... of plastics ( Ref 23 ). A wheel faced with a chlorobutyl rubber tire revolves against a stationary test specimen while a flow of sand is forced between the wheel and the specimen. The severity of the test is adjusted by varying test duration and the force with which the specimen is applied to the wheel...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.t59300301
EISBN: 978-1-62708-323-2
...-butadiene rubber (SBR) on the outside, but the inside may be lined with chlorobutyl rubber to better keep the air inside (lower permeability). Rubbers are used in tribology for bearings, belting, and all types of seals (such as O-rings). Second only to tires, a significant tribological use of rubber...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780164
EISBN: 978-1-62708-281-5
... Acrylonitrile-butadiene Electrical properties not outstanding; probably degraded by molecular polarity of acrylonitrile constituent IIR Butyl Isobutylene-isoprene Electrical properties generally good but not outstanding in any area IIR Chlorobutyl Chloroisobutylene-isoprene Same general properties...