1-20 of 811 Search Results for

composite design

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By J. W. Ekin
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860465
EISBN: 978-1-62708-348-5
... material selection and the geometrical design of superconducting composites. The chapter also contains a reference guide to composite-design factors with links to the relevant chapter sections where each design consideration is addressed. magnetic field material selection superconducting composites...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550033
EISBN: 978-1-62708-307-2
... the advantages and limitations of various types of aluminum along with their compositions, designations, and achievable strengths. It explains how some alloys are hardened through solution strengthening and cold working, while others are strengthened by precipitation hardening. It also describes production...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090271
EISBN: 978-1-62708-266-2
... the nominal composition, designation, and grade of nearly two dozen commercial titanium alloys and the different types of media (including oxidizers, organic compounds, hot salt, and liquid metal) in which SCC has been observed. It discusses the mechanical and metallurgical factors that influence SCC behavior...
Book Chapter

By M. B. Kasen
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1983
DOI: 10.31399/asm.tb.mlt.t62860413
EISBN: 978-1-62708-348-5
...Abstract Abstract Composite systems for cryogenic applications are discussed in this chapter. This chapter emphasizes filamentary-reinforced composites because they are the most widely used composite materials. It begins with a discussion on the approach to designing and fabricating with low...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860115
EISBN: 978-1-62708-338-6
... design approach for typical domes Fig. 9.17 Mandrel loads during winding and cure Fig. 9.18 Typical helical patterns Fig. 9.16 Typical segmented metal mandrels Fig. 9.2 Composite pressure vessel nomenclature Composite case nomenclature Fwd and aft port...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... in casting alloys versus wrought alloys. This chapter provides information on specifications and widely used designation systems and alloy nomenclature for aluminum casting alloys. It describes the composition of seven basic families of aluminum casting alloys: aluminum-copper, aluminum-silicon-copper...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2016
DOI: 10.31399/asm.tb.ascaam.t59190vii
EISBN: 978-1-62708-296-9
...Abstract Abstract This chapter provides an overview of the microstructure-property relationships associated with aluminum-silicon alloys. It includes information on commercial designations and grades, phase compositions, solidification paths, alloying elements, and intermetallic phases. It also...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030137
EISBN: 978-1-62708-349-2
... content, ply orientation variability, foreign objects, and other factors can degrade the composite performance. Some of these variables can be controlled through tight quality-control standards, while others are a function of the design and manufacturing of the composite part ( Ref 1 ). The use of optical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860001
EISBN: 978-1-62708-338-6
... Analysis Increasingly better methods for composite analysis have given designers a quicker, more reliable answer for closed-form analysis. There are “B”-basis allowable data for fiber/resin combinations for 121 °C (250 °F)-curing prepreg for the aircraft composite component industry (e.g., AGATE...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870489
EISBN: 978-1-62708-314-0
... analysis codes and finite element modeling tools are available for detailed composite designs. Modern design is done on workstations with advanced computer-aided design (CAD)/computer-aided manufacturing (CAM) packages. Integrated product definition teams have more freedom with composite construction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2006
DOI: 10.31399/asm.tb.pht2.t51440097
EISBN: 978-1-62708-262-4
...Abstract Abstract This chapter explains the definition of carbon steels and lists the Unified Numbering System designations and the compositions that are universally accepted by steel producers and fabricators. Compositions of higher hardenability carbon steels (higher manganese grades...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060273
EISBN: 978-1-62708-261-7
... Composition limits for the principal grades of wrought high-speed steel and tool steel alloys used in industrial applications Designation Composition (a) , % AISI UNS C Mn Si Cr Ni Mo W V Co Molybdenum high-speed steels M1 T11301 0.78–0.88 0.15–0.40 0.20–0.50 3.50–4.00 0.30...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
...Abstract Abstract This chapter is a collection of tables listing: cast alloy designations of Aluminum Association, along with their general applications; the chemical compositions of the frequently used alloys for gravity permanent molds, low-pressure permanent molds, squeeze castings, and die...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030193
EISBN: 978-1-62708-349-2
.... Higher-velocity impacts usually create a more catastrophic damage and can result in holes through the thickness of the composite, and therefore, visible damage. Accordingly, the mechanism of how composites fail is determined by the impact parameters, material characteristics, and composite design...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
...Abstract Abstract The objective of mechanical testing of an engineered material is to provide data necessary for the analysis, design, and fabrication of structural components using the material. The testing of filament-wound composite materials offers unique challenges because of the special...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.omfrc.t53030177
EISBN: 978-1-62708-349-2
...Abstract Abstract The second-generation composite materials were added to increase the strain to failure of the primary phase and/or create a dispersed second phase, thereby enhancing the fracture toughness of the thermosetting matrix. These matrices offered novel design capabilities...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870119
EISBN: 978-1-62708-314-0
... , Composites , ASM International , 1987 , p 519 – 528 13. Gutowski T.G. , Cost, Automation, and Design , Advanced Composites Manufacturing , John Wiley & Sons, Inc. , 1997 14. Poe C.C. , Dexter H.B. , and Raju L.S. , “ A Review of the NASA Textile Composites...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170528
EISBN: 978-1-62708-297-6
... and properties of lead used in battery grids, type metals, and bearings. It, likewise, discusses the use of tin in various types of solder and in bearings and provides composition and property data for application-specific designations and grades. The article also discusses the effect of impurities in tin-lead...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870179
EISBN: 978-1-62708-299-0
... corrosion characteristics of aluminum metal-matrix composites (MMCs), including composites formed with boron, graphite, silicon carbide, aluminum oxide, and mica. It also discusses the effect of stress-corrosion cracking on graphite-aluminum composites and the use of protective coatings and design criteria...