Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270126
EISBN: 978-1-62708-301-0
...Abstract Abstract A test flight was cut short after a fire warning came on indicating a problem with one of the four engines on an aircraft. A visual examination following the precautionary landing revealed several burned hoses, a melted bolt, and fuel leaking from the base of the main burner...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270156
EISBN: 978-1-62708-301-0
.... Based on these findings, investigators concluded that the failure was due to a fatigue crack initiated from a corrosion pit, which may have been caused by chemicals released by the burning of bonding resin. fatigue fracture corrosion pits SEM fractography tail rotor blades visual examination...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270197
EISBN: 978-1-62708-301-0
...Abstract Abstract One of the rotor bearings in an electric motor failed, producing excessive vibrate. The bearing was removed and disassembled, revealing craters and bruises on the inner ring raceway and balls along with evidence of melting and burning of metal. Scanning electron microscopy...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110666
EISBN: 978-1-62708-247-1
... techniques for uncovering reliability issues, namely burn-in and outlier screening. References References [1] Henderson C. , “ Quality and Reliability ”, 21 st Century Product Analysis (Chapter 17) , 1 - 20 ( 2012 ) [2] Staff, “ Statistical Process Control/Design of Experiments...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 January 2015
DOI: 10.31399/asm.tb.spsp2.t54410439
EISBN: 978-1-62708-265-5
... shortness associated with copper and overheating and burning as occur during forging. It addresses various types of embrittlement, including quench embrittlement, tempered-martensite embrittlement, liquid-metal-induced embrittlement, and hydrogen embrittlement, and concludes with a discussion on high...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.tb.msisep.t59220353
EISBN: 978-1-62708-259-4
... and fine pearlite inside the grains. Etchant: nital 4%. Courtesy of Villares Metals S.A., SP, Brazil. Fig. 11.62 (a) Shock-resistant steel ASTM A681-S7 overheated during forging (burned). Presence of oxides and evidence of start of melting (incipient fusion) at the grain boundaries. Etchant...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080335
EISBN: 978-1-62708-304-1
...Examples of flue gas compositions generated by different WTE mass-burning boilers Table 12.1 Examples of flue gas compositions generated by different WTE mass-burning boilers Gas Composition, vol% Ogden-Martin (US) (a) Saint Ouen (France) (b) Richtlinien (Germany) (c) Kuririn...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2003
DOI: 10.31399/asm.tb.cfap.t69780159
EISBN: 978-1-62708-281-5
...Abstract Abstract This article describes the basic approaches to improving the fire resistance of a polymeric material, considers the burning process on a microscale and macroscale, and discusses various test methods for determining the flammability characteristics of polymeric materials. Test...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770171
EISBN: 978-1-62708-337-9
... the propensity of quenched carburized steels to burn and crack during surface grinding. The chapter includes numerous data plots and tables showing how the various treatments influence hardness, wear resistance, tensile properties, and fatigue and fracture behaviors. References References 1. Speich...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 1999
DOI: 10.31399/asm.tb.cmp.t66770199
EISBN: 978-1-62708-337-9
... temperature indicated is for slow heating; at high heating rates, e.g., in a grinding pass, the Ac temperatures will be elevated. Note: high-speed heating raises Ac temperatures. Micrograph, 500× Fig. 8.2 Effect of grinding burns of increasing severity on microhardness. Curve 7 represents...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.tb.scm.t52870401
EISBN: 978-1-62708-314-0
... for composites except ultrahigh molecular weight polyethylene are relatively nonflammable; however, at high temperatures they soften, char, or melt, and their mechanical strength is reduced. Composite laminates tend to burn in layers. When heated, the resin in the first layer degrades, and any combustible...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2019
DOI: 10.31399/asm.tb.mfadr7.t91110634
EISBN: 978-1-62708-247-1
... Selection for Variance Reduction in IDDQ and Other Parametric Data, ” International Test Conference , 2001 , p. 92 - 100 . [24] Madge R. , Rehani M. , Cota K. , Daasch W. , “ Statistical Post-Processing at Wafersort - An Alternative to Burn-in and a Manufacturable Solution...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2018
DOI: 10.31399/asm.tb.fibtca.t52430001
EISBN: 978-1-62708-253-2
... is heated to produce hot water, steam, superheated steam, or any combination of these under pressure by the application of heat. The necessary heat is produced by burning solid, liquid, or gaseous fuel under a controlled supply of air in the combustion chamber of the boiler. Thus, the boiler is an appliance...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 October 2005
DOI: 10.31399/asm.tb.faesmch.t51270191
EISBN: 978-1-62708-301-0
... on the 17th-stage side. The trailing edges of all the 18th-stage blades had suffered mechanical damage. The gap between the 18th- and 19th-stage discs showed excessive metal burning and melting at the seal land and the gap, which should normally be in the range 6 to 8 mm. The gap had increased...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 December 2000
DOI: 10.31399/asm.tb.htgpge.t67320033
EISBN: 978-1-62708-347-8
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050245
EISBN: 978-1-62708-311-9
..., and hardness pattern Pinion pins and axles Case depth, structure, and hardness pattern Linear guide components Case depth, structure, and grinder burn Steering racks and the like Case depth, structure, and hardness pattern Source: Ref 4 Possible hardening errors during induction...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 August 2015
DOI: 10.31399/asm.tb.piht2.t55050173
EISBN: 978-1-62708-311-9
... situation. While the manufacturers state in their literature that parts can be tempered without washing, experience shows that the polymers must be rinsed or washed off before tempering. Several things can happen when parts are tempered without polymer removal. First, evaporation and burning of the polymer...
Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.smnm.t52140063
EISBN: 978-1-62708-264-8
... contact with the iron. However, such is not the case. If pure carbon powder instead of charcoal is used, no carburization occurs. Charcoal, being the remains of burned wood, contains hydrocarbons that vaporize and produce a gas containing carbon monoxide (CO). The carbon atoms are carried by gas molecules...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 November 2007
DOI: 10.31399/asm.tb.htcma.t52080259
EISBN: 978-1-62708-304-1
... of the reheater (1000 °F steam) for 3½ years in a 255 MW(e) subcritical boiler, which burned high chlorine coal (about 0.3%). The 304H reheater tubes exhibited a typical 4 year life. Courtesy of Welding Services Inc. Fig. 10.89 The cross section of alloy 52/304H overlay tube after testing as part...
Book Chapter

Series: ASM Technical Books
Publisher: ASM International
Published: 01 September 2005
DOI: 10.31399/asm.tb.gmpm.t51250163
EISBN: 978-1-62708-345-4