1-20 of 37 Search Results for

composite prepreg

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780089
EISBN: 978-1-62708-281-5
... Composite Prepregs ,” paper presented at the 26th Annual Technology Conference on Reinforced Plastics , Section 14-A, 1-14, SPE Inc., Composites Division, 1971 28. Nuss R.D. , Effect of Different Catalysts on an Identical Thermosetting Epoxy-Anhydride Resin System Evaluated Through the B...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
... by High-Performance Liquid Chromatography , Composite Materials: Quality Assurance and Processing , ASTM STP 797 , 1983 , p 3 – 14 10.1520/STP28535S 7. Carpenter J.F. , Assessment of Composite Starting Materials: Physiochemical Quality Control of Prepregs , AIAA/ASME Symposium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870201
EISBN: 978-1-62708-314-0
.... , Measurement and Control of Prepreg Impregnation for Elimination of Porosity in Composite Parts , Society of Manufacturing Engineers, Fabricating Composites ’88 , Sept 1988 • Timmerman J.F. , Hayes B.S. , and Seferis J.C. , Cryogenic Cycling of Polymeric Composite Materials: Effects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... impregnation process Abstract Abstract This chapter familiarizes readers with the many and varied thermoset composite fabrication processes and the types of applications for which they were developed. It describes wet lay-up, prepreg lay-up, and low-temperature vacuum bag curing prepreg processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
... of Composite Prepreg by Soxhlet Extraction ASTM D 618-08 Standard Practice for Conditioning Plastics for Testing ASTM D 792-08 Standard Test Methods for Density and Specific Gravity (Relative Density) of Plastics by Displacement ASTM D 883-08 Standard Terminology Relating to Plastics ASTM D 1505...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
... are discussed in Chapters 20 and 21, “Metal Matrix Composites” and “ Ceramic Matrix Composites ,” respectively. Variables that define a prepreg are fiber type, fiber form (such as unidirectional or woven), resin type, fiber areal weight (FAW), prepreg resin content, and cured per ply thickness. Fiber...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870489
EISBN: 978-1-62708-314-0
... epoxy Composite material forms Cost (material and labor), process compatibility, fiber volume control, material handling, fiber wet-out, material scrap Base form—neat resin/Rovings Prepreg (b) (a) Depends on how “highest performance” is defined—high temperature, toughness, and superior...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780115
EISBN: 978-1-62708-281-5
... , May C.A. , Ed., ACS Symposium Series 227, American Chemical Society , 1983 , p 25 – 47 10.1021/bk-1982-0227.ch002 68. Morgan R.J. , Walkup C.M. , and Hoheisel T.H. , Characterization of the Cure of Carbon Fiber/Epoxy Composite Prepregs by Differential Scanning...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
... • Repecka L. and Boyd J. , “ Vacuum-Bag-Only-Curable Prepregs That Produce Void-Free Parts ,” SAMPE 2002 , May 12–16 , 2002 • Thorfinnson B. and Bierrinann T.F. , “ Production of Void Free Composite Parts without Debulking ,” 31st International SAMPE Symposium...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870183
EISBN: 978-1-62708-314-0
... Fig. 6.1 Typical thermoplastic composite process cycle. Source: Ref 1 Fig. 6.2 Fabrication methods for sheet stock Fig. 6.3 Typical vacuum bag configuration Fig. 6.4 Principle of autoconsolidation Fig. 6.5 Typical thermoforming setup. Source: Ref 2...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870517
EISBN: 978-1-62708-314-0
... repair joints Fig. 19.13 Typical bagging sequence for field repair Fig. 19.15 Double-bag method for debulking prepreg and wet lay-up patches Fig. 19.16 Double-bag staging cycle Fig. 19.18 Composite honeycomb minor repair. Source: Ref 1 Fig. 19.19...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780383
EISBN: 978-1-62708-281-5
... survey spectra of the failure surfaces from white, spotty delaminations. (a) Board surface. (b) Prepreg surface Fig. 11 Angular-dependent method for determining compositional gradients with x-ray photoelectron spectroscopy. Depth analyzed is proportional to sin θ. Fig. 16 Auger...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860149
EISBN: 978-1-62708-338-6
... glass tow AGY Zylon HM Poly(p-phenylene-2,6-benzobisoxazole), high-performance fibers Toyobo Resin designations Table A1.2 Resin designations Resin designation Type Supplier 3501 Epoxy prepreg, 350 °F cure Hexcel Aerospace LY564 Epoxy Araldit/Huntsman 1902 Epoxy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860001
EISBN: 978-1-62708-338-6
... reliable answer for closed-form analysis. There are “B”-basis allowable data for fiber/resin combinations for 121 °C (250 °F)-curing prepreg for the aircraft composite component industry (e.g., AGATE) ( Ref 1.3 ), but there is no comparable database for filament-wound composites that use prepreg tow...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.9781627083386
EISBN: 978-1-62708-338-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870573
EISBN: 978-1-62708-314-0
... Stress-strain for monolithic and ceramic matrix composites Fig. 21.4 Crack dissipation mechanisms Fig. 21.5 Interfacial coating Fig. 21.6 Ceramic prepreg fabrication. Chemical vapor deposition (CVD) Fig. 21.7 Fabrication sequence for powder processing. Hot...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870255
EISBN: 978-1-62708-314-0
... 2002 , p 515 – 525 • “ HexWeb Honeycomb Selector Guide ,” Hexcel Composites , 1999 • Hsiao H.M. , Lee S.M. , Buyny R.A. , and Martin C.J. , “ Development of Core Crush Resistant Prepreg for Composite Sandwich Structures ,” 33rd International SAMPE Technical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
... be strong enough to open the tool. A vacuum bag process is used with prepreg sheet or liquid resins and fiberglass cloth or mat. The resin-glass composite is laid up on a one-sided mold and covered with a plastic film; a vacuum is then drawn between the film and the tool. Air pressure consolidates...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870101
EISBN: 978-1-62708-314-0
... supplier for exact values. Options for making composite tools Table 4.2 Options for making composite tools Accuracy Number of steps Master pattern Master mold Intermediate or production tool 1 step 2 steps 3 steps 3 steps 4...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870373
EISBN: 978-1-62708-314-0
...Typical properties of unidirectional composite materials Table 14.1 Typical properties of unidirectional composite materials Property E glass/epoxy Aramid/epoxy High-strength carbon/epoxy Intermediate-modulus carbon/epoxy Specific gravity 2.1 1.38 1.58 1.64 0° tensile...