1-20 of 479 Search Results for

coating selection

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500317
EISBN: 978-1-62708-317-1
... hardening, case (surface) hardening, and nitriding as well as hard chrome plating, vapor deposition, and thermal diffusion coating. It explains how to measure wear resistance using various tests and provides guidelines for selecting tool materials, treatments, and coatings. chemical vapor deposition...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
..., and ceramic coatings and various pack cementation and deposition processes. It also discusses the selection and use of industrial paints and paint application methods. buffing cleaning coating honing mass finishing SURFACE FINISHES AND COATINGS are used in a variety of ways to improve...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... by three basic mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460253
EISBN: 978-1-62708-285-3
... Mark II UFC mock-up configurations through activities involving powder selection, general coating development, UFC coating optimization, and prototyping. Canadian nuclear industry copper coatings used-fuel canisters cold spray coatings THE NUCLEAR WASTE MANAGEMENT ORGANIZATION (NWMO...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300421
EISBN: 978-1-62708-323-2
...Abstract Abstract This chapter provides guidelines and insights on the selection of materials, coatings, and treatments for friction and wear applications. It begins with a review of the system nature of tribological effects, the subtleties of friction, and the selection idiosyncrasies...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030247
EISBN: 978-1-62708-282-2
... to corrosion as encountered in applications involving oil and gas exploration and production. This is followed by a section reviewing the methods of corrosion control, namely the proper selection of materials, protective coatings, cathodic protection systems, use of inhibitors, use of nonmetallic materials...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
..., and appearance of the corroded metal. It discusses five primary methods of corrosion control, namely, material selection, coatings, inhibitors, cathodic protection, and design. Examples of the opportunities in corrosion control and the means to implement a program to capitalize on those opportunities...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280365
EISBN: 978-1-62708-267-9
... This appendix includes selected references on topics related to the production and application of superalloys, including properties and microstructure; melting/ingot breakdown; forging/powder metallurgy; machining, heat treating, joining, refurbishment/repair; investment casting; coatings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350011
EISBN: 978-1-62708-315-7
... discusses the selection and use of protective coatings and the tests that have been developed to measure their effectiveness. References References 1. Corrosion of Steels in Waters , ASM Specialty Handbook: Carbon and Alloys Steels , Davis J.R. , Ed., ASM International , 1996 , p 408...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
..., physical vapor deposition; CVD, chemical vapor deposition. Source: Ref 1 Summary of design limitations for selected organic coating processes Table 5 Summary of design limitations for selected organic coating processes Process Design limitations Electrocoating Allow for electrical...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Availability Corrosion Resistance Wear Resistance Cost of Surface Treatments Distortion or Size Change Tendencies Coating Thickness Attainable PROCESS COMPARISONS discussed in this chapter include: One of the key considerations in the materials selection process is material availability...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240563
EISBN: 978-1-62708-251-8
... in temperatures on superalloy surfaces. Coating selection is based on knowledge of oxidation/corrosion behavior in laboratory, pilot-plant, and field tests. Attributes that probably will be required for successful coating selection include: High resistance to oxidation and/or hot corrosion Ductility...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... of alloy by generic type is required. Almost any alloy can be plated. Operating environment of finished component Must be known before coating material selection can be made Need not be known. It is usually sufficient to match the properties of the base metal. Usually not required in machinery...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460227
EISBN: 978-1-62708-285-3
..., and are difficult to use on selected areas. High-temperature thermal spray processes can also create high residual stresses and can result in coatings with poor adhesion strength. The cold spray process, with its low deposition temperatures and high adhesion strengths, is an ideal method for repairing aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
... enamels are available in summer or winter grades. These enamels are the corrosion coating; they are combined with various combinations of fiberglass and/or felt to obtain mechanical strength for handling. The enamel coatings have been the workhorse coatings of the industry, and when properly selected...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910331
EISBN: 978-1-62708-250-1
...Abstract Abstract The challenge of materials selection is to achieve adequate performance at the lowest possible cost. Corrosion resistance is not the only property to be considered in making materials selections. Typical requirements and some of the procedures involved in making a selection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1989
DOI: 10.31399/asm.tb.dmlahtc.t60490415
EISBN: 978-1-62708-340-9
... Factor Basis of estimate Scatter in assumed material properties:      Cast material 20 Fig. 9.45 ; Ref 57 16 Ref 75      Wrought material 10 J 10 J Effect of coatings in air (if present) None Fig. 9.45 ; Ref 57 3 Fig. 9.32 ; Ref 25 Effect of hot corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
.../STP664-EB • Bayer R.G. , Ed., Selection on Use of Wear Tests for Coatings , American Society for Testing and Materials , West Conshohocken, PA , 1981 10.1520/STP769-EB • Budinski K. , Surface Engineering for Wear Resistance , Prentice Hall , Reston, VA , 1980...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080003
EISBN: 978-1-62708-304-1
...Abstract Abstract This chapter explains how materials selection becomes much more difficult when designing for high-temperature corrosion environments. It also discusses the use of cladding and weld overlays to compensate for material deficiencies and prolong service life. corrosion...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350001
EISBN: 978-1-62708-315-7
... Applying organic, metallic, or inorganic (glasses and ceramics) coatings Application of corrosion-resistant coatings is one of the most widely used means of protecting steel. As shown in Table 1 , there are a wide variety of coatings to choose from, and proper selection is based on the component...