Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
...Abstract Abstract This chapter discusses various factors pertinent to the applications of low-pressure permanent mold casting process, namely decorative automotive wheels, critical safety structural components, and chassis components. low-pressure permanent mold castings decorative...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700215
EISBN: 978-1-62708-279-2
.... Source: Adapted from Ref 14.4 Fig. 14.2 Gas metal arc welding (GMAW) process Fig. 14.3 Examples of welds for chassis structures. Source: Ref 14.5 Joint type Weld type Combination of joint and weld type Lap Fillet Lap Single/double-sided slot weld T-joint...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410001
EISBN: 978-1-62708-280-8
...Abstract Abstract Casting is one of the most economical manufacturing processes for providing shape to components of machinery and is used in a wide range of industries. This chapter is a brief account of the advantages, applications, limitations, and market growth of aluminum casting. It also...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700001
EISBN: 978-1-62708-279-2
... through strong material substitution appears to be the only viable route to significant vehicle weight reduction. This can be achieved by replacing heavy steel components in body structures, closure panels, chassis, wheels, bumpers, and suspension parts with lightweight materials made from ferrous...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980009
EISBN: 978-1-62708-342-3
... Trailer with planked construction and chassis in extruded aluminum sections. Source: Alusuisse Fig. 2.17 Tilting trailer walls of an open goods wagon finished in extruded hollow sections in the alloys AlMgSi0.5 and AlMgSi0.7. Source: Alusuisse Fig. 2.20 Older bus body manufactured from...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500083
EISBN: 978-1-62708-317-1
... castings. The drive train unit constitutes approximately 25% and the chassis and the body constitute nearly 50% of the total weight of a compact car ( Ref 5.33 ). Applications of die-cast components in chassis and body parts are limited, mainly because the mechanical properties of castings often do...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550001
EISBN: 978-1-62708-307-2
... applications. The dominance of steel in the automotive industry is being challenged by plastics and aluminum. In 2010, approximately 90 kg (200 lb) of aluminum was used in an average car made in the United States. The long-term goal of the aluminum community is an all-aluminum chassis, known as a “body...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870001
EISBN: 978-1-62708-299-0
.... Good weldability and resistance to corrosion. Uses include pressure vessels, fan blades, tanks, electronic panels, electronic chassis, medium-strength sheet metal parts, hydraulic tube, appliances, agricultural applications, architectural uses, automotive parts, building products, chemical equipment...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410091
EISBN: 978-1-62708-280-8
... Al Alloys with (Si+Mg), (Si+Cu), or (Si+Mg+Cu) 3XX.X Structural parts for chassis, engine and transmission components, automotive wheels, parts needing high-temperature strength, pressure-tight and leak-proof components, aircraft structures Al-Si alloys 4XX.X Nonheat treated parts. After...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140007
EISBN: 978-1-62708-335-5
... in a specific process to produce defect-free, sound castings. For gravity casting, the components of castability are generally considered to be fluidity as the measure of mold-filling capability, resistance to hot cracking during and after solidification, and feeding characteristics that promote the flow...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550621
EISBN: 978-1-62708-307-2
... primarily from mild steel. The term body-in-white refers to the stage in automobile manufacturing in which the car body sheet metal components have been welded together, but before moving parts (doors, hoods, and deck lids as well as fenders), the motor, chassis subassemblies, or trim (glass, seats...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... or protective layer on the reactive metal substrate. A coating system often is composed of multiple layers or multiple components within layers. The system can comprise a metal surface treatment, for example, a phosphate conversion coating, a primer, and a top coat. A desirable coating system provides...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.tb.ahsssta.t53700177
EISBN: 978-1-62708-279-2
... and die surface coating on tool life. Source: Ref 12.1 Fig. 12.19 Hot forming process. Source: Adapted from Ref 12.2 Fig. 12.21 Process conditions for resistance spot welding. Source: Adapted from Ref 12.12 Fig. 12.20 Principal components in resistance spot welding...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400073
EISBN: 978-1-62708-316-4
... quality; DQSK, drawing quality special killed; HR, hot rolled. Source: Ref 6.2 Drawing quality (DQ) materials are suitable for deep drawing of parts and formed components that require severe deformation. For very severe deformations, drawing quality special killed (DQSK) is specified. Generally...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870001
EISBN: 978-1-62708-314-0
... and includes application examples. anisotropic laminates orthotropic laminates A COMPOSITE MATERIAL can be defined as a combination of two or more materials that results in better properties than those of the individual components used alone. In contrast to metallic alloys, each material retains...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smff.t53400005
EISBN: 978-1-62708-316-4
... of the process and a bullet-point list identifying relevant equipment, materials, variations, and applications. The chapter also discusses critical process variables, interactions, and components and the classification of sheet metal parts based on geometry. bending blank preparation deep drawing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2008
DOI: 10.31399/asm.tb.fahtsc.t51130151
EISBN: 978-1-62708-284-6
... that had the fractured blade. (b) Detail of the fractured bottom component of the blade Fig. 28 Component drawing of the intermediate I axle. Highlighted are the section change region where the fracture developed and the crack propagation path for the total fracture of the axle. Fig. 24...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2012
DOI: 10.31399/asm.tb.smfpa.t53500179
EISBN: 978-1-62708-317-1
.../0924-0136(96)02403-X 9.23 Ahmed M. and Hashmi M.S.J. , Estimation of Machine Parameters for Hydraulic Bulge Forming of Tubular Components , J. Mater. Process. Technol. , Vol 64 ( No. 1–3 ), Feb 1997 , p 9 – 23 10.1016/S0924-0136(96)02549-6 9.24 Asnafi N...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060315
EISBN: 978-1-62708-261-7
... 5% elongation. Fig. 13.3 Pourbaix (potential-pH) diagram for the titanium-water system at 25 °C (77 °F). Fig. 13.6 Powder metallurgy nickel superalloy turbine disk component. Courtesy of Rolls-Royce Corporation Abstract Abstract Nonferrous metals are of commercial...