1-20 of 163 Search Results for

cathodic coating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910407
EISBN: 978-1-62708-250-1
..., the effects of the chemical reactions occurring at the surface of the protected structure, and the effects of cathodic protection on coatings. corrosion control cathodic protection anodic protection sacrificial cathodic protection systems impressed-current cathodic protection systems stray currents...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030165
EISBN: 978-1-62708-282-2
... so that it becomes the cathode (cathodic protection). This chapter briefly reviews these methods of corrosion protection. The factors affecting corrosion behavior are covered. In addition, the chapter provides information on coatings and inhibitors, which are used in corrosion protection...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030247
EISBN: 978-1-62708-282-2
... metals, for example, steel. Protective coatings are more difficult to maintain than in other zones. Tidal Marine fouling is apt to be present to high watermark. Oil coating from polluted harbor water may be present. Usually, ample oxygen is available. Steel at the tidal zone may act cathodically...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910001
EISBN: 978-1-62708-250-1
..., and appearance of the corroded metal. It discusses five primary methods of corrosion control, namely, material selection, coatings, inhibitors, cathodic protection, and design. Examples of the opportunities in corrosion control and the means to implement a program to capitalize on those opportunities...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910363
EISBN: 978-1-62708-250-1
... and/or too warm weather, especially with oil-based paints Scrape off wrinkles and apply thinner coat; avoid intense sunlight. Blistering Small to large broken or unbroken bubbles Solvent entrapment; oil, moisture, or salt-contaminated surfaces; or cathodic disbonding Blowers in enclosed areas...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030184
EISBN: 978-1-62708-282-2
... products. Much of the terminology of cathodic protection still relates to corrosion control of onshore buried steel pipelines. Virtually all modern pipelines are coated with an organic protective coating that is supplemented by cathodic protection systems sized to prevent corrosion at gaps or holidays...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2001
DOI: 10.31399/asm.tb.secwr.t68350011
EISBN: 978-1-62708-315-7
... help to satisfy the need for corrosion prevention. Special primers are used to provide passivation, galvanic protection, corrosion inhibition, or mechanical or electrical barriers to corrosive action. Corrosion Inhibitors Barrier Coatings Sacrificial Coatings Cathodic Protection Many...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030019
EISBN: 978-1-62708-282-2
..., depending on the configuration of the couple, the nature of the corrosion film produced, and the nature of the metals or alloys involved. Generally, there are five major categories. Dissimilar Metals Nonmetallic Conductors Metallic Coatings Cathodic Protection Metal Ion Deposition...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240323
EISBN: 978-1-62708-251-8
... ). Unfortunately, although steel also produces a surface film, the film is porous and does not adhere very well, so the corrosion continues. Uniform corrosion is normally prevented by selecting a metal that forms a protective film, by applying coatings that isolate the metal from the environment, or by cathodic...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2012
DOI: 10.31399/asm.tb.ffub.t53610501
EISBN: 978-1-62708-303-4
... particles or radicals possessing an electrical charge. The electrolyte is a conductive liquid through which the current is carried by positively charged ions (cations) to the cathode. Negatively charged ions (anions) are simultaneously attracted to the anode. Charged ions are present in solutions of acids...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030338
EISBN: 978-1-62708-282-2
... and abrasive cleaning Because of the relatively poor corrosion resistance of line pipe steels in underground environments, a combination of mitigation strategies consisting of coatings and cathodic protection (CP) is required. In this article, the most common causes and contributing factors...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.9781627082822
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.caaa.t67870075
EISBN: 978-1-62708-299-0
... Stress Corrosion with Sprayed Metal Coatings , Br. Corros. J. , Vol 4 , 1969 , p 15 10.1179/000705969798325749 13. Schwerdtfeger W.J. , Effects of Cathodic Protection on the Corrosion of an Aluminum Alloy , J. Res. Natl. Bur. Stand. , Vol 68C ( No. 4 ), 1964 , p 283 10.6028/jres...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740325
EISBN: 978-1-62708-308-9
...Abstract Abstract This chapter covers a wide range of finishing and coating operations, including cleaning, honing, polishing and buffing, and lapping. It discusses the use of rust-preventative compounds, conversion coatings, and plating metals as well as weld overlay, thermal spray...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910099
EISBN: 978-1-62708-250-1
... Films Velocity Impingement Influence of Galvanic Corrosion Nature of Metal or Alloy Heat Treatment Effects Design Environment Coatings Cathodic Protection General Description Mechanism <xref rid="t66910099-ref8" ref-type="bibr">(Ref 8)</xref> Appearance Prevention...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410551
EISBN: 978-1-62708-265-5
... or evaporative-source PVD coating, generates coating atoms by thermal evaporation from an appropriate source ( Ref 22.14 , 22.16 , 22.32 ). The source may be an electrically heated wire, an electron beam, or of hollow cathode design and is made the anode in the system. The substrate is made the cathode...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 July 2009
DOI: 10.31399/asm.tb.bcp.t52230459
EISBN: 978-1-62708-298-3
..., Battelle Memorial Institute , Columbus, OH Miller R.A. , Meyers J.R. , and Saxer R.K. , 1967 . Stress Corrosion of Beryllium in Synthetic Sea Water , Corrosion , Vol 23 , p 11 – 14 Morana S.J. , 1967 . “ Surface Passivation Coating for Beryllium Metal ,” AFML-TR-67...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910427
EISBN: 978-1-62708-250-1
... materials. The responsibility for generating this database on corrosion behavior often falls upon the alloy producers or developers of improved corrosion-control coatings or systems. After an appropriate material is selected, it is common practice to require specific quality-control tests to determine...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.t66910237
EISBN: 978-1-62708-250-1
... Not recommended Not recommended Cathodic protection Not recommended Most economical and effective method, especially with organic coatings other than paint Fairly effective with organic coatings Very effective Not recommended Effective under special conditions Inhibitors: liquid and vapor...