discussion covers consolidation and thermoforming operations as well as joining methods. composite fabrication consolidation joining thermoforming thermoplastic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... Abstract This chapter familiarizes readers with the many and varied thermoset composite fabrication processes and the types of applications for which they were developed. It describes wet lay-up, prepreg lay-up, and low-temperature vacuum bag curing prepreg processes, which are best suited...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870201
EISBN: 978-1-62708-314-0
..., and data plots. composite curing cure monitoring heat transfer mathematical models polymer matrix composites residual stress resin flow resin kinetics resin viscosity void formation PROCESSES FOR NEW COMPOSITE MATERIALS, during the 1960s and 1970s, were based solely on previous...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
..., continuous fiber ceramic composites, and carbon-carbon composites. It also describes a number of ceramic-matrix composite processing methods, including cold pressing and sintering, hot pressing, reaction bonding, directed metal oxidation, and liquid, vapor, and polymer infiltration. ceramic-matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the advantages and disadvantages of metal matrix composites and the methods used to produce them. It begins with a review of the composition and properties of aluminum matrix composites. It then describes discontinuous composite processing methods, including stir...
Image
Published: 01 August 2005
Fig. 7.22 Discontinuous crack growth process. (a) Composite microphotograph of PVC showing positions of crack tip (arrows on the left) and craze tip (arrows on the right) at given cyclic intervals. (b) Model of discontinuous cracking process. Source: Ref 7.25 More
Image
Published: 01 November 2010
Fig. 1.3 Major polymer matrix composite fabrication processes More
Image
Published: 01 October 2012
Fig. 8.4 Major polymer-matrix composite fabrication processes. Source: Ref 8.1 More
Image
Published: 01 November 2012
Fig. 34 Discontinuous crack growth process. (a) Composite micrograph of polyvinyl chloride showing positions of crack tip (arrows on the left) and craze tip (arrows on the right) at given cyclic intervals. (b) Model of discontinuous cracking process. Source: Ref 26 More
Image