Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030001
EISBN: 978-1-62708-349-2
...Abstract Abstract This chapter provides a general description of materials and methods for manufacturing high-performance composites. The materials covered are polymer matrices and prepreg materials and the methods include infusion processes, composite-toughening methods, matrix-toughening...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610377
EISBN: 978-1-62708-303-4
... mechanism in detail along with related factors. It also discusses the primary differences between composites and metals, the effect of manufacturing defects, damage tolerance, and testing and certification. References References 1. Campbell F.C. , Introduction to Composite Materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870333
EISBN: 978-1-62708-314-0
... method along with best practices and procedures. composite manufacturing radiographic inspection thermographic inspection ultrasonic inspection visual inspection FLAWS CAN OCCUR, unfortunately, at almost any stage of the composite manufacturing process or during service. A summary of some...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860081
EISBN: 978-1-62708-338-6
...Abstract Abstract The technology of fabricating composite hardware and structures by filament winding has evolved empirically through the development and manufacturing of specific components. This chapter reviews areas of technology used in building composite parts and discusses the processes...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860115
EISBN: 978-1-62708-338-6
..., and manufacturing operation follows. The chapter introduces the basic design approach and shows some sizing techniques along with example calculations. It discusses the processes involved in the testing of the composite pressure vessel. References References 9.1 Wilson B. , SAMPE J. , May/June...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
... for advanced composites. Fibers may be continuous or discontinuous, depending on the application and manufacturing process. This chapter covers the fibers used for organic matrix composites, with an emphasis on continuous fibers. Fibers used for metal- and ceramic-matrix composites are discussed...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2021
DOI: 10.31399/asm.tb.ciktmse.t56020001
EISBN: 978-1-62708-389-8
... and their relevance in design and manufacturing. It begins with a review of compositional impurities, the physical arrangement of atoms in solid solution, and the factors that determine maximum solubility. It then describes different types of structural imperfections, including point, line, and planar defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170193
EISBN: 978-1-62708-297-6
...Abstract Abstract This article discusses the effect of alloying on high-strength low-alloy (HSLA) steels. It explains where HSLA steels fit in the continuum of commercial steels and describes the six general categories into which they are divided. It provides composition data for standard types...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240411
EISBN: 978-1-62708-251-8
... work tool steels, low-alloy special-purpose tool steels, mold tool steels, high-speed tool steels, and powder metallurgy tool steels. This chapter provides discusses the manufacturing process, composition, properties, types, and applications of these tool steels and other cutting tool materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440191
EISBN: 978-1-62708-262-4
... by the manufacturer. Five steels are listed by AISI under the symbol S, although only the two most widely used grades are shown in Table 1 (S1 and S5). There is a considerable difference between the compositions of S1 and S5, as shown in Table 1 . However, they are both intended for similar applications...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290201
EISBN: 978-1-62708-319-5
...Nominal 17-4 PH composition for wrought and powder alloys Table 10.1 Nominal 17-4 PH composition for wrought and powder alloys Alloy form Composition, wt% Cr Ni Cu Si Mn Nb + Ta C Wrought 15.5 4.5 3.5 0.5 0.4 0.3 0.04 Powder 16.5 4.0 4.0 1 max 1 max 0.3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560039
EISBN: 978-1-62708-291-4
... the composition and structure of low-carbon irons and steels, particularly those used in the production of hot-rolled strip. It describes the manufacturing process from the production of ingots to coiling, and it explains how finishing and coiling temperatures affect ferritic grain size and the distribution...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550621
EISBN: 978-1-62708-307-2
... alternative names Material component designations (composite/assembly) Material production history Manufacturability strengths and limitations Material composition(s) Material condition (fabrication) Material assembly technology Constitutive equations relating to properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.9781627083492
EISBN: 978-1-62708-349-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... Laying for Affordable Manufacturing of Large Composite Structures , 46th International SAMPE Symposium , May 2001 , p 2484 – 2494 4. Evans D.O. , Fiber Placement , ASM Handbook , Vol 21 , Composites , ASM International , 2001 , p 477 – 479 10.31399/asm.hb.v21.a0003410 5...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170596
EISBN: 978-1-62708-297-6
... that make and break electrical circuits. Contacts are made of either elemental metals or alloys made by the melt-cast method or composites manufactured by powder metallurgy (P/M) processes. Powder metallurgy facilitates combinations of metals that ordinarily cannot be achieved by conventional alloying...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870307
EISBN: 978-1-62708-314-0
... structures hole drilling mechanical fasteners sealing trimming COMPOSITES ALLOW for the manufacture of large integral structures, thereby reducing the number of parts and mechanical fasteners required to assemble them. Many structures can be either cocured or bonded together to integrate...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120131
EISBN: 978-1-62708-269-3
... of change in the business climate. New alloys are no longer coming from the producers with much regularity. Virtually all the more recently applied conventional alloys were invented prior to 1990. Ti-6Al-4V alloy, around for nearly a half century, is still the most-used composition. Manufacturers...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870101
EISBN: 978-1-62708-314-0
... of the basics of bond tools for composites, primarily for autoclave curing. As other composite manufacturing processes are introduced in later chapters, additional tooling information specific to those processes will be presented. Tooling for composite structures is a complex discipline in its own right...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860035
EISBN: 978-1-62708-338-6
... of Liverpool ) 4.9 Eckold G.C. and Wells G.M. , Computer Aided Design and Manufacture of Advanced Composites , Proceedings of Second Conference on Materials Engineering, I. Mech. E. & P.R.I. , Nov 5–7, 1985 4.10 Ulrich R. and Friedrich R. , Fiber Reinforced Plastic...