..., malleable iron, compacted graphite iron (CGI), ductile iron, austempered ductile iron (ADI), and carbon steel and low-alloy steel; its versatile attributes; and its individual applications. A large section of the chapter covers the impact of electric vehicles on the future of the iron and steel castings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320207
EISBN: 978-1-62708-332-4
... standards for CGI are provided. The chapter describes the critical factors that control CGI and discusses methods of CGI manufacturing. carbon compacted graphite iron ductile iron iron castings mechanical properties silicon thermal properties COMPACTED GRAPHITE IRON (GCI) is a cast iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320031
EISBN: 978-1-62708-332-4
..., for applications where stiffness is the key requirement, gray iron and ductile iron should be considered (as well as compacted graphite iron, CGI). Fig. 4.12 Comparison of properties of gray iron, malleable iron, ductile iron, and steel. Source: Ref 9 4.14.1 Gray Iron Versatility Gray iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.9781627083324
EISBN: 978-1-62708-332-4
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220583
EISBN: 978-1-62708-259-4
..., and examines the growth mechanisms and structural details that set them apart. It also discusses the formation of compacted (vermicular) graphite and malleable iron, and compares and contrasts the composition, properties, and heat treatment of whiteheart and blackheart malleable types. chilled cast iron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320323
EISBN: 978-1-62708-332-4
.... Metallographic examination of austempered ductile iron is done to examine the ausferrite and the retained austenite (see Chapter 10 , “ Engineering Austempered Ductile Iron Castings ,” in this book). CGI (e.g., cylinder blocks) is examined for limited nodularity, as detailed in Chapter 10 . Steel castings...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390456
EISBN: 978-1-62708-459-8
... steels, called free-machining steels ( Sec. 13.7.1 ) [ 40 – 43 ]. The formation of Al 2 O 3 layers on CBN has been used to explain the improved machinablility of certain cast irons [ 44 ]. Many other examples exist, such as various SiO-containing tribolayers on a TiN-coated carbide tool when machining...