1-20 of 88 Search Results for

coating characterization

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
... strength, is dependent on the materials and their properties and is generally characterized as a mechanical bond between the coating and the substrate, unlike the metallurgical bond found in weld-overlay coatings. Spray deposits can be applied in thinner layers than welded coatings, but thick deposits...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110447
EISBN: 978-1-62708-247-1
... Abstract There are several analytical methods available that can be used in-line on whole wafers as well as off-line on de-processed products that are returned from the field. These techniques are surface analytical techniques that can be used to characterize the bulk of the material. The main...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.tb.ssde.t52310181
EISBN: 978-1-62708-286-0
... information on high-speed tool steel and carbide tooling, along with tool coatings and coolants applicable to stainless steel. machinability stainless steel machining high-speed steel carbide tooling coolants tool coatings MACHINING STAINLESS STEELS is a complex operation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280287
EISBN: 978-1-62708-267-9
... protective coatings, including aluminide diffusion, overlay, and thermal barrier types, and how they perform in different environments based on their ability to tolerate strain. coatings corrosion resistance corrosion testing hot corrosion superalloys...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550193
EISBN: 978-1-62708-307-2
... coatings, and health and safety concerns. aluminum-beryllium alloys beryllium corrosion protection forming powder consolidation powder production BERYLLIUM is a metal with an unusual combination of physical and mechanical properties that make it particularly effective in optical components...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290243
EISBN: 978-1-62708-306-5
... information on the theory of adhesion. The chapter then describes the considerations for designing adhesively bonded joints and for testing or characterizing adhesive materials. The following section covers the characteristics of the most important synthetic adhesive systems and five groups of adhesives...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720021
EISBN: 978-1-62708-305-8
... Abstract Visual inspection is the most important method of inspection of materials. This chapter describes the procedures involved in visual inspection such as identification markings, identification of defects caused by heating problems, scaling of materials, cracking characterization, and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110603
EISBN: 978-1-62708-247-1
... inspection followed by material evaluation and characterization. These processes are typically followed by evaluation of the packages to identify defects, degradations, and failure mechanisms that are caused by the processes (e.g., cleaning, solder dipping of leads, reballing) used in creating counterfeit...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870063
EISBN: 978-1-62708-314-0
..., epoxy, bismaleimide, cyanate ester, polyimide, and phenolic resins and various toughening methods. The chapter also covers thermoplastic matrix materials and product forms and provides an introduction to the physiochemical tests used to characterize resins and cured laminates. physiochemical test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110461
EISBN: 978-1-62708-247-1
... Abstract The ultimate goal of the failure analysis process is to find physical evidence that can identify the root cause of the failure. Transmission electron microscopy (TEM) has emerged as a powerful tool to characterize subtle defects. This article discusses the sample preparation procedures...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290099
EISBN: 978-1-62708-306-5
... concentration due to weld shape and joint geometry; stress concentration due to weld imperfections; and residual welding stresses. Inspection and characterization of welds are described in the final section of this chapter. cast iron fusion welding residual stress solid-state transformation steel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2000
DOI: 10.31399/asm.tb.fec.9781627083027
EISBN: 978-1-62708-302-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.9781627083157
EISBN: 978-1-62708-315-7
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.t61280323
EISBN: 978-1-62708-267-9
... environments from those ordinarily experienced and may behave in a manner that could not have been predicted from normal test data. Failure may be separation or it may just be inability of a component to perform its mission. Not all failures are caused by cracking or fracture. If a coating is degraded, a...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110402
EISBN: 978-1-62708-247-1
... conditional/possible follow-up analyses) based on information provided by the customer, and the possible implications that these factors have on sample preparation methods to be used. These considerations are crucial prior to selecting downsizing and cross-sectioning method(s), coatings, and/or chemical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
... absorption. Therefore, proper control of the interface is critical. Coatings are often applied to protect the fibers during processing and to provide a weak fiber-to-matrix bond. Fig. 11.1 Comparison of polymer-matrix composites with ceramic-matrix composites. Source: Ref 11.1 Fig. 11.2...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550299
EISBN: 978-1-62708-307-2
..., face-centered cubic. Source: Ref 6.1 In addition to their low ductility at ambient temperatures, another negative feature of titanium aluminides is their oxidation resistance, which is lower than desirable at elevated temperatures. The titanium aluminides are characterized by a strong...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410029
EISBN: 978-1-62708-280-8
... and bonded by passing steam through the vents, filling the cavity. The parts of the foam pattern and the gating are assembled using glue. The assembly is dipped in a ceramic slurry and dried thoroughly. The coated and dried pattern assembly is held by a gripper in a flask while dry, unbonded silica...