Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030247
EISBN: 978-1-62708-282-2
... in Ref 1 to 14 . The initially oxygen-free geologic environment may be altered by a variety of oxygen-contaminated fluids that can be introduced. Examples are drilling fluids (often referred to as “muds”), which are used during drilling and maintenance of wells. These can include high-density clear...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2013
DOI: 10.31399/asm.tb.mfub.t53740213
EISBN: 978-1-62708-308-9
... machining (WJM) Abrasive waterjet machining (AWJM) Ultrasonic machining (USM) Electrical Electrochemical machining (ECM) Electrochemical grinding (ECG) Electrochemical discharge grinding (ECDG) Electrostream drilling (ES) Capillary drilling (CD) Shaped tube electrolytic machining (STEM) Thermal...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.9781627083195
EISBN: 978-1-62708-319-5
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 June 2007
DOI: 10.31399/asm.tb.pmsspmp.t52000167
EISBN: 978-1-62708-312-6
... Al 30 0.95 Ti 8.7 1.0 Zr 11.7 1.0 Effect of resin impregnation and sintering parameters on machinability Table 10.6 Effect of resin impregnation and sintering parameters on machinability Grade Sintering parameters Resin impregnation Drill life (number of holes) Drill...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290279
EISBN: 978-1-62708-306-5
... welding methods for thermoplastics. Source: Ref 10.2 The usual bolts, pins, and blind fasteners are used for composites; however, problems have led to the development of numerous special-purpose fasteners. Some of these problems are drilling of and installation damage to the composite...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.t62440001
EISBN: 978-1-62708-352-2
.... , 1968 . The Solid Phase Welding of Metals , Edward Arnold • Vianco P.T. and Rejent J.A. , 1997 . Capillary Flow Solder Wettability Test , Solder. Surf. Mt. Technol. , Vol 25 (No. 2 ), p 4 – 7 10.1108/09540919710777743 • Wang X.H. and Conrad H. , 1995...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2012
DOI: 10.31399/asm.tb.lmub.t53550511
EISBN: 978-1-62708-307-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2004
DOI: 10.31399/asm.tb.ps.9781627083522
EISBN: 978-1-62708-352-2
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.t51230001
EISBN: 978-1-62708-351-5
... modifies the properties of the parent material as it will work-harden when mechanically deformed. Fig. 1.22 Calculated time for molten tin and copper to flow up a perfectly wetted capillary [ Nicholas 1989 ] Fig. 1.21 Effect of temperature on the joint clearance between tubular brass...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2011
DOI: 10.31399/asm.tb.mnm2.t53060117
EISBN: 978-1-62708-261-7
... clean during heating to the flow temperature of the brazing alloy, and a suitable joint design that allows capillary action is used. Strong, uniform, leakproof joints can be made rapidly, inexpensively, and even simultaneously. Joints that are inaccessible and parts that may not be joinable at all...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2005
DOI: 10.31399/asm.tb.pb.9781627083515
EISBN: 978-1-62708-351-5
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030200
EISBN: 978-1-62708-282-2
... , 153 19. Bilhartz H.L. , Sweet Oil Well Corrosion—API Drilling and Production Practice , American Petroleum Institute , 1952 , p 54 20. Bilhartz H.L. , High Pressure Sweet Oil Well Corrosion , Corrosion , Vol 7 ( No. 8 ), Aug 1951 , p 256 – 264 10.5006/0010-9312...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2020
DOI: 10.31399/asm.tb.bpapp.t59290111
EISBN: 978-1-62708-319-5
... as pressure inside the chamber increases to values typically near 400 MPa (58 ksi). Fig. 6.2 Green machining is common after compacting powder-binder structures, prior to sintering. This micrograph shows holes drilled in a compact. Individual particles are discernible, and slight edge roughness...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2011
DOI: 10.31399/asm.tb.jub.t53290079
EISBN: 978-1-62708-306-5
... and distribution of filler metal takes place by deposition rather than by capillary action. Equipment and some filler metals used in braze welding are the same as those used in torch brazing. In braze welding of ferrous metals, the base metal is not melted. The filler-to-base-metal bond is the same as in torch...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.tb.cub.9781627082501
EISBN: 978-1-62708-250-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110563
EISBN: 978-1-62708-247-1
Series: ASM Technical Books
Publisher: ASM International
Published: 01 April 2013
DOI: 10.31399/asm.tb.imub.t53720183
EISBN: 978-1-62708-305-8
... workpieces using a water washable, fluorescent penetrant system. Source: Ref 1 Fig. 1 Actions of penetrant and developer. (a) Penetrant liquid is drawn into an open crack by capillary action. (b) Excess surface penetrant is removed by wiping with a cloth, washing directly with water, treating...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 March 2002
DOI: 10.31399/asm.tb.stg2.9781627082679
EISBN: 978-1-62708-267-9
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.t67850060
EISBN: 978-1-62708-260-0
.... These problems can be completely eliminated by good technique. Clamps, are generally machined from plate stock about ¼ in thick that has been cut into blocks about ½ by 1½ in, as shown in Fig. 2-4 . Holes are drilled into each end of the clamp halves. One half is threaded to receive a bolt of suitable...