1-3 of 3 Search Results for

coaxial cable connectors

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220185
EISBN: 978-1-62708-341-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780164
EISBN: 978-1-62708-281-5
... Rectangular … A = ( a + g ) ( b + g ) … Square … A = ( a + g ) 2 … Tubes … A = π D 0 ( L + g ) … Cables ρ r = 2 π LR v ln D 2 D 1 … γ r = ln D 2 D 1 2 π LR v...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5