... Abstract This appendix is a compilation of suggested analysis methods for suspected component failure causes. component failure causes failure analysis Table A.1   Suspected component failure cause Suggested analysis method Nonconforming dimensions Dimensional...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130001
EISBN: 978-1-62708-284-6
... Abstract A systematic procedure for minimizing risks involved in heat treated steel components requires a combination of metallurgical failure analysis and fitness for service with respect to safety and reliability based on risk analysis. This chapter begins with an overview of heat treat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130351
EISBN: 978-1-62708-284-6
... Abstract This chapter presents various case histories that illustrate a variety of failure mechanisms experienced by the high-strength steel components in aerospace applications. The components covered are catapult holdback bar, AISI 420 stainless steel roll pin, main landing gear (MLG) lever...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410009
EISBN: 978-1-62708-280-8
... This chapter is a brief account of various factors pertinent to the development of an engineering component. The discussion covers the disciplines and interactions of design development, engineering of component design, validation of design and process analysis, and matrix of design and manufacturing elements...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290193
EISBN: 978-1-62708-319-5
... procedure. Mechanical hardness and strength tabulations are provided to document sintered properties. mechanical properties performance test sintering Sintering produces a strong engineering component. Properties are dominated by composition, such as the high density associated with tungsten...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270165
EISBN: 978-1-62708-301-0
... Abstract Two filtration components installed on a developmental aircraft cracked during pressure impulse testing. Both parts were made from an aluminum alloy, solutionized and aged, and cracked due to fatigue. In both cases, the crack initiated at a transition region on an inner surface...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 November 2013
DOI: 10.31399/asm.tb.uhcf3.9781627082709
EISBN: 978-1-62708-270-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130177
EISBN: 978-1-62708-284-6
... Abstract This chapter provides information on various contributors to failure of carburized and carbonitrided components, with the primary focus on carburized components. The most common contributors covered include component design, selection of proper hardenability, increased residual stress...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130395
EISBN: 978-1-62708-284-6
... analysis case hardening powder metal steel components POWDER METALLURGY (PM) technology provides a cost-effective method of producing near-net shape products, especially when a large number of the same or similar products are required. While the initial powder used is expensive compared to wrought...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230513
EISBN: 978-1-62708-298-3
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.9781627082846
EISBN: 978-1-62708-284-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130043
EISBN: 978-1-62708-284-6
... Abstract This chapter provides an overview of the possible mechanisms of failure for heat treated steel components and discusses the techniques for examining fractures, ductile and brittle failures, intergranular failure mechanisms, and fatigue. It begins with a description of the general...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
... Abstract This chapter focuses on common failure characteristics exhibited by mechanical and electrical components. The topic is considered from two perspectives: one possibility is that the system failed because parts were nonconforming to drawing requirements and another possibility...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110524
EISBN: 978-1-62708-247-1
... Abstract Optoelectronic components can be readily classified as active light-emitting components (such as semiconductor lasers and light emitting diodes), electrically active but non-emitting components, and inactive components. This chapter focuses on the first category, and particularly...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110587
EISBN: 978-1-62708-247-1
... Abstract Passive components can be broadly divided into capacitors, resistors, and inductors. Failure analysis of these components helps determine the root cause and improve the overall quality and reliability of the electronic systems. This article describes different failure analysis...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780093
EISBN: 978-1-62708-268-6
... Abstract After the fault-tree, a failure-cause identification method has identified potential failure causes and the failure analysis team has prepared a failure mode assessment and assignment (FMA&A). The team knows specifically what to search for when examining components...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
... Abstract This chapter discusses various factors pertinent to the applications of low-pressure permanent mold casting process, namely decorative automotive wheels, critical safety structural components, and chassis components. low-pressure permanent mold castings decorative automotive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270162
EISBN: 978-1-62708-301-0
... Abstract Several components from the tail boom of a helicopter were found fractured at a crash site, including gusset plates, the hat section near the lower yoke, and a cable that controls the pitch of the tail rotor. The components were recovered from the wreckage and taken to a lab for closer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310225
EISBN: 978-1-62708-286-0
... Abstract This chapter is a detailed account of the applications of stainless steel in automotive and transport systems. The discussion covers exhaust systems, structural components, automotive components, trucks, and rail transport. stainless steel automotive exhaust systems automotive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460277
EISBN: 978-1-62708-285-3
... Abstract This chapter focuses on high-pressure cold spray applications pertaining to repair and refurbishment in the aerospace, oil and gas, and power-generation industries, the last specifically involving repair of gas turbine components. Advantages of cold spray coating in the repair...