1-20 of 390 Search Results for

coating defects

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
... the soil accelerates corrosion of the pipe wall at the discharge point, causing stray current corrosion. The morphology of stray current corrosion tends to be very localized at holidays (defects or holes) in the pipeline coating. Rates of attack can be very high, resulting in rapid perforation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030360
EISBN: 978-1-62708-282-2
... access difficult. Internal coatings can be damaged while accessing the internal surfaces. Cannot be done through coating (although the coating itself can be examined) Noninvasive Inspection Noninvasive inspection techniques make it possible to test material for corrosion or defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050173
EISBN: 978-1-62708-311-9
... and defects associated with various quenchants and processing atmospheres and provides insights on how they can be removed and, in some cases, prevented. It also recommends the application of a rust preventative shortly after parts have cooled. cleaning rust protection WORKPIECES MAY NEED CLEANING...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350011
EISBN: 978-1-62708-315-7
... metals likely to be affected. It also discusses the selection and use of protective coatings and the tests that have been developed to measure their effectiveness. corrosion control corrosion testing electrochemical corrosion CORROSION of metal is a chemical or electrochemical process...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 1997
DOI: 10.31399/asm.tb.wip.t65930197
EISBN: 978-1-62708-359-1
... cables can cause arc burns. Careless handling of a cutting torch can result in flame gouging of a part. In hardenable alloys, arc strikes, arc burns, and flame gouges cause a variety of thermal responses that degrade the properties of base metal. These responses can include the generation of defects...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... of the specified coating system to the proper thickness Observation of application parameters, such as minimum and maximum temperatures, interval between coats, and coating thickness Verification of proper hardening or cure of the coating Testing to ensure that defects such as pinholes, skips, or holidays...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 1988
DOI: 10.31399/asm.tb.eihdca.t65220001
EISBN: 978-1-62708-341-6
.... Curing of Organic Coatings Induction is used to cure organic coatings such as paints on metallic substrates by generating heat within the substrate. By this means, curing occurs from within, minimizing the tendency for formation of coating defects. A typical application is the drying of paint...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110402
EISBN: 978-1-62708-247-1
... conditional/possible follow-up analyses) based on information provided by the customer, and the possible implications that these factors have on sample preparation methods to be used. These considerations are crucial prior to selecting downsizing and cross-sectioning method(s), coatings, and/or chemical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500211
EISBN: 978-1-62708-317-1
.... It explains how to determine strip width and bending sequences and identifies the cause of common roll-forming defects. It also discusses the selection of roll materials and explains how software helps simplify the design of roll forming lines. forming equipment roll forming IN ITS GENERAL FORM...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 September 2023
DOI: 10.31399/asm.tb.stmflw.t59390284
EISBN: 978-1-62708-459-8
..., material flow, friction, die wear, heat generation, and lubrication requirements. The chapter also provides information on hydrostatic, friction-assisted, and severe plastic deformation extrusion processes, discusses the cause of instabilities and defects, and explains how to select and apply lubricants...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.tpmpa.t54480207
EISBN: 978-1-62708-318-8
... ingot structure can be worked with less danger of cracking. Protective Coatings Protective coatings are used on ingots and billets to lower surface contamination levels of hydrogen and oxygen and to help reduce the galling effect of the titanium on the forging die. Coatings are often...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... This chapter describes surface modification processes that go beyond conventional heat treatments, including plasma nitriding, plasma carburizing, low-pressure carburizing, ion implantation, physical and chemical vapor deposition, salt bath coating, and transformation hardening via high-energy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110603
EISBN: 978-1-62708-247-1
... inspection followed by material evaluation and characterization. These processes are typically followed by evaluation of the packages to identify defects, degradations, and failure mechanisms that are caused by the processes (e.g., cleaning, solder dipping of leads, reballing) used in creating counterfeit...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110461
EISBN: 978-1-62708-247-1
... Abstract The ultimate goal of the failure analysis process is to find physical evidence that can identify the root cause of the failure. Transmission electron microscopy (TEM) has emerged as a powerful tool to characterize subtle defects. This article discusses the sample preparation procedures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060385
EISBN: 978-1-62708-261-7
...-phosphorus alloy plating Ceramic (WC, CrC, aluminum oxide) or cobalt-base coatings applied by thermal spray processes ( Fig. 16.2 ) Physical vapor deposition (PVD) coatings such as TiN and TiAlN Fig. 16.2 Application of thermal spray coating on a shaft. Courtesy of ASB Industries, Inc...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2022
DOI: 10.31399/asm.tb.dsktmse.t56050001
EISBN: 978-1-62708-432-1
.... It discusses the mechanisms behind interstitial, substitutional, grain boundary, and surface diffusion, the derivation and use of Fick’s laws, and the basic principles of diffusion coating processes, including carburizing, nitriding, nitrocarburizing, cyaniding, carbonitriding, boriding, aluminizing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110010
EISBN: 978-1-62708-247-1
..., and electro-optical terahertz pulse reflectometry. The final step is the step-by-step inspection and deprocessing stage that begins once the defect has been imaged. electrical verification electro-optical terahertz pulse reflectometry external optical inspection infrared microscopy IR lock...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.horfi.t51180061
EISBN: 978-1-62708-256-3
... tell from the table title whether the data apply to their situation. Causes of failures in some industry investigations Table 1 Causes of failures in some industry investigations Failure origin Percentage Improper material selection 37 Fabrication defects 16 Improper heat...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250257
EISBN: 978-1-62708-345-4
... Coatings , Gear Technology , July/Aug 1999 , p 35 – 44 7. Errichello R. , Tutorial: How to Analyze Gear Failures , Practical Failure Analysis , Vol 2 ( No. 6 ), December 2002 , p 8 – 16 10.1007/BF02715492 8. Miller B.A. , Overload Failures , Failure Analysis...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.tb.sfa.t52780109
EISBN: 978-1-62708-268-6
..., but humidity, sea spray, adhesives, and so forth may become unintended electrolytes. Insulatory materials (paint or other special coatings) can be used to inhibit or prevent galvanic corrosion; the absence or incorrect application of these coatings should be considered as potential galvanic corrosion causes...