... designations Fiber designation Type Commercial source AS-4 High-strength carbon/graphite Hexcel T-400 Carbon/graphite Toray, SGL T-650 Carbon/graphite Toray IM-7 Intermediate-modulus carbon/graphite Toray M46J High-modulus carbon/graphite Toray OC 463 750 yield E-glass...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860001
EISBN: 978-1-62708-338-6
... composite wall is thicker, which may negatively influence hydraulics ( Ref 1.10 – 1.16 ). The design of high-speed rotors now benefits from the use of very high-strength carbon fibers such as Toray T 800 and T 1000 (Toray Composites America, Tacoma WA). The research into high-speed rotor design started...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860095
EISBN: 978-1-62708-338-6
... 3529M-97(2008) Standard Test Method for Matrix Solids Content and Matrix Content of Composite Prepreg ASTM D 3530/D 3530M-97(2008) Standard Test Method for Volatiles Content of Composite Material Prepreg ASTM D 3531-99(2009) Standard Test Method for Resin Flow of Carbon Fiber-Epoxy Prepreg...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860065
EISBN: 978-1-62708-338-6
... doubled. A 48-fiber package is shown in Fig. 6.7 . Both carbon- and glass-fiber packages are mounted horizontally on a platform that moves with the filament winding machine carriage. Fiber tension is very low for the least fiber damage in the total fiber-delivery system. Leather straps over a steel...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860115
EISBN: 978-1-62708-338-6
... Propulsion Conference , June 21–23, 1982 ( Cleveland, OH ) 10.2514/6.1982-1067 9.11 Halpin J.C. , Primer on Composite Materials: Analysis , Technomic Publishing Company , revised 1984 9.12 Reynolds H.M. and Dhillon M. , “ Development of the Orbus-1 Carbon Fiber/Epoxy Motor...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.9781627083386
EISBN: 978-1-62708-338-6
Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2011
DOI: 10.31399/asm.tb.cfw.t52860007
EISBN: 978-1-62708-338-6
... ), LPG tanks, self-contained breathing apparatus tanks, hydrogen tanks, electrical isolators, rollers, drive shafts, and many other items too numerous to list. Fig. 2.23 Filament winding a pressure vessel with carbon fiber Complex-shaped parts, such as elbows and T-parts for the pipe...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870031
EISBN: 978-1-62708-314-0
... Abstract This chapter discusses the properties and processing characteristics of glass, aramid, carbon, and ultra-high molecular weight polyethylene fibers and related product forms, including woven fabrics, prepreg, and reinforced mats. It also includes a review of fiber terminology as well as...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870373
EISBN: 978-1-62708-314-0
... Abstract This chapter examines the static, fatigue, and damage tolerance properties of glass, aramid, and carbon fiber systems. It also explains how delaminations, voids, porosity, fiber distortion, and fastener hole defects affect impact resistance and strength. aramid fibers carbon...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780295
EISBN: 978-1-62708-281-5
... Polyphenylene sulfide (a) 49 Polyethylene, branched (a) 100–220 Polypropylene (a) 81–100 Polystyrene (a) 50–83 Polyvinyl chloride (a) 50–100 Glass (b) 8.3–9.7 Gold (b) 14.3 Cast iron (b) 10.6 Carbon graphite (b) 7.9 Hardened stainless steel (b) 17.3 (a...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.9781627082914
EISBN: 978-1-62708-291-4
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 1999
DOI: 10.31399/asm.tb.lmcs.t66560081
EISBN: 978-1-62708-291-4
... Abstract This chapter covers a broad range of low-carbon steels optimized for structural applications. Low-carbon structural steels are generally considered the highest-strength steels that can be welded without undue difficulty, even in the field. They include mild steels, carbon-manganese and...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550385
EISBN: 978-1-62708-307-2
.../density) of high-strength fiber composites, especially carbon, are higher than other comparable aerospace metallic alloys. This translates into greater weight savings, resulting in improved performance, greater payloads, longer range, and fuel savings. Composites do not corrode, and their fatigue...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2008
DOI: 10.31399/asm.tb.emea.t52240607
EISBN: 978-1-62708-251-8
...-performance carbon, metallic, or ceramic additions, as depicted in Fig. 33.1 . Reinforcements, characterized as either continuous or discontinuous, may constitute from 10 to 70 vol% of the composite. Continuous fiber reinforcements include graphite, silicon carbide (SiC), boron, aluminum oxide (Al 2 O 3...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550457
EISBN: 978-1-62708-307-2
... nonferrous alloy, and the reinforcement consists of high-performance carbon, metallic, or ceramic additions. Reinforcements, either continuous or discontinuous, may constitute from 10 to 70 vol% of the composite. Continuous fiber or filament (f) reinforcements include graphite, silicon carbide (SiC), boron...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550569
EISBN: 978-1-62708-307-2
..., continuous fiber ceramic composites, and carbon-carbon composites. It also describes a number of ceramic-matrix composite processing methods, including cold pressing and sintering, hot pressing, reaction bonding, directed metal oxidation, and liquid, vapor, and polymer infiltration. ceramic-matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870285
EISBN: 978-1-62708-314-0
... Thermoplastics , Technomic Publishing , 1993 • “ User’s Guide for Short Carbon Fiber Composites ,” Zoltek Companies Inc. , 2000 For a single fiber embedded in a matrix, as shown in Fig. 10.1 , the stress applied to the matrix is transferred to the fiber by shear across the interface. The matrix...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780276
EISBN: 978-1-62708-281-5
.... , Ed., North Holland , 1972 10.1016/B978-0-7204-0247-6.50005-6 19. Tewari U.S. , Bijwe J. , Mathur J.N. , and Sharma I. , Studies on Abrasive Wear of Carbon Fiber (Short) Reinforced Polyamide Composites , Tribol. Int. , Vol 25 , 1992 , p 53 – 60 10.1016/0301-679X(92...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870537
EISBN: 978-1-62708-314-0
... much larger, ranging from 3.9 to 5.5 mil (100 to 140 μm) in diameter, and are made one filament at a time by chemical vapor deposition on a small substrate, normally tungsten wire or carbon fiber. Large, stiff boron and silicon carbide monofilament fibers ( Fig. 20.5 ) have been evaluated for high...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.mmfi.t69540319
EISBN: 978-1-62708-309-6
... fibers of glass, carbon, boron, aramid, or ceramic. The preforms may be a unidirectional prepreg tape or a multidirectional fabric (e.g., woven, weaved, braided, or knitted). In general, prepreg tapes made of thermoplastic resins have much longer shelf lives. The fiber-reinforced composite laminates also...