1-20 of 210 Search Results for

cobalt-base corrosion-resistant alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300227
EISBN: 978-1-62708-323-2
... subjected to liquid, droplet, and solid particle erosion. It also discusses the tribology of nickel- and cobalt-base alloys as well as titanium, zinc, tin, aluminum, magnesium, beryllium, graphite, and different types of wood. alloy composition cobalt-base alloys corrosion-resistant metals friction...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000001
EISBN: 978-1-62708-313-3
... Containing Iron, Chromium, and Aluminum , U.S. Patent 3,542,530 , 1970 13. Evans D. and Elam R. , Cobalt Base Coating for the Superalloys , U.S. Patent 3,676,085 , 1972 14. Goward G. , Boone D. , and Pettit F. , High-Temperature Oxidation-Resistant Coating Alloy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000009
EISBN: 978-1-62708-313-3
... wrought alloys. (Haynes 25 and S-816 are also available in cast form.) Typical applications for cobalt-base superalloys in GTEs are vanes and other stationary components, due to their superior stress-rupture properties and hot corrosion resistance. Cobalt-base superalloys can also be used to fabricate GTE...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000059
EISBN: 978-1-62708-313-3
... working B, C Fe, Ni 3 Ti, B, C Fe, B, C Retards γ′ coarsening … … Re Source: Ref 1 , 2 Table 5.3 Effects of notable alloying elements in superalloys Element Nickel-iron base Cobalt base Nickel base Cr Improves hot corrosion and oxidation resistance Solid...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000025
EISBN: 978-1-62708-313-3
.... Jiang W.H. , Yao X.D. , Guan H.R. , and Hu Z.Q. , Secondary M 6 C Precipitation in a Cobalt-Base Superalloy , J. Mater. Sci. Lett. , Vol 18 , 1999 , p 303 – 305 23. Microstructure of Wrought Heat-Resisting Alloys , Atlas of Microstructures of Industrial Alloys , Vol 7...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000017
EISBN: 978-1-62708-313-3
... Properties of a Mechanically Alloyed Oxide Dispersion-Strengthened Nickel-Base Superalloy , J. Mater. Sci. , Vol 33 , 1998 , p 3361 – 3370 10.1023/A:1013293515482 8. Davis J. , Nickel, Cobalt, and Their Alloys, ASM Specialty Handbook , ASM International , 2000 9. Park L.J...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.sap.t53000117
EISBN: 978-1-62708-313-3
.... , Three-Phase Controlled Expansion Superalloys with Oxidation Resistance , Superalloys 1992 , Antolovich S.D. et al. , Ed., TMS , 1992 , p 217 – 226 10.7449/1992/Superalloys_1992_217_226 11. Davis J. , Nickel, Cobalt, and Their Alloys, ASM Specialty Handbook , ASM International...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240547
EISBN: 978-1-62708-251-8
... that lead to increased hardness, elevated temperature strength, creep resistance, and resistance to abrasive wear. Cobalt-base alloys may be grouped as wear-resistant, corrosion-resistant, or heat-resistant alloys. The single largest application of cobalt-base alloys is for wear resistance. In heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080249
EISBN: 978-1-62708-304-1
... Abstract This chapter examines the hot corrosion resistance of various nickel- and cobalt-base alloys in gas turbines susceptible to high-temperature (Type I) and low-temperature (Type II) hot corrosion. Type I hot corrosion is typically characterized by a thick, porous layer of oxides with the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170540
EISBN: 978-1-62708-297-6
... carbides affect toughness, hardness, ductility, and strength as well as resistance to heat, corrosion, and wear. cobalt-base corrosion-resistant alloys cobalt-base heat resistant alloys cobalt-base wear-resistant alloys Composition Selected References • Cobalt-Base Alloys...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080445
EISBN: 978-1-62708-304-1
... Abstract This appendix is a collection of tables listing the chemical compositions of wrought ferritic steels; wrought stainless steels; cast corrosion- and heat-resistant alloys; wrought iron-, nickel-, and cobalt-base alloys; cast nickel- and cobalt-base alloys; oxide-dispersion-strengthened...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030074
EISBN: 978-1-62708-282-2
... alloy composition for heat-resistant alloys, nickel corrosion-resistant alloys, and nickel-base alloys. This chapter also discusses the corrosion implications of changing the alloy microstructure via solid-state transformation, second-phase precipitation, or cold work. It concludes with a comparison of...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030176
EISBN: 978-1-62708-282-2
... Abstract Stainless steels and nickel-base alloys are recognized for their resistance to general corrosion and other categories of corrosion. This chapter examines the effects of specific alloying elements, metallurgical structure, and mechanical conditioning on the corrosion resistance of these...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170457
EISBN: 978-1-62708-297-6
... Stress-Corrosion Cracking of Some Copper-base Alloys , Trans. AIME , Vol 185 , 1949 , p 100 10.1007/BF03398082 2. Pugh E.N. , Craig J.V. , and Sedriks A.J. , The Stress-Corrosion Cracking of Copper, Silver, and Gold Alloys , in Proc. Conf. Fundamental Aspects of Stress...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550223
EISBN: 978-1-62708-307-2
... nickel-base superalloys, yielding excellent strength-to-weight ratios. Fatigue strength . Titanium alloys have much better fatigue strength than aluminum alloys and are frequently used for highly loaded bulkheads and frames in fighter aircraft. Operating temperature capability . When the...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170495
EISBN: 978-1-62708-297-6
... element in materials designed for aqueous corrosion resistance. On the other hand, cobalt imparts unique strengthening characteristics to alloys designed for high-temperature service. Cobalt, like iron, increases the solubility of carbon in nickel-base alloys, and this increases resistance to...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170550
EISBN: 978-1-62708-297-6
... for soft inlays are gold-silver-palladium types. Gold content in dental alloys generally ranges between approximately 50 and 88%. Gold brazing alloys are used for joining jet and rocket engine components made from nickel-or cobalt-base superalloys or stainless steel. Here, joint ductility is high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
... steels) typically do not exhibit any detectable stage I fatigue crack growth. Notches, sharp corners, or preexisting cracks can also eliminate detectable stage I propagation in many metals. Similarly, some alloys (such as certain nickel-base superalloys and cobalt-base alloys) can display very extensive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2017
DOI: 10.31399/asm.tb.sccmpe2.t55090135
EISBN: 978-1-62708-266-2
... Applications to the Environmental Stress Cracking of Nickel-Base and Cobalt-Base Alloys , Stress Corrosion Cracking—The Slow Strain Rate Technique , STP 665, Ugianski G.M. and Payer J. , Ed., ASTM , 1979 , p 279 – 293 10.1520/STP38121S 5.147 Wilson I.L.W. and Aspden R.G...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2001
DOI: 10.31399/asm.tb.aub.t61170614
EISBN: 978-1-62708-297-6
... Traction control Alnicos are a family of low-cost iron-base alloys containing aluminum, nickel, and cobalt. Various other elements are often added to Alnicos. For example, to lessen the deleterious effect of carbon, carbide stabilizers such as titanium or niobium may be added. Titanium and...