1-20 of 4017 Search Results for

castings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410103
EISBN: 978-1-62708-280-8
... Abstract The die casting process is a widely applied technique used by a variety of industries. This chapter reviews the casting design and engineering requirements for optimizing the characteristics of die castings. die castings casting design The die casting process is a widely...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410151
EISBN: 978-1-62708-280-8
... Abstract This chapter discusses the various factors pertinent to gravity permanent mold (GPM) castings, along with their advantages, limitations, and significance. The discussion covers the geometric factors, process and manufacturing elements, gating practices, and feeding principles...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.t68410215
EISBN: 978-1-62708-280-8
... Abstract This chapter discusses various factors pertinent to the applications of low-pressure permanent mold casting process, namely decorative automotive wheels, critical safety structural components, and chassis components. low-pressure permanent mold castings decorative automotive...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.aceg.9781627082808
EISBN: 978-1-62708-280-8
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720293
EISBN: 978-1-62708-305-8
... Abstract The inspection of castings normally involves checking for shape and dimensions, coupled with aided and unaided visual inspection for external discontinuities and surface quality. This chapter discusses methods for determining surface quality, internal discontinuities, and dimensional...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.ttg2.t61120039
EISBN: 978-1-62708-269-3
... Abstract Titanium castings are used in a wide range of aerospace, chemical process, marine, biomedical, and automotive applications. This chapter provides an overview of titanium casting and associated processes and how they compare with other manufacturing methods. It also discusses the role...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.9781627083355
EISBN: 978-1-62708-335-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200001
EISBN: 978-1-62708-354-6
... Abstract This chapter defines steel castings, explains when to use steel castings, gives an overview of casting processes, and gives examples of suitable applications for cast steel parts. steel castings near net shape Opening image for Chapter 1, “Introduction to Steel Castings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200007
EISBN: 978-1-62708-354-6
... Abstract Steel castings are produced in thousands of designs for different applications. They fill needs in many industries, including transportation, construction machinery, earthmoving equipment, rolling mills, mining, oil and gas exploration, and power generation. This chapter touches upon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200048
EISBN: 978-1-62708-354-6
... Abstract Casting is one of the basic processes used for the shaping of steel. It is economical in both cost and time of production. Numerous components are produced from cast steel because of the advantages of the process. These advantages can best be described under the following headings...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200065
EISBN: 978-1-62708-354-6
... Abstract This chapter discusses the role of standards and specifications for steel castings. It defines specifications and discusses how certification, testing, examination, methods, practices, procedures, compositions, properties, facilities, statistical process control, and documentation...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200144
EISBN: 978-1-62708-354-6
... Abstract Parts of machines and equipment that have previously been designed as wrought or fabricated parts, or as cast parts of metals other than steel, are often reconsidered as steel castings. This chapter presents bending test data for several junction designs of L and box sections...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1995
DOI: 10.31399/asm.tb.sch6.t68200295
EISBN: 978-1-62708-354-6
... Abstract Nickel-base castings are produced from a group of alloys with compositions that are typically greater than 50% Ni and less than 10% iron. This chapter presents the casting compositions of nickel-base alloys. It then provides an overview of heat treatment, mechanical properties...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140047
EISBN: 978-1-62708-335-5
.... This chapter describes the causes and control of porosity and inclusions in aluminum castings as well as the combined effects of hydrogen, shrinkage, and inclusions on the properties of aluminum alloys. In addition, it discusses the applications of radiography to reveal internal discontinuities in aluminum...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140061
EISBN: 978-1-62708-335-5
... Abstract The metallurgy of aluminum and its alloys offers a range of opportunities for employing heat treatments to obtain desirable combinations of mechanical and physical properties such that castings meet defined temper requirements. This chapter discusses the processes involved in solution...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.tb.aacppa.t51140069
EISBN: 978-1-62708-335-5
... Abstract This chapter reviews and provides data tables for the wide range of properties and performance characteristics that are possible with specific aluminum casting alloys and tempers. Properties and performance attributes addressed include casting and finishing characteristics; typical...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320103
EISBN: 978-1-62708-332-4
... Abstract This chapter covers mechanical properties, microstructures, chemical compositions, manufacturing processes, and engineering of gating practices for several applications of gray, white, and alloyed cast irons. It begins with a description of material standards, followed by a section...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320157
EISBN: 978-1-62708-332-4
... guidelines for malleable iron castings. composition iron castings malleabilization malleable iron tensile strength yield strength THE DEVELOPMENT OF MALLEABLE IRON in 1720 was a unique innovation because this new type of iron was strong, tough, machinable, and malleable for piercing...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320163
EISBN: 978-1-62708-332-4
... Abstract Ductile iron has far superior mechanical properties compared to gray iron as well as significantly improved castability and attractive cost savings compared to cast steel. This chapter begins with information on graphite morphology and matrix type. It then discusses the advantages...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2022
DOI: 10.31399/asm.tb.isceg.t59320195
EISBN: 978-1-62708-332-4
...). Information on the growth of premachined ADI components is also provided. Further, the chapter describes two slightly different systems for austempering: atmospheric-salt and salt-salt systems. Finally, it presents general guidelines for component designers, casting manufacturers, and heat treaters to apply...