Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780064
EISBN: 978-1-62708-281-5
...-speed resin transfer molding or fast resinject 2 0.3 30 3370 … … n y n y n y n n y y Foam polyurethane 0.5 0.07 n/a … … … n y y y y y n n y y Reinforced foam 1 0.15 30 3370 3.0 30 y y y y n y n n y y Filament winding n/a n/a n/a n/a … … n...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2015
DOI: 10.31399/asm.tb.cpi2.t55030247
EISBN: 978-1-62708-282-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2006
DOI: 10.31399/asm.tb.ex2.t69980195
EISBN: 978-1-62708-342-3
... of tin. This is important for the mechanically fatigue loaded sheathed cables on, for example, bridges. Lead forms a eutectic with 11.1% antimony at 253 °C. This has to be taken into account when determining the deformation temperature for the extrusion of PbSb alloys with eutectic, low-melting point...
Series: ASM Technical Books
Publisher: ASM International
Published: 30 April 2021
DOI: 10.31399/asm.tb.tpsfwea.9781627083232
EISBN: 978-1-62708-323-2
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1984
DOI: 10.31399/asm.tb.mpp.9781627082600
EISBN: 978-1-62708-260-0