1-20 of 472 Search Results for

composite fracture properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610327
EISBN: 978-1-62708-303-4
...Abstract Abstract This chapter covers the fatigue and fracture behaviors of ceramics and polymers. It discusses the benefits of transformation toughening, the use of ceramic-matrix composites, fracture mechanisms, and the relationship between fatigue and subcritical crack growth. In regard...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770011
EISBN: 978-1-62708-337-9
... gradients. It describes how these changes influence the development of high-temperature transformation products as well as microstructure, hardenability, and carbon content and properties such as fatigue and fracture behaviors, hardness, and wear resistance. It also explains how to manage internal oxidation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170123
EISBN: 978-1-62708-297-6
... the effect of alloying on structure and composition and explains how alloy content can be controlled to optimize properties and behaviors such as ductility, strength, toughness, fatigue and fracture resistance, and resistance to corrosion, wear, and high-temperature creep. It also examines the effect...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090043
EISBN: 978-1-62708-266-2
... environments. It explains how composition and microstructure influence SCC, as do mechanical properties such as strength and fracture toughness and processes such as welding and cold work. It also discusses the role of materials selection and best practices for welding. carbon steel low-alloy steel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140069
EISBN: 978-1-62708-335-5
... … 851.0 S, P 4 4 4 4 … 1 4 3 … … 5 3 5 … 852.0 S, P 4 4 4 4 … 1 4 3 … … 5 3 5 … Source: Ref 3 - 5 Typical physical properties of aluminum sand castings Table 8.2(a) Typical physical properties of aluminum sand castings Metric unit values generally derived...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.fdsm.t69870325
EISBN: 978-1-62708-344-7
... and ceramic fiber-reinforced metal-matrix composites. bone cyclic loading ceramics fatigue crack growth fatigue modeling fatigue properties fatigue test polymers Introduction Polymers Bone Ceramics Composite Materials References References 12.1 Ashby M.F...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540319
EISBN: 978-1-62708-309-6
... Fracture Toughness and Damage Tolerance ,” Report CP 3038, NASA, 1989 , p 75 – 89 8.51. Gause L.W. and Alpaer J.M. , “ Mechanical Properties of Magnaweave Composites ,” Report NADC-84030–60, Naval Air Development Center , 1983 8.52. Gause L.W. , Alpaer J.M...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480113
EISBN: 978-1-62708-318-8
... approach to lifing of a part (by assuming a preexisting crack) using the FCGR and the fracture toughness of the material is presented. The intermetallics Ti x Al (where x = 1 or 3) are discussed ( Ref 6.3 , 6.4 ) and their characteristics summarized. The properties of titanium metal-matrix composites...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ems.t53730115
EISBN: 978-1-62708-283-9
...Abstract Abstract This chapter discusses the properties and uses of fiber-reinforced composites. It also describes the effect of volume fraction and fiber length. fiber length fiber-reinforced composites WITH COMPOSITE MATERIALS, combinations of properties can be achieved that could...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170337
EISBN: 978-1-62708-297-6
..., chromium, and manganese), increase oxidation resistance (niobium and tantalum) or enhance combined properties. Table 8 lists tensile properties and fracture toughness of γ alloys as functions of composition, processing/microstructure, and temperature. Ternary alloys of Ti-48Al with approximately 1...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.9781627083096
EISBN: 978-1-62708-309-6
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240371
EISBN: 978-1-62708-251-8
... properties compared to plain carbonsteels as a result of alloying additions. This chapter describes the beneficial effects of these alloying elements in steels. It discusses the mechanical properties, nominal compositions, advantages, and engineering applications of various classes of alloy steels...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120095
EISBN: 978-1-62708-269-3
..., and property relationships in titanium alloys. It provides information on microstructures and strengthening mechanisms, the role of alloy and interstitial elements, and the effect of composition, processing, and surface treatments on tensile and yield strength, fracture toughness, hardness, ductility...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140175
EISBN: 978-1-62708-264-8
...Abstract Abstract This chapter discusses the composition, properties, microstructure, grain formation, and fracture behavior of gray, white, ductile, and malleable cast iron and how these critical factors are affected when iron is heated to different temperatures prior to or during...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230145
EISBN: 978-1-62708-298-3
... for several “metal-metal” glasses for which the composition is very nearly equiatomic. Mechanical properties of selected amorphous alloys with comparison to a beryllium amorphous alloy Table 12.1 Mechanical properties of selected amorphous alloys with comparison to a beryllium amorphous alloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
... by the following: Their processing methodology is similar to that of monolithic ceramics, and therefore, any increases in the cost of the composite relative to the monolithic should be small. Their mechanical and physical properties are approximately isotropic. Their fracture toughness is typically 25...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550299
EISBN: 978-1-62708-307-2
... slowly with temperature. Tensile properties and fracture toughness values of gamma titanium aluminides tested in air Table 6.6 Tensile properties and fracture toughness values of gamma titanium aluminides tested in air Alloy designation and composition, at. % Processing and microstructure...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060247
EISBN: 978-1-62708-261-7
... of the “steely” matrix. White and Gray Cast Irons Controlling the Eutectic Reaction Typical Cast Iron Compositions Matrix Microstructure Heat Treatment The historical classification of gray and white cast irons, based on fracture appearance, still applies today. Cast irons are also classified...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230163
EISBN: 978-1-62708-298-3
...Abstract Abstract This chapter discusses the composition, properties, and uses of the most common beryllium alloys and composites. It provides information on beryllium-aluminum, beryllium-copper, and beryllium-titanium as well as beryllium-antimony and beryllium-iron systems. alloying...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170234
EISBN: 978-1-62708-297-6
... how maraging steels typically have high levels of nickel, cobalt, and molybdenum with little carbon content and how that affects their dimensional stability, fracture toughness, weldability, and resistance to stress-corrosion cracking. maraging steel Composition Fracture toughness...