1-20 of 722 Search Results for

coating process

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 01 March 2002
Fig. 13.18 Flow diagram for typical pack diffusion coating process More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230361
EISBN: 978-1-62708-298-3
... in the deposits. In attempting to classify the different coating processes under various categories, difficulties arise since some of the processes overlap the different categories. Accordingly, different classification schemes exist [ Bunshah 1982 ]. In addition, many of these processes are not applicable...
Image
Published: 01 August 2012
Fig. 16.14 Typical coating thicknesses and process temperature for common coating methods. CVD, chemical vapor deposition; TD, thermal diffusion; PVD, physical vapor deposition. Source: Ref 16.54 More
Image
Published: 01 August 2013
Fig. 5.7 The continuous annealing line (CAL) process for producing coated DP Steel. Source: Adapted from Ref 5.5 More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... mechanisms: barrier protection, chemical inhibition, and galvanic (sacrificial) protection. This chapter begins with a section on organic coating and linings, providing a detailed account of the steps involved in the coating process, namely, design and selection, surface preparation, application...
Image
Published: 01 June 2016
Fig. 2.18 Optical micrographs of cold-sprayed copper coatings on thermally sprayed Al 2 O 3 coatings. (a) Copper on a cold-sprayed aluminum bond coat, processed onto a D-gun-sprayed Al 2 O 3 coating using a nonheated substrate. (b) Copper directly cold sprayed onto a suspension high-velocity More
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2022
DOI: 10.31399/asm.tb.dsktmse.t56050001
EISBN: 978-1-62708-432-1
.... It discusses the mechanisms behind interstitial, substitutional, grain boundary, and surface diffusion, the derivation and use of Fick’s laws, and the basic principles of diffusion coating processes, including carburizing, nitriding, nitrocarburizing, cyaniding, carbonitriding, boriding, aluminizing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040020
EISBN: 978-1-62708-428-4
... and engineering industries. It is being developed continuously to meet market evolution and new requirements. This evolution raises challenges that must be addressed for the advancement of thermal spray processes and coatings, and to direct academic research into promising industrial applications that offer...
Image
Published: 01 March 2001
Fig. 3 Some examples of line-of-sight limitations in spraying or ion-beam coating processes More
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350195
EISBN: 978-1-62708-315-7
... operations may be required before or after processing and how to estimate or predict coating thickness, case depth, hardness, and the likelihood of distortion. It also addresses related issues and considerations such as part handling and fixturing, surface preparation and cleaning requirements...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350183
EISBN: 978-1-62708-315-7
... Abstract This chapter compares and contrasts surface-engineering processes based on process availability, corrosion and wear performance, distortion effects, penetration depth or attainable coating thickness, and cost. It provides both quantitative and qualitative information as well...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300335
EISBN: 978-1-62708-323-2
... significant thickness (microns), and their role is to help establish separating tribofilms in lubricated tribosystems. Steel and cast iron gears were widely treated with this process to establish conformability. This simple dip coating could easily double the wear life of treated tribocomponents. The coating...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... This chapter describes surface modification processes that go beyond conventional heat treatments, including plasma nitriding, plasma carburizing, low-pressure carburizing, ion implantation, physical and chemical vapor deposition, salt bath coating, and transformation hardening via high-energy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... be cleaned of a coating and, furthermore, easily inspected for complete coating removal and/or underlying alloy damage. Internal passages, such as the cooling passages in gas turbine engine airfoils, are a more challenging task. Removal processes have more constraints, and inspection is limited. Because...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350125
EISBN: 978-1-62708-315-7
... Abstract This chapter discusses the use of coating methods and materials and their impact on corrosion and wear behaviors. It provides detailed engineering information on a wide range of processes, including organic, ceramic, and hot dip coating, metal plating and cladding, and the use of weld...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2022
DOI: 10.31399/asm.tb.tstap.t56040010
EISBN: 978-1-62708-428-4
... process, a combustible gas serves as the heat source that melts the coating material, which may be in rod, wire, or powder form. Commonly selected gases include acetylene, propane, methyl-acetylene-propadiene (MAPP) gas, and hydrogen, along with oxygen. In general, changing the nozzle and/or air cap...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.t56060001
EISBN: 978-1-62708-440-6
... Abstract This chapter presents the theory and practice associated with the application of thin films. The first half of the chapter describes physical deposition processes in which functional coatings are deposited on component surfaces using mechanical, electromechanical, or thermodynamic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.tb.hpcspa.t54460121
EISBN: 978-1-62708-285-3
... Abstract This chapter elucidates the indispensable role of characterization in the development of cold-sprayed coatings and illustrates some of the common processes used during coatings development. Emphasis is placed on the advanced microstructural characterization techniques that are used...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 1998
DOI: 10.31399/asm.tb.ts5.t65900305
EISBN: 978-1-62708-358-4
... Abstract Surface modification technologies improve the performance of tool steels. This chapter discusses the processes involved in oxide coatings, nitriding, ion implantation, chemical and physical vapor deposition processing, salt bath coating, laser and electron beam surface modification...
Series: ASM Technical Books
Publisher: ASM International
Published: 31 January 2023
DOI: 10.31399/asm.tb.itfdtktmse.9781627084406
EISBN: 978-1-62708-440-6